分析铜渣组成结构和形貌特性的基础上,研究了铜渣与含砷污酸反应行为及脱砷规律,阐明了反应动力学过程,揭示了铜渣除砷机理.结果表明:在铜渣用量为0.2g/mL,反应温度为23℃,反应时间为24h的最优条件下,铜渣的最大去除容量达到25.89mg/g,除砷率达到99.56%,并且除砷后铜渣的砷浸出浓度低于5mg/L的危险废弃物界定限值,属于一般固体废弃物.铜渣除砷过程符合拟二级动力学模型,该过程受铁离子释放速度限制,离子交换吸附和化学沉淀方式同步进行实现了砷的脱除,两种方式的结合有利于砷的稳定化.铜渣与污酸反应释放大量的铁离子,通过离子交换吸附与砷酸根离子发生沉淀反应,形成较为稳定的砷酸盐及其衍生化合物,进而达到除砷目的.铜渣表现出优越的除砷性能,为重有色冶炼污酸处置提供了一种高效和低成本的方法.  相似文献   

2.
生命周期评价是判断生产工艺是否真正属于清洁生产范畴的基本方法,为了对铜渣回收工艺的清洁生产评价提供依据,有必要对铜渣回收工艺进行生命周期评价。据此对国内铜渣的回收现状和对钢铁、锌、镁、铬渣、再生铜和电解铜的生产工艺生命周期评价现状进行研究。研究表明:用统计方法和SimaPro7.1软件,通过Eco-indicator99生态指数法,对铜渣回收工艺进行生命周期评价有很好的应用前景。  相似文献   

3.
水淬渣作吸附剂处理含铜冶炼工业废水的研究   总被引:6,自引:0,他引:6  
研究了以水淬渣为吸附剂对含Cu(Ⅱ)的铜冶炼工业废水进行处理。实验结果表明,在不调节铜冶炼废水pH值的条件下,水淬渣用量为0.05g/mL,作用时间为30min,温度为25℃,Cu(Ⅱ)的去除率达96.91%,处理后的水符合国家污水综合排放标准(GB8978-1996)一级标准,达到以废治废的目的。  相似文献   

4.
文章阐述了目前国内外对干法脱硫渣综合利用的现状,以胶凝材料学以及水泥化学为理论基础,将干法脱硫渣中的物质划分为三类,并提出在充分激发其活性的基础上,对干法脱硫渣进行高技术附加值的利用,并详细阐述了其原理和途径。  相似文献   

5.
工业固体废物生命周期管理方法及案例分析   总被引:2,自引:1,他引:1       下载免费PDF全文
通过分析工业固体废物管理过程与工业生产过程间的耦合关系,提出了涵盖减量化过程的工业固体废物生命周期管理框架和方法,并应用于铜渣管理的方案评估与决策过程中.结果表明,铜渣3种不同管理方案的环境负荷值依次为2800.46,2156.00,2162.04Pt.与熔池熔炼法相比,闪速熔炼法虽有利于铜渣的源头减量,但其减少的铜渣量并未导致精铜生产与铜渣管理全过程环境影响的整体下降.单从铜渣的内部再循环工艺来看,处理同样数量的铜渣,选矿法的环境表现优于电炉贫化法.案例研究证实了工业固体废物管理应将减量化过程纳入全生命周期管理方案中进行综合评估,而非简单遵循废物管理的优先顺序和等级制度.  相似文献   

6.
吴龙  吴华峰  吴跃东  贾少华  王会刚 《环境工程》2020,38(9):190-193,88
我国高温熔渣年产生量超过6亿t,其热资源价值巨大,但浪费情况严重。对干法粒化、化学法、冷却水余热利用、直接制备产品4种熔渣热能利用技术进行了论述探讨。熔渣热能回收技术的应用离不开熔渣资源利用,综合经济效益最大化是热能利用技术应用的关键因素。对于高温熔渣热回收技术建议如下:针对活性物料含量低的熔渣采用干法粒化、化学法进行热能回收;活性物料含量高的熔渣,在确保熔渣产品活性的条件下进行热能回收技术开发;因地制宜地进行冲渣冷却水余热利用;解决熔渣直接制备产品的关键工艺技术难点,提质降本;加强熔渣液固转变矿物结构变化过程的研究,实现固化渣的矿物组成调控。  相似文献   

7.
论述了对诺砂采用压制成型法试制低成本地面砖的工艺流程、试验过程及其结果分析,并对其反应机理进行了简单的探讨,为诺砂的综合利用提供了一定的参考.  相似文献   

8.
采用配碳还原和熔融造渣方法回收铜渣中铁和铜,研究了CaO、Al2O3、CaF2、Na2CO3成分对铁和铜回收效果的影响。在碳氧比1.5和1 450℃条件下,CaO加入量约30%时,铁和铜的回收率较高,分别是93.85%和92.73%。实验表明:添加Al2O3、Na2CO3均降低铁和铜的回收效果,使渣中含铁量增加;CaF2添加量小于2%时,有利于铜渣中铁的回收,CaF2添加量较大时不利于铁和铜的回收。  相似文献   

9.
对新余钢铁公司0~10 mm的细粒钢渣干式磁选分离所得到的产品进行扫描电镜检测、分析,找出了影响细粒钢渣干式磁选指标难以得到提高的原因,用于指导生产实践。研究结果表明:钢渣在干式磁选过程中,包裹有微细粒的金属铁或与金属铁连生的浮氏体以及具有一定磁性的铁酸盐容易进入磁性分离物中,这些物质自身铁品位较低,从而造成了磁性分离物中铁品位的降低。  相似文献   

10.
用偏高岭石、铜矿尾砂、粉煤灰生产土聚水泥试验   总被引:1,自引:0,他引:1  
胡旭亮  成岳  苏晓渊 《环保科技》2011,17(1):37-40,43
以偏高岭石和固体废物铜矿尾砂、粉煤灰为基料,以氢氧化钠、水玻璃等作为激发剂,在室温条件下制备土聚水泥。通过正交试验,研究不同基料配比、激发剂、外加剂的不同加入量等因素对试条抗压强度的影响,并确定最优配方;同时通过SEM观察了土聚水泥的形貌并研究了土壤聚合的反应机理。结果表明:其最佳配方中铜矿尾砂、粉煤灰的质量比之和接近60%,7天抗压强度比标号为P.O42.5的水泥高5%;该土聚水泥呈层状结构,缝隙较小,结构紧密。  相似文献   

11.
A mathematical model was developed to estimate the weight percent of diamond abrasive particles incorporated in nickel binder matrix during abrasive microtool fabrication by pulse-plating process. The proposed model is based on the hypothesis that, embedment of an inert micro abrasive diamond particle on the substrate will only occur when a few nickel ions from the adsorbed ionic cloud are chemically reduced at the cathode by hydrogen ions present in the diffusion layer. Experimental verification of the model developed was performed by pulse electroplating of diamond abrasive particles on tungsten micro tool shank using an in-house built experimental setup. The predictive model developed was found to estimate diamond abrasive content in nickel binder matrix within 1–7 wt% of experimental results for different pulse-plating conditions.  相似文献   

12.
钢渣深处理技术   总被引:1,自引:0,他引:1  
瞿仁静 《云南环境科学》2010,29(5):63-65,81
以昆钢本部及红钢所产的转炉钢渣作为研究对象,研究热泼钢渣的矿物组成,分析钢渣中有价金属的组成,确定不同的粒级、不同的磁场强度,采用干式磁选与湿式磁选相结合的“一段闭路破碎,磁滑轮磁选;一段开路磨矿,一粗一精选别”深度处理流程,应用于红钢钢渣磁选车间及昆钢钢渣磁选厂,获得良好的磁选指标。分析了项目实施过程中渣浆输送断流的原因,找出解决办法。总结了项目产生的效益。  相似文献   

13.
文章采用WPI水污染指数法评价滇池北岸各片区河道的水质,并分析其变化趋势,同时采用pearson相关分析方法研究旱季和雨季各片区河道WPI指数变化趋势的相关度。结果表明:1988-2001年滇池北岸河道水质污染主要为减轻的趋势;2001-2007年随着昆明市的大规模扩张,其加重趋势非常明显;2007-2009年,随着河道水环境综合整治工程的大规模开展,又主要表现为减轻趋势,且旱季水质污染减轻的趋势比雨季明显,在纳入统计的5个片区河道中,旱季有4个片区河道水质好转,雨季有3个片区河道水质好转。这是由于2007-2009年间开展的河道水环境综合整治工程主要针对点源污染控制。此外,由于面源污染特征在5个片区中的4个片区都非常相似,雨季各片区河道WPI指数变化趋势的相关度比旱季高。  相似文献   

14.
The Langat River in Malaysia has been experiencing anthropogenic input from urban, rural and industrial activities for many years. Sewage contamination, possibly originating from the greater than three million inhabitants of the Langat River Basin, were examined. Sediment samples from 22 stations (SL01-SL22) along the Langat River were collected, extracted and analysed by GC-MS. Six different sterols were identified and quantified. The highest sterol concentration was found at station SL02 (618.29 ng/g dry weight), which situated in the Balak River whereas the other sediment samples ranged between 11.60 and 446.52 ng/g dry weight. Sterol ratios were used to identify sources, occurrence and partitioning of faecal matter in sediments and majority of the ratios clearly demonstrated that sewage contamination was occurring at most stations in the Langat River. A multivariate statistical analysis was used in conjunction with a combination of biomarkers to better understand the data that clearly separated the compounds. Most sediments of the Langat River were found to contain low to mid-range sewage contamination with some containing `significant' levels of contamination. This is the first report on sewage pollution in the Langat River based on a combination of biomarker and multivariate statistical approaches that will establish a new standard for sewage detection using faecal sterols.  相似文献   

15.
拉拉铜矿区土壤重金属含量及其污染特征   总被引:2,自引:0,他引:2  
分析了拉拉铜矿区土壤中重金属含量,并运用地积指数对其污染状况进行了评价。结果表明,拉拉矿区是Cu、Cd、Hg污染严重的区域,而Cr、Pb、As污染不明显。与中国土壤元素背景值相比,矿区土壤中Hg含量平均增加了13.4倍,Cd含量平均增加了19.5倍,Cu含量平均增加了4.9倍。运用Muller地积指数进行评价,证明拉拉矿区Cd属于强-极强污染;Hg属于强污染;Cu以中等污染为主,部分强污染;Cr属于无-中污染;Pb以无污染为主;As属于无污染。矿区土壤重金属污染程度由高到低依次为:Cd>Hg>Cu>Cr>Pb>As。建议重视矿区Cu、Cd、Hg等重金属的污染问题,加强重金属的生态健康效应研究。  相似文献   

16.
为了优化镍转炉渣加压条件下H2SO4选择性浸出Co、Ni、Cu,抑制Fe浸出的工艺,采用响应曲面法的中心组合设计原理,建立影响选择性浸出率的二次多项式数学模型,研究浸出温度、c(H2SO4)及液固比及上述因素两两交互作用对提高Co、Ni、Cu浸出率及减少Fe浸出率的影响规律. 结果表明:浸出温度和c(H2SO4)对浸出率影响最显著,液固比次之. c(H2SO4)越高,Co、Ni、Cu和Fe的浸出率越高,而提高浸出温度有利于降低Fe浸出率. 响应曲面法优化获得的最佳工艺条件:浸出温度为210 ℃、c(H2SO4)为0.38 mol/L、液固比为4.25 mL/g,在该条件下,Co和Ni的浸出率均大于98%,Cu浸出率大于96%,Fe浸出率小于0.4%. 浸出控制参数优化后提高了有价金属的浸出率,同时也降低了Fe浸出率,实现了镍转炉渣中有价金属的回收及其与Fe的高效分离.   相似文献   

17.
城市控制爆破安全工作的探讨   总被引:5,自引:0,他引:5  
本文从爆破安全的评估,设计,审查,施工组织和监测等过程对城市控制爆破的安全性进行分析,并提出安全技术措施。  相似文献   

18.
以硫化砷渣为原料,用氯化铜酸性溶液浸出砷渣的全湿法进行实验,着重研究氯化铜浸出砷的过程中氯化铜用量、溶液p H和浸出时间对砷浸出率的影响,探讨用氯化亚锡还原砷盐酸溶液从硫化砷渣得到单质砷的方法。  相似文献   

19.
君安矿区复垦土壤的环境质量分析与评价   总被引:1,自引:0,他引:1  
以君安矿区复垦土壤为调查研究对象,分析了该矿区不同复垦基质的主要重金属污染元素Pb、Cu、Cd和Cr的含量,并采用三步评价法对该矿不同区域复垦土壤的环境质量进行了分析与评价。结果表明:君安矿西区、东区复垦土壤环境质量合格,北区、南区和中区复垦土壤均不符合我国土壤环境质量标准;通过将矿区与全国土壤背景值进行比较可知,矿区复垦土壤未受到重金属Cu的污染,受Cd、Cr的污染较轻,受Pb的污染较严重。该研究可为进一步确定矿区土壤复垦方向提供依据。  相似文献   

20.
The steel industry is characterised by large amounts of CO2 emissions, but there is no easy means to reduce these emissions. One interesting option for the reduction of CO2 emissions could be the utilisation of steelmaking slags for carbon dioxide mineralisation. In this option CO2 is bound with the calcium of the slag material, producing stable carbonate as an end product. The utilisation of steelmaking slags as the raw material for carbon dioxide mineralisation will change the quality of the slags. If, however, this change degrades the slags it could prevent the use of slags in carbon dioxide mineralisation or make it very expensive.The purpose of the research presented here is to evaluate this issue with the help of a case study where the quality of the residual slag from the recently suggested carbonation method was experimentally investigated. The CO2 mineralisation method, based on steelmaking slags and ammonium salt solutions, was found to change the quality of the slags: the calcium content was reduced, the CaO and Ca(OH)2 phases were completely dissolved, and the solubility of the V and Cr increased notably. This residual slag would presumably have to be handled as waste. Currently, the steelmaking slag used in the case study is defined as a by-product, but if it is used for CO2 mineralisation instead of liming its legal status will be re-evaluated. Subsequently, the CO2 mineralisation process could possibly be defined as an end-of-waste procedure.  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号