1.
The rheologies, morphologies, crystallization behaviors, mechanical and thermal properties of poly(lactic acid) (PLA)/polypropylene (PP) blends and PLA/PP/maleic anhydride-grafted PP (MAPP) blends were investigated. The results showed that the complex viscosities of PLA/PP blends were between those of neat PLA and neat PP, and MAPP had a thinning effect on those of the blends. PLA/PP blends exhibited the distinct phase separation morphologies due to the limited partial miscibility of the blend components. MAPP slightly improved the miscibility between PLA and PP. Both the cold crystallization of PLA component and melt crystallization of PP component were enhanced, probably because PLA and PP were reciprocal nucleating agents. The tensile strength and flexural modulus decreased, while the tensile strain at break and heat deflection temperature (HDT) increased with the increasing PP content. MAPP had the positive effects on the notched impact strength and HDT of PLA-rich blends and also increased the flexural modulus of the binary blends. The thermal stability of the blend was improved by PP, and the incorporation of MAPP further enhanced the thermal stability.  相似文献   

2.
Natural composites have been important materials system due to preservation of earth environments. Natural fibers such as jute, hemp, bagasse and so on are very good candidate of natural composites as reinforcements. On the other hand regarding matrix parts thermosetting polymer and thermoplastic polymer deriver form petrochemical products are not environmental friendly material, even if thermoplastic polymer can be recycled. In order to create fully environmental friendly material (FEFM) biodegradable polymer which can be deriver from natural resources is needed. Therefore poly(lactic acid) (PLA) polymer is very good material for the FEFM. In this paper jute fiber filled PLA resin (jute/PLA) composites was fabricated by injection moldings and mechanical properties were measured. It is believable that industries will have much attention to FEFM, so that injection molding was adopted to fabricate the composites. Long fiber pellet fabricated by pultrusion technique was adopted to prepare jute/PLA pellet. Because it is able to fabricate composite pellets with relative long length fibers for injection molding process, where, jute yarns were continuously pulled and coated with PLA resin. Here two kinds of PLA materials were used including the one with mold releasing agent and the other without it. After pass through a heated die whereby PLA resin impregnates into the jute yarns and sufficient cooling, the impregnated jute yarns were cut into pellets. Then jute/PLA pellets were fed into injection machine to make dumbbell shape specimens. In current study, the effects of temperature of PLA melting temperature i.e. impregnation temperature and the kinds of PLA were focused to get optimum molding condition. The volume fractions of jute fiber in pellet were measured by several measuring method including image analyzing, density measurement and dissolution methods. Additionally, thermal and mechanical properties were investigated. It is found that 250° is much suitable for jute/PLA long fiber pultrusion process because of its less heat degradation of jute, better impregnation, acceptable mechanical property and higher production efficiency. Additionally the jute fibers seem much effective to increase deflection temperature under load, tensile modulus and Izod strength.  相似文献   

3.
Poly(l-lactic acid) (PLLA)/poly(caprolactone) (PCL) and two types of organoclay (OMMT) including a fatty amide and ocatdecylamine montmorillonite (FA-MMT and ODA-MMT) were employed to produce polymer nanocomposites by melt blending. Materials were characterized using X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, thermogravimetric analysis (TGA), elemental analysis, scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Mechanical properties were also investigated for these nanocomposites. The nanocomposites showed increasing mechanical properties and thermal stability. XRD results indicated that the materials formed nanocomposites. SEM morphology showed that increasing content of OMMT reduced the domain size of phase separated particles. TEM outcomes have confirmed the intercalated type of nanocomposite. Additionally, a solution casting process has been used to prepare these nanocomposites and characterized to compare these results with the above process.  相似文献   

4.
This is, to our knowledge, the first study of wheat-gluten-based nanocomposite films prepared by a solvent-free extrusion process. Wheat gluten/montmorillonite nanocomposite films were obtained in a single screw-extruder using urea as a combined denaturant and plasticizer. The oxygen permeability and water vapor transmission rate of the films decreased by respectively factors of 1.9 and 1.3 when 5 wt.% clay was added. At the same time, the stiffness increased by a factor of 1.5, without any critical loss of extensibility. Field emission scanning electron microscopy (FE-SEM) and Energy-dispersive X-ray analysis indicated that the clay particles were layered mainly in the plane of the extruded film. It was possible to identify individual platelets/tactoids with FE-SEM and, together with findings from transmission electron microscopy, atomic force microscopy and X-ray diffraction, it was concluded that the clay existed as individual clay platelets, intercalated tactoids and agglomerates. Thermogravimetric analysis showed that the thermal stability of the extrudates was improved by the addition of clay.  相似文献   

5.
Polylactic acid (PLA)/starch fibers were produced by twin screw extrusion of PLA with granular or gelatinized starch/glycerol followed by drawing through a set of winders with an intermediate oven. At 30% starch, fibers drawn 2–5x were highly flexible (elongation 20–100%) while undrawn filaments were brittle (elongation 2–9%). Tensile strength and moduli increased with increasing draw ratio but decreased with increasing starch content. Mechanical properties were better for composites made with gelatinized starch/glycerol than granular starch. In conclusion, orientation greatly increases the flexibility of PLA/starch composites and this may be useful not only in fibers but also possibly in molded articles. Other advantages of starch addition could include fiber softness without added plasticizer, moisture/odor absorbency and as a carrier for active compounds.  相似文献   

6.
Journal of Polymers and the Environment - Poly ε-caprolactone (PCL) synthesized by ring-opening polymerization method, and then it blended with polylactic acid (PLA). The blend was loaded with...  相似文献   

7.
In this study, the hydrolytic degradation of Poly(lactic acid) (PLA) and acetylated PLA (PLA-Ac)–clay nanocomposites were investigated. The organo clay was obtained by ion exchange reaction using cetyl tri methyl ammonium bromide (CTAB). Nanocomposites containing 2, 5 and 8% mass ratio of organo clay (CTAB-O) were prepared. PLA and its organo clay nanocomposites were characterized by scanning electron microscope (SEM), thermo gravimetric analysis (TGA) and X-ray diffraction (XRD) to determine the morphology before and after hydrolytic degradation. Fourier transform infrared (FTIR) analyses of PLA and PLA-Ac were also obtained. The hydrolytic degradation of polymers and their composites were investigated in the phosphate buffered saline solution (PBS). The results showed that controlled hydrolytic degradation was observed in the samples with end group modification of PLA. While weight loss of PLA films was 28%, that of PLA-Ac films was 18% after 60 days degradation time. The weight loss was obtained as 29.5 and 25.5% for PLA-5 wt% organo clay (PLA/5CTAB-O) and PLA-Ac-5 wt% organo clay (PLA-Ac/5CTAB-O) nanocomposites films, respectively. It was also observed that thermal degradation of PLA-Ac was much more than that of PLA. Hydrolytic degradation increased depending on organo clay content. The end group modificated PLA results in controlled hydrolytic degradation. While hydrolytic degradation in polymer films occurred as surface erosion, bulk erosion was observed in composite films.  相似文献   

8.
Epoxy resin prepared by the reaction of a diglycidyl ether of bisphenol A (DGEBA) and m-xylylenediamine (m-XDA) was modified with 10% wt of epoxidized palm oil (EPO). The EPO was first pre-polymerized with m-XDA at various temperatures and reaction times. The resulting product was then mixed with the epoxy resin at 40?°C and allowed to react at 120?°C for another 3?h. The fully reacted DGEBA/m-XDA/EPO blend was characterized by using scanning electron microscopy (SEM), differential scanning calorimetry (DSC), thermal gravimetric analysis, tensile test, hardness indentation and dynamic mechanical analysis. The SEM study shows that different types of morphology, ranging from phase separated to miscible blends were obtained. A miscible blend was obtained when the m-XDA and EPO were reacted for more than 2?h. The results from DSC analysis show that the incorporation of EPO at 10% wt in the epoxy blend reduced the glass transition temperature (T g). The lowered T g and mechanical properties of the modified epoxy resins are caused by a reduction in crosslinking density and plasticizer effect.  相似文献   

9.
Novel polymer blends based on completely renewable polymers were reported. Polymer blends based on polylactic acid (PLA) and oxidized and hydroxylated soya bean oil polymers were prepared. Plasticization and mechanical strength effect of the soya bean oil polymers on the PLA were observed. Fracture surface analysis of the polymer blends was carried out by using scanning electron microscopy. The PLA blends showed more amorphous morphologies compared to pure PLA. The blends had better elongation at break in view of the stress–strain measurement. Blend of PLA with the hydroxylated polymeric soya bean oil indicated the slightly antibacterial properties.  相似文献   

10.
Poly (lactic acid) (PLA) and poly (butylene adipate-co-terephthalate) (PBAT) blend nanocomposites were prepared using melt blending technique followed by compression moulding. The blend nanocomposites were prepared with a variation of PBAT loading along with maleic anhydride and benzoyl peroxide ranging from 5 to 20 wt% along with two different commercially available nanoclays cloisite 93A and cloisite 30B (C30B) at 3 wt% loading. The maleic anhydride and benzoyl peroxide were used during the melt blending of the blend nanocomposites as a compatibilizer and as an accelerator respectively. Maleic anhydride used to enhance the compatibility of the PLA/PBAT blend and as well as the uniform adhesion of the nanoclays with them. The properties and characterizations of PLA matrix and the PLA/PBAT blend nanocomposites have been studied. The tensile strength, % elongation and impact strength increased with the preparation of PLA/PBAT blend nanocomposites as compared with PLA matrix. PLA/PBAT/C30B blend nanocomposites exhibited optimum tensile strength at 15 wt% of PBAT loading. Differential scanning calorimetry and thermogravimetric analysis also showed improved thermal properties as compared with virgin PLA. The wide angle X-ray diffraction studies indicated an increase in d-spacing in PLA/PBAT/C30B blend nanocomposite thus revealing intercalated morphology.  相似文献   

11.
The concern related to solid waste increases efforts to develop products based on biodegradable materials. At present, PLA has one of the highest potentials among biopolyesters, particularly for packaging. However, its application is limited in some fields. In order to optimize PLA properties, organo-modified montmorilonites have been extensively used to obtain nanocomposites. Although PLA nanocomposites studies are widely reported in the literature, there is still few information about the influence of organoclays on de biodegradation process, which is a relevant information, since one of the main purposals related to the final disposal of biopolymers as PLA is composting. Besides, in the last years some research has been conducted in order to evaluate the potential toxicity of montmorilonite, unmodified or organo-modified. Since the use of montmorilonite is expanding in different applications, human exposure and risk assessment are important issues to be investigated. In this context, this review intends to compile available information related to common organoclays used for PLA nanocomposites, its properties, biodegradation analysis and potential toxicity evaluation of nanocomposites, focused on montmorilonite as filler. Two issues of relevance were pointed out. The first is food safety and quality, and the second consideration is the environmental effect.  相似文献   

12.
Extrusion-coating experiments were carried out in the pilot line at Tampere Univesity of Technology (Institute of Paper Converting). Typical paper and paperboard substrates were coated with commercially produced 3-hydroxybutyrate/3-hydroxyvalerate. The resulting physical properties of extrusion-coated composite structures were studied. Adhesion between PHB/V and a fiber-based substrate was rather poor, regardless of typically used pretreatments (corona and flame). On the other hand, adhesion was sufficient (mode of failure was fiber tear as the materials were separated) when the substrate was primed with an acrylic-based primer. The surface energy and polarity of PHB/V were much higher than the respective ones of LDPE. Curling of PHB/V was reduced by the addition of wax or tall oil rosin into the base polymer.  相似文献   

13.
This paper investigates and compares the performances of polylactic acid (PLA)/kenaf (PLA-K) and PLA/rice husk (PLA-RH) composites in terms of biodegradability, mechanical and thermal properties. Composites with natural fiber weight content of 20% with fiber sizes of less than 100 μm were produced for testing and characterization. A twin-screw extrusion was used to compound PLA and natural fibers, and extruded composites were injection molded to test samples. Flexural and Izod impact test, TGA, soil burial test and SEM were used to investigate properties. All results were compared to a pure PLA matrix sample. The flexural modulus of the PLA increased with the addition of natural fibers, while the flexural strength decreased. The highest impact strength (34 J m−1), flexural modulus (4.5 GPa) and flexural strength (90 MPa) were obtained for the composite made of PLA/kenaf (PLA-K), which means kenaf natural fibers are potential to be used as an alternative filler to enhance mechanical properties. On the other hand PLA-RH composite exhibits lower mechanical properties. The impact strength of PLA has decreased when filled with natural fibers; this decrease is more pronounced in the PLA-RH composite. In terms of thermal stability it has been found that the addition of natural fibers decreased the thermal stability of virgin PLA and the decrement was more prominent in the PLA-RH composite. Biodegradability of the composites slightly increased and reached 1.2 and 0.8% for PLA-K and PLA-RH respectively for a period of 90 days. SEM micrographs showed poor interfacial between the polymer matrix and natural fibers.  相似文献   

14.
This study is focused on the preparation, characterization, and determination of thermal properties and thermal reliability of paraffin/polypropylene (PP) composite as a novel form-stable phase change material (PCM) for thermal energy storage applications. In the composite, paraffin acts as a PCM when PP is operated as supporting material. The composites prepared at different mass fractions of paraffin (50, 60, 70, 80, and 90 w/w%) by solution casting method were subjected to leakage test by heating the composites over the melting temperature of the PCM. The paraffin/PP composite (70/30 w/w%) is found as the maximum paraffin containing composite and was characterized using Fourier transform infrared spectroscopy, optic microscopy, differential scanning calorimetry (DSC), and thermal gravimetric analysis (TGA) techniques. DSC analysis indicated that the form-stable paraffin/PP composite melts at 44.77–45.52 °C and crystallizes at 53.55–54.80 °C. It has latent heats of 136.16 and −136.59 J/g for melting and crystallization, respectively. These thermal properties make it potential PCM for latent heat thermal energy storage (LHTES) purposes such as solar space heating applications. Accelerated thermal cycling tests indicated that the form-stable PCM had good thermal reliability. TGA also showed that the form-stable PCM degrades in two distinguishable steps and had good chemical stability.  相似文献   

15.
The objective of this work was to improve the impact and thermal properties of polylactic acid (PLA)-based biocomposite by appropriate application of cellulosic fiber and a bioelastomer. Biocomposites formulations with fiber contents of up to 20% in combination with a bioelastomer were extrusion-compounded in a twin-screw extruder followed by molding in an injection molding system. Fibers used in the formulations included three types of cellulosic fiber; namely, raw fiber from oat hull biomass (RF), hydrolysis byproduct (ATF) which was the solid fraction obtained from an acid-catalyzed hydrolysis of RF, and delignified fibers (AD30, AD65, AD100) which were the products of delignification of ATF. Formulated biocomposites were characterized for thermal (glass transition and melting temperatures, and enthalpy of melting) and physico-mechanical (tensile and bending strengths, stiffness, impact energy, and water absorption) properties. Among all types of biofibers, RF resulted in poor properties in the biocomposites due to the high hemicellulose content in the structure. On the other hand, the ratio of lignin to cellulose (in the absence of hemicellulose) in the modified fibers did not significantly affect the physico-mechanical and thermal properties of the biocomposites. The elastomer applied in the formulations improved the impact energy, thermal properties, and elongation at break of the composites. However, it adversely affected the strength and water resistance of biocomposites, especially in the presence of hemicellulose. The results indicated that, depending on the application, a wide range of PLA green composites with different physico-mechanical properties can be achieved.  相似文献   

16.
Elongation properties of extruded cornstarch were improved by blending with glycerol. Further blending of starch-glycerol with polyvinyl alcohol (PVOH) resulted in significant improvements in both tensile strength (TS) and elongation at break. Samples of starch-glycerol without PVOH equilibrated at 50% relative humidity had a TS of 1.8 MPa and elongation of 113%, whereas those containing PVOH had a TS and elongation of 4 MPa and 150%, respectively. Dynamic mechanical analysis (DMA) of starch-glycerol-PVOH blends showed that decreases in glass transition temperatures (T g values) were proportional to glycerol content. Scanning electron microscopy (SEM) of fractured surfaces revealed numerous cracks in starch-glycerol (80:20) samples. Cracks were absent in starch-glycerol (70:30) samples. In both blends, many starch granules were exposed at the surface. No exposed starch granules were visible in blends with added PVOH. Starch-glycerol samples incubated in compost lost up to 70% of their dry weight within 22 days. Addition of PVOH lowered both the rate and extent of biodegradation.  相似文献   

17.
In this study water soluble sodium carboxymethyl cellulose (CMC) was blended with high density polyethylene (HDPE) by peroxide-initiated melt compounding technique. The compatibility of the blended polymers were carried out by silane crosslinking agent. A series of blends were prepared by varying the CMC contents up to a maximum of 50 phr. The physical properties of non-crosslinked and crosslinked blends were investigated in detail. FTIR analysis of crosslinked blend confirmed the presence of Si–O–Si and Si–O–C absorption peaks at 1050 and 1159 cm?1. Thermal stability of crosslinked blends improved as compared to its non-crosslinked congener. Rheological study of crosslinked blends illustrated high complex viscosity and dynamic shear storage modulus. The tensile strength of virgin polyethylene was 8.1 MPa whereas the maximum tensile strength of 19.6 MPa was observed in crosslinked blend. Similarly lower deformation was observed in crosslinked blends under static load. Scanning electron microscopy of crosslinked formulations also showed strong adhesion between the polymers interface. The compatibility of HDPE and CMC is attributed to both free radical and condensation reactions.  相似文献   

18.
“Green”/bio-based blends of poly(lactic acid) (PLA) and cellulolytic enzyme lignin (CEL) were prepared by twin-screw extrusion blending. The mechanical and thermal properties and the morphology of the blends were investigated. It was found that the Young’s modulus of the PLA/CEL blends is significantly higher than that of the neat PLA and the Shore hardness is also somewhat improved. However, the tensile strength, the elongation at break, and the impact strength are slightly decreased. Thermogravimetric analysis (TGA) shows that the thermal stability of the PLA is not significantly affected by the incorporation of the CEL, even with 40 wt% CEL. The results of FT-IR and SEM reveal that the CEL and the PLA are miscible and there are efficient interactions at the interfaces between them. These findings show that the CEL is a kind of feasible filler for the PLA-based blends.  相似文献   

19.
Polylactic acid (PLA) has been modified by electron beam radiation in the presence of glycidyl methacrylate (GMA) to enhance the melt strength of PLA. The modified PLA was prepared by varying both the amount of GMA and the irradiation dose and was characterized by observing the thermal properties, the melt viscoelastic properties and the gel fraction. For comparison, virgin PLA was also irradiated. All irradiated virgin PLA had a lower complex viscosity and a storage modulus compared to virgin PLA due to irradiation-induced chain scission. However, these properties were remarkably improved due to formation of long chain branching and retarding chain scission if GMA was introduced in this system. The increase in melt viscoelastic property was much dependent on the irradiation dose. At optimum doses of radiation, it showed maximum complex viscosity and storage modulus. The PLA irradiated with 20 kGy in the presence of 3 phr GMA showed a complex viscosity of about 10 times higher and a storage modulus of 100 times higher than those of virgin PLA at 0.1 rad/s. Gel fraction measurement revealed that chain scission and branching was more dominant than crosslinking. The biodegradability of irradiated PLA was slightly decreased by the presence of GMA.  相似文献   

20.
Journal of Polymers and the Environment - In this study, a biodegradable wheat gluten (WG) film containing calcium chloride and nano silica (WG/CaCl2/SiO2) was prepared and the physicochemical...  相似文献   