1.
制备了分子印迹硅纳米-氧化石墨烯复合吸附材料,并研究了复合材料对双酚A(Bisphenol A,BPA)的吸附性能。实验结果表明:复合吸附材料对BPA的吸附在35min内达到吸附平衡,Langmuir等温线模型得出最大吸附容量约为338.3mg/g;相对于BPA的结构类似物,对BPA具有良好的选择吸附性能;在溶液p H接近6时对BPA的去除率最高,低温条件有利于吸附的进行;该材料具有优异的循环吸附性能。  相似文献   
2.
On-line in-tube solid phase microextraction (in-tube SPME) coupled to high performance liquid chromatography and tandem mass spectrometry (HPLC-MS/MS) was successfully applied to the determination of selected triazines in water samples. The method based on the employment of a packed column containing graphene oxide (GO) supported on aminopropyl silica (Si) showed that the extraction phase has a high potential for triazines extraction aiming to its physical-chemical properties including ultrahigh specific surface area, good mechanical and thermal stability and high fracture strength. Injection volume and loading time were both investigated and optimized. The method validation using Si-GO to extract and concentrate the analytes showed satisfactory results, good sensitivity, good linearity (0.2–4.0 µg L?1) and low detection limits (1.1–2.9 ng L?1). The high extraction efficiency was determined with enrichment factors ranging from 1.2–2.9 for the lowest level, 1.3–4.9 intermediate level and 1.2–3.0 highest level (n = 3). Although the analytes were not detected in the real samples evaluated, the method has demonstrated to be efficient through its application in the analysis of spiked triazines in ground and mineral water samples.  相似文献   
3.
纳米二氧化钛复合石墨烯催化剂的制备及处理染料废水   总被引:1,自引:0,他引:1  
以硫酸钛为原料,采用共沉淀法,制备了一系列纳米二氧化钛复合石墨烯催化剂,采用XRD和FTIR对样品进行表征。通过紫外光照射亚甲基蓝溶液光催化降解实验,研究石墨烯的加入量对TiO2光催化性能的影响,结果表明,TiO2-GO-5具有最佳的光催化性能。在pH=6.00、TiO2-GO-5的投加量为0.070 g/50 mL、光照3 h条件下,100 mg/L亚甲基蓝溶液的脱色率达到最大值为90.52%。  相似文献   
4.
磺化石墨烯对小麦幼苗生长及生理生化指标的影响   总被引:1,自引:0,他引:1  
随着石墨烯生产量和使用量的不断增大,其对生态环境的风险逐渐引起了环境学家的关注。采用水培试验,探究了磺化石墨烯(SGO)对小麦幼苗的生长、抗氧化酶活性及脂质过氧化的影响。结果表明:在培养10 d后,低浓度磺化石墨烯对小麦根系的生长有显著促进作用(P0.05),200 mg·L-1浓度处理与对照处理相比提高了84.3%,随着浓度增加促进作用逐渐减弱,1 000 mg·L-1时与对照相比提高了19.9%。但对小麦地上部的生长没有影响。磺化石墨烯处理的小麦幼苗根系和叶片组织中超氧化物歧化酶(SOD)、过氧化氢酶(CAT)、过氧化物酶(POD)及丙二醛(MDA)都呈现先下降后上升的趋势。当磺化石墨烯浓度低于200 mg·L-1时,处理组小麦抗氧化酶的活性及MDA含量相对于对照处理大都有所降低,说明低浓度时磺化石墨烯没有对小麦的生长产生氧化胁迫,这与磺化石墨烯可能具有一定的抗氧化能力有关,而高浓度时由于产生氧化胁迫使各项生理生化指标逐渐上升。本实验结果为石墨烯材料对植物的毒理学研究提供了基础数据。  相似文献   
5.
以钛酸四正丁酯和石墨为原料,通过水热法制备了锐钛矿型为主的纳米TiO2复合光催化剂(纳米TiO2-石墨烯),并采用XRD,FTIR,FESEM,TEM技术对其进行了表征。通过紫外光照射降解溶液中的罗丹明B(RhB)研究了TiO2-石墨烯的光催化活性,分析了初始罗丹明B质量浓度、催化剂加入量、溶液pH和催化剂使用次数等影响降解效果的因素。实验结果表明:在初始RhB质量浓度为20 mg/L、溶液pH为7.10、催化剂加入量为1.000 g/L的条件下,紫外光照射30 min时,纳米TiO2-石墨烯对RhB的降解率高达98.69%,明显高于纳米TiO2的44.69%;纳米TiO2-石墨烯稳定性较强,可多次重复使用。  相似文献   
6.
石墨烯是一种应用广泛的新兴非金属纳米材料,具有独特的电学机械性能、超大的比表面积以及潜在的生物相容性,在材料、电子、能源、光学以及生物医学等领域得到广泛应用。与此同时,石墨烯的环境行为和生物毒性也随之引起日益广泛的关注。本文通过对石墨烯纳米材料的动物毒性、细胞毒性、毒性影响因素和毒性机制等相关研究进展进行总结。石墨烯纳米材料可通过气管滴注、吸入、静脉注射、腹腔注射以及口服等方式进入体内,通过机械屏障、血脑屏障和血液胎盘屏障等积累在肺、肝、脾等部位引起急性或者慢性损伤;目前有关石墨烯毒性机制的研究主要集中于线粒体损伤、DNA损伤、炎性反应、凋亡等终点及氧化应激参与的复杂信号通路,不同石墨烯纳米材料的浓度、尺寸、表面结构和官能团等对石墨烯的生物毒性影响不同。鉴于当前该领域研究的局限性,对石墨烯纳米材料生物毒性研究的发展方向进行了展望,进而为石墨烯材料的安全应用提供理论借鉴和实践参考。  相似文献   
7.
Biomaterial industry is a widely growing field that is closely related to advanced materials. With development in fabrication techniques new materials are being created by researchers daily. The currently used biomaterials for biomedical applications have some limitations. This review examines those limitations such as corrosion, short fatigue life, less wear resistance, and inadequate mechanical properties. These limitations may lead to adverse effects. To overcome these limitations carbon-based nanomaterials may be incorporated such that these biomaterials reach the level of ideal biomaterials. Upgrade of biomaterials with graphene and carbon nanotubes (CNTs) needs to be done only after checking the safety profile of these materials. Biocompatibility of functionalized graphene and CNT is found to be adequate for the use in many applications such as drug delivery, biosensing and imaging, cancer therapeutics, and tissue regeneration whereas pristine graphene and CNT may produce adverse effects. The potential of carbon-based nanomaterials and graphene (and its derivatives) in overcoming those limitations and enhancing biological activities of ongoing biomaterials by acting as composites and coating material is examined. In addition, nanomaterials employ new techniques in biomedical application such as cancer therapy for more efficient results.  相似文献   
8.
综述了基于石墨烯构建的电化学传感器在重金属、有毒气体、农药残留、酚类有机污染物等对环境造成一定危害的物质检测中的应用,并展望了石墨烯电化学传感器在环境监测领域中的发展。  相似文献   
9.
Because of its significant toxicological effects on the environment and human health,arsenic(As) is a major global issue.In this study,an Fe-based metal-organic framework(MOF)(Materials of Institut Lavoisier:MIL-100(Fe)) which was impregnated with reduced graphene oxide(rGO) by using a simple hydrothermal method and coated with birnessitetype manganese oxide(δ-MnO_2) using the one-pot reaction process(MIL-100(Fe)/rGO/δ-MnO_2 nanocomposites) was synthesized and applied successfully in As removal.The removal efficiency was rapid,the equilibrium was achieved in 40 min and 120 min for As(Ⅲ) and As(Ⅴ),respectively,at a level of 5 mg/L.The maximum adsorption capacities of As(Ⅲ) and As(Ⅴ) at pH 2 were 192.67 mg/g and 162.07 mg/g,respectively.The adsorbent revealed high stability in pH range 2-9 and saturated adsorbent can be fully regenerated at least five runs.The adsorption process can be described by the pseudo-second-order kinetic model and Langmuir monolayer adsorption.The adsorption mechanisms consisted of electrostatic interaction,oxidation and inner sphere surface complexation.  相似文献   
10.
氧化石墨烯对亚甲基蓝和铜离子的共吸附行为研究   总被引:6,自引:4,他引:2       下载免费PDF全文
氧化石墨烯(GO)具有高比表面积和丰富的含氧官能团,表面存在着大量的吸附点位,被认为是去除水体污染物的高效吸附剂,而其在有机物-重金属复合污染环境中的吸附行为却鲜有报道.因此,本文采用改良Hummers法制备出GO,通过扫描电镜(SEM)、透射电镜(TEM)、红外光谱(FTIR)、拉曼光谱(Raman)和X射线衍射(XRD)等物理表征方法对GO的形貌结构和表面官能团进行了表征.随后,侧重研究了GO对有机物及重金属污染物的单独和共吸附行为,选取亚甲基蓝(MB)与Cu(Ⅱ)作为复合污染水体的特征污染物,探讨了不同浓度Cu(Ⅱ)对MB及不同浓度MB对Cu(Ⅱ)的吸附性能的影响.结果表明,不同类型的污染物单独存在时,GO对MB和Cu(Ⅱ)的吸附量分别为29.13和424.16mg·g-1;而当上述两种污染物共存时,GO对MB和Cu(Ⅱ)的吸附性能均明显下降,这说明MB与Cu(Ⅱ)在GO表面的吸附点位存在着竞争吸附关系,并且MB对Cu(Ⅱ)吸附的抑制作用明显高于Cu(Ⅱ)对MB吸附的影响.  相似文献   