1.
The goal of this work was to evaluate the effect of chemical modification of cellulose nanofibers (CNF) on the properties of polylactic acid (PLA) nanocomposites. Acetylated nanofibers (ACNF), with degree of substitution 1.07, were isolated from acetylated kenaf fibers by mechanical treatments. Acetylated nanofibers showed more hydrophobic properties compared to non-acetylated ones. The results showed that both crystallinity and thermal stability of acetylated nanofibers were lower than non-acetylated ones. The nanocomposites were prepared by premixing two PLA master batches, one with a high concentration of ACNF and the second with CNF. These were diluted to final concentrations (5?wt%) during the extrusion. The morphology studies of PLA and its nanocomposites showed nanofiber aggregates in both materials. The results showed that the tensile and dynamic mechanical properties were enhanced for both acetylated and non-acetylated nanocomposites compared to the neat PLA matrix while no significant improvement was observed for the acetylated nanocomposites compared to non-acetylated ones. However, the storage modulus increased slightly for acetylated nanocomposites compared to non-acetylated ones.  相似文献   

2.
Biodegradation of poly(lactic) acid (PLA) has been studied extensively, but there is only limited knowledge about the effect of irradiation sterilization on its biodegradability. The aim of this work was to examine the aerobic biodegradation of gamma and electron beam irradiated PLA films along with the effects of aging (3, 6, and 9 months of storage) using a direct measurement respirometric system. Commercial PLA film was exposed to a simulated aerobic compost environment, and its mineralization was 96 % at day 85. Gamma and electron beam irradiation affected the biodegradation of the post-irradiated PLA film. Aging irradiated PLA had some potential to increase the biodegradation rate, as the average value of mineralization after 9 months of storage was higher than for the non-irradiated PLA. Comparison of the effect of storage time on the biodegradability of PLA showed a significant increase in biodegradation of the gamma irradiated PLA after 3 months (70 %) and 9 months of storage (130 %). Similarly, there was a significant difference in the biodegradation of electron beam irradiated PLA between 3 months (68 %) and 9 months of storage (120 %). Due to the priming effect, the percent mineralization of gamma irradiated and E-beam irradiated PLA after 9 months of storage was greater than 100 %. Both non-irradiated and irradiated PLA films can be considered biodegradable plastics since they showed mineralization percentage larger than 90 % of that of the positive control at the end of the test period.  相似文献   

3.
Life cycle analysis (LCA) of limonene plasticized poly(lactic acid) (PLA) films containing cellulose nanocrystals (CNC) extracted, by acid hydrolysis, from Phormium tenax leaf fibres, was assessed and compared with the results of acetyl tributyl citrate (ATBC) plasticized PLA films, having equivalent mechanical properties, containing organo-modified montmorillonite (OMMT). Eco-Indicator 99 tool has been adopted as the main method for life cycle assessment. Results indicated that, despite CNC are biobased fillers obtained by natural sources, the related chemical extraction leads to a large environmental footprint and a relatively relevant energy expense. LCA characterization of these films demonstrated that the environmental impact of PLA/limonene film reinforced with 1% in weight of CNC (PLA/CNC/limonene) is comparable to the environmental impact of polylactic acid films reinforced with OMMT and plasticized with a petroleum based plasticizer (ATBC) (PLA/OMTT/ATBC). A “cradle to gate” approach has been considered for both the film typologies.  相似文献   

4.
In this study, the biodegradation of PLA films using microorganisms from Lake Bogoria (Kenya) were investigated. The biodegradation tests done using certain strains of thermophilic bacteria showed faster biodegradation rates and demonstrated temperature dependency. The biodegradation of the PLA films was studied using Gel Permeation Chromatography (GPC) and light microscopy. The biodegradation of PLA was demonstrated by decrease in molecular weight. The preparation and characterization of PLA/Gum Arabic blends were also investigated using DSC, TGA, TMA and NMR. In summary, the results obtained in this research show that PLA films undergo fast biodegradation using thermophiles isolated from Lake Bogoria. The PLA/GA blends studies show it is possible to prepare films of varying hydrophobic–hydrophilic properties for various applications.  相似文献   

5.
The environmental aging behaviour of montmorillonite (MMT) filled polylactic acid (PLA) nanocomposites (PLA/MMT) and linear low density polyethylene (LLDPE)-toughened PLA (PLA/LLDPE ratio = 90/10) nanocomposites (PLA/LLDPE/MMT) were investigated in this study. The nanocomposites were subjected to water absorption, hygrothermal degradation and soil burial analysis. Both PLA/MMT and PLA/LLDPE/MMT nanocomposites were immersed in distilled water at three different temperatures (room temperature, 60, and 90 °C) and the weight difference before and after immersion was calculated. The kinetics of water absorption for both nanocomposites followed the Fick’s second law of diffusion, where a linear relationship exists between the initial moisture absorption at any time t and t 1/2 (the square root of time), followed by a horizontal plateau (saturation). The equilibrium moisture content (M m ) and diffusion coefficient (D) of PLA nanocomposites increased with the addition of MMT (2 phr) and LLDPE. However, the D values of both nanocomposites decreased by increasing MMT (4 phr). The M m for PLA/MMT and PLA/LLDPE/MMT nanocomposites increased by increasing immersion temperature (60 °C) and prolonged immersion resulted in hygrothermal degradation of both nanocomposites. The hygrothermal degradation studies showed that PLA degrades much faster at 90 °C as compared to 60 °C in both the nanocomposites. The addition of MMT and LLDPE improved the hygrothermal stability of PLA in both nanocomposites. Soil burial test revealed deterioration of impact strength in all samples while the rate of biodegradation was retarded in the presence of MMT and LLDPE.  相似文献   

6.
This paper examines the effect of biobased chitin nanowhisker fillers on the thermal, rheological, physical, mechanical and morphological properties of biobased polylactic acid (PLA) and PLA/polyhydroxybutyrate-co-valerate (PHBV) blended nanocomposites as well as the physical, mechanical and morphological properties of porous PLA and PLA/PHBV nanocomposite foams. Solid nanocomposites of PLA, PLA/PHBV and chitin nanowhiskers were manufactured through melt blending while porous nanocomposites foams were fabricated through a batch foaming process with the aid of CO2 as blowing agent. It was found that by incorporating small quantities of chitin nanowhiskers (<2 wt%) the mechanical properties of solid specimens are improved while strength and expandability of the foam can be significantly improved, yielding a homogenously distributed cell morphology with average cell size of 1.5 μm.  相似文献   

7.
To evaluate the potential of halloysite nanotubes (HNT) as nanofiller for polylactide (PLA), various nanocomposites have been successfully produced by melt-blending the polyester matrix with HNT (HNT(QM)). HNT were also surface treated by silanization reaction with 3-(Trimethoxysilyl) propyl methacrylate (TMSPM). The morphology, thermal, tensile and impact strength properties of the nanocomposites containing 3?C12?% HNT were evaluated and compared to those of pristine (unfilled) PLA. The nanocomposites were characterized by higher rigidity (with Young??s modulus increasing with HNT loading), higher tensile strength (about 70?MPa at 6?% HNT(QM)), whereas the elongation at break and impact strength did not decrease. As demonstrated under dynamic solicitation (DMA), melt-blending PLA with HNT led to enhancement of storage modulus (E??) and offers the possibility to use PLA in applications requiring higher temperatures of utilization. However, with few exceptions, TGA and DSC measurements did not reveal important changes of thermal parameters. The surface silanization treatment proved to improve the quality of the nanofiller dispersion even at higher loading. As a result, good thermal stability associated to high tensile strength, and noticeable increases in impact properties were recorded. Furthermore, enhanced nucleating ability and crystallization kinetics of the PLA matrix were revealed as specific characteristics.  相似文献   

8.
Poly (lactic acid) (PLA) and poly (butylene adipate-co-terephthalate) (PBAT) blend nanocomposites were prepared using melt blending technique followed by compression moulding. The blend nanocomposites were prepared with a variation of PBAT loading along with maleic anhydride and benzoyl peroxide ranging from 5 to 20 wt% along with two different commercially available nanoclays cloisite 93A and cloisite 30B (C30B) at 3 wt% loading. The maleic anhydride and benzoyl peroxide were used during the melt blending of the blend nanocomposites as a compatibilizer and as an accelerator respectively. Maleic anhydride used to enhance the compatibility of the PLA/PBAT blend and as well as the uniform adhesion of the nanoclays with them. The properties and characterizations of PLA matrix and the PLA/PBAT blend nanocomposites have been studied. The tensile strength, % elongation and impact strength increased with the preparation of PLA/PBAT blend nanocomposites as compared with PLA matrix. PLA/PBAT/C30B blend nanocomposites exhibited optimum tensile strength at 15 wt% of PBAT loading. Differential scanning calorimetry and thermogravimetric analysis also showed improved thermal properties as compared with virgin PLA. The wide angle X-ray diffraction studies indicated an increase in d-spacing in PLA/PBAT/C30B blend nanocomposite thus revealing intercalated morphology.  相似文献   

9.
In this study, nanocomposites of PLA and organoclays Cloisite 20A and Cloisite 30B were prepared by the melt intercalation method and the obtained samples were characterized by transmission electron microscopy (TEM). Since composting is an important proposal to the final disposal of biopolymers, the influence of clays on the hydrolytic degradation process of PLA was evaluated by visual analysis and monitoring of molecular weight after periods of 15 and 30 days of degradation in compost. After degradation of the materials in composting environment, the evaluation of cytotoxic, genotoxic and mutagenic effects of compost aqueous extract was carried out using a bioassay with Allium cepa as test organism. The TEM micrographs permitted the observation of different levels of dispersion, including exfoliated regions. In the evaluation of hydrolytic degradation it was noted that the presence of organoclays can decrease the rate of degradation possibly due to the barrier effect of clay layers and/or the higher degree of crystallinity in the nanocomposite samples. Nevertheless, even in the case of nanocomposites, the molecular weight reduction was significant, indicating that the composting process is favorable to the chain scission of PLA in studied materials. In the analysis performed by the bioassay using A. cepa as test organism, it was found that after degradation of the PLA and its nanocomposites the aqueous extract of compost samples induced a decreasing in the mitotic index and an increasing in the induction of chromosomal abnormalities. These results were statistically significant in relation to the negative control (distilled water). By comparing the results obtained for the nanocomposites in relative to pure polymer, there were no statistically significant differences. The types of the observed chromosomal aberrations indicated a possible genotoxic effect of the materials, which may be related to an aneugenic action of PLA degradation products.  相似文献   

10.
The anaerobic biodegradation rates of four different sizes of poly (lactic acid) (PLA) films (thickness 25???m) in anaerobic sludge at 55?°C were examined. The anaerobic biodegradation rates of small pieces of PLA film were slower than for large pieces of PLA film. We also examined whether PLA film could also be used as a reference material in the anaerobic biodegradation test in addition to PLA powder. The anaerobic biodegradation rate of PLA film became slower with lower activity sludge, but the rate of decrease was gradual, and the anaerobic biodegradation rate of PLA film was faster than the PLA powder (125?C250???m). The anaerobic biodegradation rate of the PLA powder (125?C250???m) reflected the plastic anaerobic biodegradation activity of the sludge more accurately than the thin PLA film (thickness 25???m). Consequently, PLA powder (125?C250???m) is more suitable than thin PLA film (thickness?<?25???m) for use as a reference material to assess the plastic anaerobic biodegradation activity of the sludge in an anaerobic biodegradation test at 55?°C.  相似文献   

11.

Polylactic acid (PLA) and thermoplastic starch (TPS) are biodegradable polymers of biological origin, and the mixture of these polymers has been studied due to the desirable mechanical properties of PLA and the low processing cost of TPS. However, the TPS/PLA combination is thermodynamically immiscible due to the poor interfacial interaction between the hydrophilic starch granules and the hydrophobic PLA. To overcome these limitations, researchers studied the modification, processing, and properties of the mixtures as a strategy to increase the compatibility between phases. This review highlights recent developments, current results, and trends in the field of TPS/PLA-based compounds during the last two decades, with the main focus of improving the adhesion between the two components. The TPS/PLA blends were classified as plasticized, compatible, reinforced and with nanocomposites. This article presents, based on published research, TPS/PLA combinations, considering different methods with significant improvements in mechanical properties, with promising developments for applications in food packaging and biomedicine.

  相似文献   

12.
Polylactic acid (PLA) composites comprising up to 25 wt% cotton linter (CL) or up to 50 % maple wood fibre (WF) were prepared by compounding and injection moulding. A reduction of crystallinity in the PLA matrix was observed as a result of the thermal processing method. These PLACL and PLAWF composites provided excellent improvements in both stiffness (with increases in tensile and flexural modulus) and toughness (increases in notched impact strength) properties over the neat PLA resin, while the tensile and flexural strengths of the composites were generally unchanged, while the strain at break values were reduced in comparison to the neat PLA. DMA results indicated incorporating these fibres caused the mechanical loss factor (tan δ) to decrease, suggesting better damping capabilities were achieved with the composites. SEM analysis of the impact fractured surfaces of the PLACL composites showed debonding-cavitation at the matrix-fibre interface while the PLAWF composites showed good wetting along its matrix-fibre interface. The composting of these composites up to 90 days showed that the degradation onset time was increased when increasing the fibre loadings, but the maximum degree of degradation and the maximum daily rates of degradation were decreased compared to neat PLA. On a weight basis of fibre loading, the PLACL composites had a quicker onset of biodegradation, a higher maximum daily rate of biodegradation and, overall, a higher degree of biodegradation at 90 days than the PLAWF composites, possibly due to the quicker thermal hydrolysis observed in the PLA matrix of the PLACL composites during processing and composting.  相似文献   

13.
In this study, surface modification is used to improve the compatibility of Kenaf fibers (KFs) and multi-walled carbon nanotubes (MWCNTs) in a polylactic acid (PLA) matrix, as well as to enhance the mechanical properties. Through the use of a silane coupling agent, the KF is grafted with functional groups to generate a chemical bond with the PLA; the modified KF shows high compatibility in the PLA matrix. Compared to the bare PLA, the optimal KF/MWCNT/PLA composite (PC1F30-OX) shows increases of 58% in tensile strength, and 113% in impact strength. A small addition of MWCNTs (1 wt%) dramatically improves the antistatic ability by lowering the surface resistance to 3.47 GΩ. With the addition of hydrophilic KF into the PLA, the composite becomes much more environmentally friendly, and the biodegradation rate can be controlled by the amount of KF added. The addition of hydrophilic KF allowed the composite to accommodate more enzyme to hasten the biodegradation; almost complete decomposition occurred after 11 weeks.  相似文献   

14.
This paper investigated the influence of TiO2 nanoparticles on the morphologies, as well as crystallization behaviour and kinetics, of neat PLA and PCL, and of these polymers in different PLA/PCL blends. We used transmission electron microscopy to evaluate the morphologies of the systems, while the crystallization behaviour and kinetics were investigated through differential scanning calorimetry (DSC). In addition to standard and modulated (StepScan) DSC analyses, the self-nucleation temperatures of neat PCL and PCL in the different nanocomposites were determined, followed by a self-nucleation and annealing thermal fractionation analysis of PCL crystallization and an Avrami isothermal kinetic analysis of PCL crystallization and PLA cold crystallization. We found that the nanoparticles were well dispersed, but only in the PLA phase of the blends, with only a few on the interface or in the PCL phase. They did nucleate and accelerate, and influence the mechanism of, the PCL crystallization in neat PCL, but had little influence on PCL crystallization in the blends. They strongly influenced the rate of cold crystallization of PLA, but had little influence on this parameter in the blends. The tensile properties were also determined, and changes in these properties could be related to the morphologies of the systems.  相似文献   

15.
Polylactic acid (PLA) is one of the important biodegradable polymers. It is widely used in many industrial applications such as films and fibers. Its biodegradability is based on data derived mostly from composting processes. For a broad application of the PLA material in personal care products, an understanding of anaerobic biodegradability is essential because soiled personal care products are usually disposed of in sanitary landfills, where biodegradability mechanisms are predominately in anaerobic conditions. Extensive laboratory results are acquired to elucidate the effects of the temperature on the PLA anaerobic sludge biodegradation. When the temperature is higher than PLA glass transition temperature (Tg), anaerobic degradation is accelerated. A plausible mechanism to explain this observation is that amorphous part of the polymer is easily accessible by microorganisms. When the degrading temperature is below PLA glass transition temperature, sample mineralization under anaerobic conditions is apparently slowed. The mechanisms elucidated by Tg modification can be utilized to control the rate of PLA biodegradation for sustainable waste management.  相似文献   

16.
This study presents the effect of biodegradation, in a composting medium, on properties of membrane-like crosslinked and noncrosslinked polyvinyl alcohol (PVA) and nanocomposites. The composting was carried out for 120 days and the biodegradation of these materials was characterized using various techniques. The changes in the PVA resin and nanocomposite surface topography and microstructure during composting were also characterized. The results from the analyses suggest biodegradation of PVA based materials in compost medium was mainly by enzymes secreted by fungi. The results also indicate that the enzymes degraded the amorphous regions of the specimens first and that the PVA crystallinity played an important role in its biodegradation. The surface roughness of the specimens was seen to increase with composting time as the microbial colonies grew which in turn facilitated further microorganism growth. All specimens broke into small pieces between 90 and 120 days of composting as a result of deep biodegradation. Glyoxal and malonic acid crosslinking decreased the PVA biodegradation rate slightly. Addition of highly crystalline microfibrillated cellulose and naturally occurring halloysite nanotubes in PVA based nanocomposites also decreased the biodegradation rate. The three factors: PVA crystallinity, crosslinking and additives, may be utilized effectively to extend the life of these materials in real life applications.  相似文献   

17.
Nano-biocomposites based on a biodegradable bacterial copolyester, poly(hydroxybutyrate-co-hydroxyvalerate), have been elaborated with an organo-modified montmorillonite (OMMT) clay as nanofiller, and acetyl tributyl citrate as plasticizer. The corresponding (nano)structures, thermal and mechanical properties, permeability, and biodegradability have been determined. Polyhydroxyalkanoates are very thermal sensitive then to follow the degradation the corresponding matrices have been analyzed by size exclusion chromatography. The results indicate that the addition of the plasticizer decreases the thermo-mechanical degradation, during the extrusion. These nano-biocomposites show an intercalated/exfoliated structure with good mechanical and barrier properties, and an appropriated biodegradation kinetic. Intending to understand the changes in the thermal properties, the nano-biocomposites were characterized by thermal gravimetric analysis and differential scanning calorimetry. The presence of the OMMT clay did not influence significantly the transition temperatures. However, the filler not only acted as a nucleating agent which enhanced the crystallization, but also as a thermal barrier, improving the thermal stability of the biopolymer. The results indicated that the addition of the plasticizer reduces the glass transition temperature and the crystalline melting temperature. The plasticizer acts as a processing aid and increases the processing temperature range (lower melting temperature).  相似文献   

18.
The biodegradability of polylactide (PLA) and gelatinized starches (GS) blend films in the presence of compatibilizer was investigated under controlled soil burial conditions. Various contents (0–40 wt%) of corn and tapioca starches were added as fillers; whereas, different amounts of methylenediphenyl diisocyanate (MDI) (0–2.5 wt%) and 10 wt% based on PLA content of polyethylene glycol 400 (PEG400) were used as a compatibilizer and a plasticizer, respectively. The biodegradation process was followed by measuring changes in the physical appearance, weight loss, morphological studies, and tensile properties of the blend films. The results showed that the presence of small amount of MDI significantly increased the tensile properties of the blends compared with the uncompatibilized blends. This is attributed to an improvement of the interfacial interaction between PLA and GS phases, as evidenced by the morphological results. For soil burial testing, PLA/GS films with lower levels (1.25 wt%) of MDI had less degradation; in contrast, at high level of MDI, their changes of physical appearance and weight loss tended to increase. These effects are in agreement with their water absorption results. Furthermore, biodegradation rates of the films were enhanced with increasing starch contents, while mechanical performances were decreased.  相似文献   

19.
In this study, the hydrolytic degradation of Poly(lactic acid) (PLA) and acetylated PLA (PLA-Ac)–clay nanocomposites were investigated. The organo clay was obtained by ion exchange reaction using cetyl tri methyl ammonium bromide (CTAB). Nanocomposites containing 2, 5 and 8% mass ratio of organo clay (CTAB-O) were prepared. PLA and its organo clay nanocomposites were characterized by scanning electron microscope (SEM), thermo gravimetric analysis (TGA) and X-ray diffraction (XRD) to determine the morphology before and after hydrolytic degradation. Fourier transform infrared (FTIR) analyses of PLA and PLA-Ac were also obtained. The hydrolytic degradation of polymers and their composites were investigated in the phosphate buffered saline solution (PBS). The results showed that controlled hydrolytic degradation was observed in the samples with end group modification of PLA. While weight loss of PLA films was 28%, that of PLA-Ac films was 18% after 60 days degradation time. The weight loss was obtained as 29.5 and 25.5% for PLA-5 wt% organo clay (PLA/5CTAB-O) and PLA-Ac-5 wt% organo clay (PLA-Ac/5CTAB-O) nanocomposites films, respectively. It was also observed that thermal degradation of PLA-Ac was much more than that of PLA. Hydrolytic degradation increased depending on organo clay content. The end group modificated PLA results in controlled hydrolytic degradation. While hydrolytic degradation in polymer films occurred as surface erosion, bulk erosion was observed in composite films.  相似文献   

20.
Poly(lactic acid) (PLA) has gained considerable attention nowadays as a biocompatible polymer owing to its advantage of being prepared from renewable resources. PLA exhibits excellent tensile strength, fabricability, thermal plasticity and biocompatibility properties comparable to many petroleum based plastics. However, low heat distortion temperature, brittleness and slow crystallization rate limit the practical applications of PLA. In order to address these limitations, an attempt has been made in the current work to prepare binary blends of PLA with ethylene vinyl acetate (EVA) at different compositions via melt mixing technique. Systematic investigation on the mechanical properties, thermal degradation and crystallization behavior for PLA-EVA blends was carried out. The impact strength of binary blends of PLA–EVA was found to increase significantly by 176% for 15 wt% of EVA compared to virgin PLA. This is due to the strong interfacial adhesion among PLA and EVA resulting in brittle to ductile transition. Scanning electron microscopy analysis for impact fractured surfaces of binary blends of PLA implied the toughening effect of PLA by EVA. Thermogravimetry analysis results revealed that the activation energy of PLA–EVA blends decreased with increase in EVA content in the PLA matrix. While, differential scanning calorimetry results obtained for PLA–EVA blends revealed the improvement in crystallinity when compared with neat PLA. The effect of EVA on non-isothermal melt crystallization kinetics of PLA was also examined via DSC at various heating rates. Decreasing trend in the t1/2 values indicated the faster rate of crystallization mechanism after addition of EVA in the PLA matrix.  相似文献   