舰载飞机腐蚀控制与防护技术
引用本文:孙盛坤,孙志华,汤智慧,陈亚争,杨宗琪,李斌,张骐,韩保红,潘峤.舰载飞机腐蚀控制与防护技术[J].装备环境工程,2017,14(3):18-22.
作者姓名:孙盛坤  孙志华  汤智慧  陈亚争  杨宗琪  李斌  张骐  韩保红  潘峤
作者单位:1. 海军驻北京地区航空军事代表室,北京,100041;2. 中国航发北京航空材料研究院,航空材料先进腐蚀与防护航空科技重点实验室,北京 100095;3. 中航工业沈阳飞机设计研究所,沈阳,110035;4. 南昌航空大学,南昌,330063
摘    要:分析了舰载飞机高温、高湿、高盐雾的服役环境特点,并阐述了舰载飞机易发生的腐蚀问题,提出了舰载飞机腐蚀防护与控制的研究思路,并对舰载飞机先进腐蚀控制与防护技术进行了总结,包括结构防护设计、选用综合性能优良的耐蚀材料、防护技术、舰上腐蚀控制维护/维修技术等。总结了舰载飞机全面腐蚀控制研究重点发展方向及建议。

关 键 词:舰载飞机  腐蚀控制  防护技术
收稿时间:2016/11/6 0:00:00
修稿时间:2017/3/15 0:00:00

Corrosion Control and Protection Technology of Carrier-borne Aircraft
SUN Sheng-kun,SUN Zhi-hu,TANG Zhi-hui,CHEN Ya-zheng,YANG Zong-qi,LI Bin,ZHANG Qi,HAN Bao-hong and PAN Qiao.Corrosion Control and Protection Technology of Carrier-borne Aircraft[J].Equipment Environmental Engineering,2017,14(3):18-22.
Authors:SUN Sheng-kun  SUN Zhi-hu  TANG Zhi-hui  CHEN Ya-zheng  YANG Zong-qi  LI Bin  ZHANG Qi  HAN Bao-hong and PAN Qiao
Institution:Navy Aeronautical Military Delegate Department in Beijing Area, Beijing 100041, China,AECC Beijing Institute of Aeronautical Materials, Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Material, Beijing 100095, China,AECC Beijing Institute of Aeronautical Materials, Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Material, Beijing 100095, China,AVIC Shenyang Aircraft Design and Researcher Institute, Shenyang 110035, China,Nanchang Hangkong University, Nangchang 110035, China,AECC Beijing Institute of Aeronautical Materials, Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Material, Beijing 100095, China,AECC Beijing Institute of Aeronautical Materials, Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Material, Beijing 100095, China,AECC Beijing Institute of Aeronautical Materials, Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Material, Beijing 100095, China and AECC Beijing Institute of Aeronautical Materials, Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Material, Beijing 100095, China
Abstract:Service environment characteristics such as high temperature, high humidity, and high salt fog were analyzed, and corrosion problems which are likely to occur on carried-borne aircraft were stated. The development research direction of corrosion control and protection were also put forward. The novel corrosion control and protection technologies such as structural protection design, selection anti-corrosion materials, protection technology, maintenance and repairing technology on board were summarized. Major development directions and suggestions on overall corrosion control and research of corrosion control were also summarized.
Keywords:carried-borne aircraft  corrosion control  protection technology