This research investigated the feasibility of reducing volatilization of heavy metals (lead, zinc and cadmium) in municipal solid waste incineration (MSWI) fly ash by forming pyromorphite-like minerals via phosphate pre-treatment. To evaluate the evaporation characteristics of three heavy metals from phosphate-pretreated MSWI fly ash, volatilization tests have been performed by means of a dedicated apparatus in the 100-1000 °C range. The toxicity characteristic leaching procedure (TCLP) test and BCR sequential extraction procedure were applied to assess phosphate stabilization process. The results showed that the volatilization behavior in phosphate-pretreated MSWI fly ash could be reduced effectively. Pyromorphite-like minerals formed in phosphate-pretreated MSWI fly ash were mainly responsible for the volatilization reduction of heavy metals in MSWI fly ash at higher temperature, due to their chemical fixation and thermal stabilization for heavy metals. The stabilization effects were encouraging for the potential reuse of MSWI fly ash.  相似文献   

2.
Fly ash (FA) from municipal solid waste incinerators has been known as hazardous waste, which is mostly because of the high content of heavy metal and dioxins. Besides the content, the form of the heavy metals in fly ash is also very important, because it is tightly related with the leaching behavior of fly ash in diverse circumstances. To evaluate the environment potential risk of fly ash, the Tessier chemical extraction method was adopted. In this study, four kinds of fly ash were examined, one sample from China (CFA) and the other three from Japan (RFA, CaFA and NaFA). Five metal elements were detected and they were Ni, Cr, Cd, Pb, and Cu. The result of total heavy metals’ concentration showed CFA has the lowest content. As to the Tessier chemical extraction experiments, the results show that Cd, Pb, and Cu have higher leaching risk in the environment than other heavy metals. The result of leaching test experiment showed that the more exchangeable speciation of Cd, Cr and Pb in FA, the more it could leach out in natural environment.  相似文献   

3.
The municipal solid waste incinerators (MSWIs) in Taiwan generate about 300,000 tons of fly ash annually, which is mainly composed of calcium and silicon compounds, and has the potential for recycling. However, some heavy metals are present in the MSWI fly ash, and before recycling, they need to be removed or reduced to make the fly ash non-hazardous. Accordingly, the purpose of this study was to use a hydrocyclone for the separation of the components of the MSWI fly ash in order to obtain the recyclable portion. The results show that chloride salts can be removed from the fly ash during the hydrocyclone separation process. The presence of a dense medium (quartz sand in this study) is not only helpful for the removal of the salts, but also for the separation of the fly ash particles. After the dense-medium hydrocyclone separation process, heavy metals including Pb and Zn were concentrated in the fine particles so that the rest of the fly ash contained less heavy metal and became both non-hazardous and recyclable.  相似文献   

4.
Calcium phosphate stabilization of fly ash with chloride extraction   总被引:5,自引:0,他引:5  
Municipal solid waste incinerator by products include fly ash and air pollution control residues. In order to transform these incinerator wastes into reusable mineral species, soluble alkali chlorides must be separated and toxic trace elements must be stabilized in insoluble form. We show that alkali chlorides can be extracted efficiently in an aqueous extraction step combining a calcium phosphate gel precipitation. In such a process, sodium and potassium chlorides are obtained free from calcium salts, and the trace metal ions are immobilized in the calcium phosphate matrix. Moderate calcination of the chemically treated fly ash leads to the formation of cristalline hydroxylapatite. Fly ash spiked with copper ions and treated by this process shows improved stability of metal ions. Leaching tests with water or EDTA reveal a significant drop in metal ion dissolution. Hydroxylapatite may trap toxic metals and also prevent their evaporation during thermal treatments. Incinerator fly ash together with air pollution control residues, treated by the combined chloride extraction and hydroxylapatite formation process may be considered safe to use as a mineral filler in value added products such as road base or cement blocks.  相似文献   

5.
The extraction of gallium from coal fly ash by leaching and extraction with commercial extractants Amberlite LA-2 and LIX 54N dissolved in kerosene was studied. Leaching of gallium and other metals from the fly ash was carried out with 6 M hydrochloric acid. The leaching liquor is first contacted with Amberlite LA-2 which extracts the gallium and iron. The iron is then precipitated with sodium hydroxide, while gallium remains in solution. Gallium is extracted selectively from the base solution with LIX 54; the resulting stripped solution contains 83% of the gallium present in the leaching liquor. A flow diagram for this dual-extraction process is proposed.  相似文献   

6.
Metal containing wastes like MSWI fly ashes and blast furnace sludge form a major environmental problem as they are polluted with heavy metals. The ash has to be landfilled or can be used as a construction material, but a pretreatment is in general necessary. Washing of the ashes with water in order to dissolve soluble salts or extracting the heavy metals with chemicals are possibilities. Blast furnace sludge contains large quantities of iron and carbon and could be recycled in the blast furnace, if the zinc content were not that high. Using a hydrometallurgical process the zinc can be removed from the sludge particles. In order to evaluate such treatment methods knowledge of the leaching behaviour of the studied material is very important. One of the factors influencing the leaching behaviour is the composition and mineralogy of the solids. A sequential extraction procedure, whereby the material is sequentially leached with different leaching solutions, can be used as an aid to characterize the material and to determine which chemical conditions are needed to obtain a sufficient extraction efficiency. To verify the accuracy of the sequential extraction procedure, a method is tested on MSWI fly ash and evaluated by comparing the results with those of leaching experiments whereby the final pH of the leaching solutions is varied over a wide range. Based upon this evaluation some suggestions for the use of the sequential extraction procedure are made and an adapted procedure is suggested, and applied to a blast furnace sludge.  相似文献   

7.

Waste treatment using thermal technologies, such as incineration, leads to the production of pollutants and wastes, including fly ash (FA). Fly ash contains heavy metals (HMs) and other contaminants and can potentially pose high risks to the environment and negatively impact health and safety. Consequently, stabilizing fly ash prior to either use or landfilling is crucial. The toxicity of fly ash through heavy metal leaching can be assessed using leaching tests. The leaching rates of heavy metals primarily depend on the surrounding conditions as well as fly ash properties and metal speciation. Physical separation, leaching or extraction, thermal treatment and solidification/chemical stabilization are proposed as suitable approaches for fly ash treatment. Economic considerations, environmental concerns, energy consumption and processing times can define the efficiency and selection of the treatment approach. This review considers the latest findings and compares the advantages and shortcomings of different fly ash treatment methods with the aim of highlighting the recent advances in the field. The review concludes that the simultaneous implementation of various methods can lead to highly efficient heavy metals removal/stabilization while simultaneously taking economic and environmental considerations into account.

  相似文献   

8.
Heavy metals in fly ash from municipal solid waste incinerators are present in high concentrations. Therefore fly ash must be treated as a hazardous material. On the other hand, it may be a potential source of heavy metals. Zinc, lead, cadmium, and copper can be relatively easily removed during the thermal treatment of fly ash, e.g. in the form of chlorides. In return, wet extraction methods could provide promising results for these elements including chromium and nickel. The aim of this study was to investigate and compare thermal and hydrometallurgical treatment of municipal solid waste fly ash. Thermal treatment of fly ash was performed in a rotary reactor at temperatures between 950 and 1050 °C and in a muffle oven at temperatures from 500 to 1200 °C. The removal more than 90% was reached by easy volatile heavy metals such as cadmium and lead and also by copper, however at higher temperature in the muffle oven. The alkaline (sodium hydroxide) and acid (sulphuric acid) leaching of the fly ash was carried out while the influence of temperature, time, concentration, and liquid/solid ratio were investigated. The combination of alkaline-acidic leaching enhanced the removal of, namely, zinc, chromium and nickel.  相似文献   

9.
This study investigated that water washing effects on the metals emission reduction in melting of municipal solid waste incinerator (MSWI) fly ash. Experimental conditions were conducted at liquid-to-solid (L/S) ratio 10, 20, and 100 for water-washing process and its subsequent melting treatment at 1450 °C for 2 h. The simple water-washing process as a pre-treatment for MSWI fly ash can remove most of the chlorides, leachable salts, and amphoteric heavy metals from the MSWI fly ash, resulting in the washed ash having lowered chlorine content. MSWI fly ashes washed by L/S ratio 10 and above that were melted at 1450 °C produced slag containing relatively high vitrificaton ratio of Cu and Pb. Besides, the vitrification ratios of Na, K, Ca, and Mg in washed MSWI fly ash were also higher than that of MSWI fly ash. The results indicated that washed MSWI fly ash can reduce the emission of metallic chlorides during its subsequent melting treatment.  相似文献   

10.
In previous studies, we focused on a mechanochemical process for recycling fly ash for use in cement; this process was expected to immobilize heavy metals in the fly ash, a desirable outcome in light of the fact that recycled fly ash is commonly used in the synthesis of inorganic materials. Here, we investigated the leaching of lead (Pb) from fly ash treated by a mechanochemical process and from cement prepared from the treated fly ash. We used lead oxide (PbO), a typical Pb compound in fly ash, as a model substance. Mechanochemical treatment of the fly ash inhibited Pb leaching by 93%, and further inhibition (more than 99.9%) was observed in cement produced from the treated fly ash. During the mechanochemical treatment, PbO was reduced to Pb by iron from the stainless-steel mill used for processing, and the lower solubility of Pb in water resulted in immobilization of the Pb.  相似文献   

11.
The 3R Process: (1) recovers fly ash and HCl from the flue gases; (2) removes heavy metals from the fly ash by extraction with HCl; (3) and returns a pelletized fly ash to the incinerator. Recoveries of about 90% of the Cd, 65% of the Zn and 20% of the Pb and Cu have been achieved in pilot tests. Full scale experiments proved the thermal decomposition of PCDD/PCDF. The 3R products meet the Swiss elution requirements.  相似文献   

12.
Municipal solid waste incineration (MSWI) fly ash is by-product and hazardous waste produced from MSWI plant. In the MSWI fly ash there are high contents heavy metals, among which cadmium (Cd) is more active and toxic. Although inorganic acid leaching is an effective way to remove heavy metals out from the MSWI fly ash and nitric acid has great efficiency for Cd removal, little literature reported the redistribution of remaining Cd in the MSWI fly ash. This investigation focused on the change of different factions (exchangeable, bound to carbonates, bound to Fe–Mn oxides, bound to organic matter and residual) of Cd in treated (i.e. washed with nitric acid) MSWI fly ash. Sequence extraction procedures (SEP) have been used to derive different fractions of Cd, results indicated that fractions of Cd have changed significantly after nitric acid washing procedures. Due to the changes of main compounds and microstructures stable Cd (bound to organic matter and residual) had opportunity to leach out, which resulted in a higher potential risk (or higher bioavailability index) for living creatures, although the total amount of Cd decreased. X-ray diffraction (XRD) and images of scanning electron microscope (SEM) proved these changes in washed MSWI fly ash.  相似文献   

13.
Thermal treatment of municipal solid waste (MSW) has become a common practice in waste volume reduction and resource recovery. For the utilization of molten slag for construction materials and metal recovery, it is important to understand the behavior of heavy metals in the melting process. In this study, the correlation between the contents of elements in feed materials and MSW molten slag and their distributions in the ash melting process, including metal residues, are investigated. The hazardous metal contents in the molten slag were significantly related to the contents of metals in the feed materials. Therefore, the separation of products containing these metals in waste materials could be an effective means of producing environmentally safe molten slag with a low hazardous metals content. The distribution ratios of elements in the ash melting process were also determined. The elements Zn and Pb were found to have a distribution ratio of over 60% in fly ash from the melting furnace and the contents of these metals were also high; therefore, Zn and Pb could be potential target metals for recycling from fly ash from the melting furnace. Meanwhile, Cu, Ni, Mo, Sn, and Sb were found to have distribution ratios of over 60% in the metal residue. Therefore, metal residue could be a good resource for these metals, as the contents of Cu, Ni, Mo, Sn, and Sb in metal residue are higher than those in other output materials.  相似文献   

14.
A water extraction process can remove the soluble salts present in municipal solid waste incinerator (MSWI) fly ash, which will help to increase the stability of the synthetic materials produced from the MSWI fly ash. A milling process can be used to stabilize the heavy metals found in the extracted MSWI fly ash (EA) leading to the formation of a non-hazardous material. This milled extracted MSWI fly ash (MEA) was added to an ordinary Portland cement (OPC) paste to induce pozzolanic reactions. The experimental parameters included the milling time (96 h), water to binder ratios (0.38, 0.45, and 0.55), and curing time (1, 3, 7 and 28 days). The analysis procedures included inductively coupled plasma atomic emission spectroscopy (ICP/AES), BET, mercury intrusion porosimetry (MIP), X-ray diffraction (XRD), and nuclear magnetic resonance (NMR) imaging. The results of the analyses indicate that the milling process helped to stabilize the heavy metals in the MEA, with an increase in the specific surface area of about 50 times over that of OPC. The addition of the MEA to the OPC paste decreased the amount of Ca(OH)2 and led to the generation of calcium–silicate–hydrates (C–S–H) which in turned increased the amount of gel pores and middle sized pores in the cement. Furthermore, a comparison shows an increase in the early and later strength over that of OPC paste without the addition of the milled extracted ash. In other words, the milling process could stabilize the heavy metals in the MEA and had an activating effect on the MEA, allowing it to partly substitute OPC in OPC paste.  相似文献   

15.
A step-wise treatment of Municipal Solid Waste (MSW) incinerator fly ash including washing, milling and sintering was investigated in order to manufacture ceramic materials with improved physical, mechanical and environmental properties and, possibly, to reduce the power input of the sintering process. An interpretation of the test results based on the microstructure of sintered products and sintering kinetic modeling was also attempted to identify the densification mechanisms. It was found that milling of washed fly ash represents a basic step for manufacturing high-density ceramic materials with very high compressive strengths (up to 500 N/mm2). A significant reduction in the power input of the sintering process (reduction of firing temperature from 1210 degrees C for washed fly ash to 1140 degrees C for milled-washed fly ash) is also achieved. A dense, well-sintered microstructure is formed through an intermediate-stage, liquid-phase sintering mechanism controlled by liquid-phase diffusion and grain shape accommodation. Such a microstructure is able to strongly immobilise heavy metals, thus giving good environmental properties to sintered product.  相似文献   

16.
The aim of this study was to provide a comprehensive risk assessment for medical waste incineration fly ash from another aspect through various leaching methods. The differences and connections between leaching concentrations achieved via the toxicity characteristic leaching procedure (TCLP), the physiologically based extraction test (PBET) and the sequential extraction procedure were also described. Heavy metal contents of the used medical waste incineration fly ash were 1.7–31 times higher than that from Japan, indicating poor medical waste management in China. The fly ash leaching concentration in the TCLP test exceeded the regulation value and can be characterized as hazardous waste under current regulations. However, the PBET concentrations were only 1/10 of the TCLP value or even lower, and the calculated ingested contents of all heavy metals were lower than tolerable daily intake, demonstrating that TCLP might have overestimated the environment risk to some degree. The leaching metal content of TCLP ranged from exchangeable to residual forms, and the leaching percentage varied from 7.75 to 92.55 %, while the content for PBET was equal to or lower than the exchangeable form.  相似文献   

17.
In the present work, bottom and fly ash, generated from incinerated medical waste, was used as a raw material for the production of geopolymers. The stabilization (S/S) process studied in this paper has been evaluated by means of the leaching and mechanical properties of the S/S solids obtained. Hospital waste ash, sodium hydroxide, sodium silicate solution and metakaolin were mixed. Geopolymers were cured at 50 °C for 24 h. After a certain aging time of 7 and 28 days, the strength of the geopolymer specimens, the leachability of heavy metals and the mineralogical phase of the produced geopolymers were studied. The effects of the additions of fly ash and calcium compounds were also investigated. The results showed that hospital waste ash can be utilized as source material for the production of geopolymers. The addition of fly ash and calcium compounds considerably improves the strength of the geopolymer specimens (2–8 MPa). Finally, the solidified matrices indicated that geopolymerization process is able to reduce the amount of the heavy metals found in the leachate of the hospital waste ash.  相似文献   

18.
Thermal treatment is a promising technology for the fast disposal of hazardous municipal solid waste incineration (MSWI) fly ash in China. However, fly ash produced in grate incinerator (GFA) is rich in CaO and chlorides, which promote the formation of toxic hexavalent chromium [Cr(VI)] and ash agglomeration during the thermal process, inhibiting the thermal disposal of GFA. In this study, sintering characteristics of CaO-rich GFA were improved by adding Si/Al-rich MSWI ash residues. According to the results, ash agglomeration was well suppressed during thermal treatment of the mixed ash. Si/Al/Fe-compounds competed with un-oxidized Cr-compounds to react with CaO and suppressed Cr(VI) formation. Meanwhile, chlorides in GFA facilitated heavy metal volatilization from added ashes to the secondary fly ash, favoring the recovery of these metals. Ca-aluminosilicates was found as the main mineral phase in the thermally treated mixed ash, which has attractive potential for applications. The formation of the aluminosilicates made the heavy metals that remained in the treated mixed ash more stable than the thermally treated single ash.  相似文献   

19.
The objective of this research was to compare the leaching characteristics of heavy metals such as cadmium, chromium, copper, nickel, lead, etc., in Korean and Japanese municipal solid waste incineration (MSWI) ash. The rate of leaching of heavy metal was measured by KSLT and JTL-13, and the amount of heavy metals leached was compared with the metal content in each waste component. Finally, bio-availability testing was performed to assess the risks associated with heavy metals leached from bottom ash and fly ash. From the results, the value of neutralization ability in Japanese fly ash was four times higher than that in Korean fly ash. The reason was the difference in the content of Ca(OH)(2) in fly ash. The amount of lead leached exceeded the regulatory level in both Japanese and Korean fly ash. The rate of leaching was relatively low in ash with a pH in the range of 6-10. The bio-availability test in fly ash demonstrated that the amount of heavy metals leached was Pb>Cd>Cr, but the order was changed to Pb>Cr>Cd in the bottom ash. The leaching concentration of lead exceeded the Japanese risk level in all fly ashes from the two countries, but the leaching concentration of cadmium exceeded the regulatory level in Korean fly ash only.  相似文献   

20.
A five-stage sequential extraction procedure was used to determine the distribution of 11 metals (Cd, Cr, Cu, Mo, Pb, Zn, As, Co, V, Ni, Ba), and sulphur (S) in bottom ash and in fly ash from a fluidized bed co-combustion (i.e. wood and peat) boiler of Stora Enso Oyj Oulu Mill at Oulu, Northern Finland, into the following fractions: (1) water-soluble fraction (H2O); (2) exchangeable fraction (CH3COOH); (3) easily reduced fraction (NH2OH-HCl); (4) oxidizable fraction (H2O2 + CH3COONH4); and (5) residual fraction (HF + HNO3 + HCl). Although metals were extractable in all fractions, the highest concentrations of most of the metals occurred in the residual fraction. From the environmental point of view, this fraction is the non-mobile fraction and is potentially the least harmful. The Ca concentrations of 29.3 g kg(-1) (dry weight) in bottom ash and of 68.5 g kg(-1) (dry weight) in fly ash were correspondingly approximately 18 and 43 times higher than the average value of 1.6 g kg(-1) (dry weight) in arable land in Central Finland. The ashes were strongly alkaline pH (approximately 12) and had a liming effects of 9.3% (bottom ash) and 13% (fly ash) expressed as Ca equivalents (dry weight). The elevated Ca concentrations indicate that the ashes are potential agents for soil remediation and for improving soil fertility. The pH and liming effect values indicate that the ashes also have a pH buffering capacity. From the environmental point of view, it is notable that the heavy metal concentrations in both types of ash were lower than the Finnish criteria for ash utilization.  相似文献   