De novo formation characteristics of dioxins in the dry zone of an iron ore sintering bed |
| |
Authors: | Suzuki K Kasai E Aono T Yamazaki H Kawamoto K |
| |
Affiliation: | Department of Architectural Environmental Engineering, Kanto Gakuin University, 1-50-1 Mutsuurahigashi, Kanazawa-ku, Yokohama 236-8501, Japan. suzuki.kazuyuki@nies.go.jp |
| |
Abstract: | The objectives of this work are to understand the details of the mechanism of dioxin formation in the part of a sintering bed termed the dry zone, and to obtain ideas on how to prevent their formation. Sinter mixtures of various composition types were heated in a packed bed reactor, and dioxins in the outlet gas and in the sinter mixture residue were measured. The dioxin formation potential of a simple sinter mixture composed of iron ore, coke and limestone was markedly lower than that of fly ash from a municipal solid waste incinerator (MSWI). In consideration of this result, a series of experiments were conducted using a sinter mixture impregnated with CuCl2. Experimental results showed that dioxin formation was temperature-dependent in the range of 300-550 degrees C, with the maximum observed at around 300 degrees C, which was quite similar to that of fly ash from the MSWI. The homologue distribution of PCDD/Fs in gas and solid reflected the possible difference in carbonaceous materials in coke and activated coke. Gaseous hydrogen chloride acted as a chlorinating reagent for dioxin formation. |
| |
Keywords: | |
本文献已被 PubMed 等数据库收录! |
|