首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 31 毫秒
1.
Pyrolysis and steam gasification of woody biomass chip (WBC) obtained from construction and demolition wastes, refuse-derived fuel (RDF), and refuse paper and plastic fuel (RPF) were performed at various temperatures using a lab-scale instrument. The gas, liquid, and solid products were examined to determine their generation amounts, properties, and the carbon balance between raw material and products.The amount of product gas and its hydrogen concentration showed a considerable difference depending on pyrolysis and steam gasification at higher temperature. The reaction of steam and solid product, char, contributed to an increase in gas amount and hydrogen concentration. The amount of liquid products generated greatly depended on temperature rather than pyrolysis or steam gasification. The compositions of liquid product varied relying on raw materials used at 500 °C but the polycyclic aromatic hydrocarbons became the major compounds at 900 °C irrespective of the raw materials used. Almost fixed carbon (FC) of raw materials remained as solid products under pyrolysis condition whereas FC started to decompose at 700 °C under steam gasification condition.For WBC, both char utilization by pyrolysis at low temperature (500 °C) and syngas recovery by steam gasification at higher temperature (900 °C) might be practical options. From the results of carbon balance of RDF and RPF, it was confirmed that the carbon conversion to liquid products conspicuously increased as the amount of plastic increased in the raw material. To recover feedstock from RPF, pyrolysis for oil recovery at low temperature (500 °C) might be one of viable options. Steam gasification at 900 °C could be an option but the method of tar reforming (e.g. catalyst utilization) should be considered.  相似文献   

2.
Pyrolysis of sewage sludge was studied in a free-fall reactor at 1000–1400 °C. The results showed that the volatile matter in the sludge could be completely released to gaseous product at 1300 °C. The high temperature was in favor of H2 and CO in the produced gas. However, the low heating value (LHV) of the gas decreased from 15.68 MJ/N m3 to 9.10 MJ/N m3 with temperature increasing from 1000 °C to 1400 °C. The obtained residual solid was characterized by high ash content. The energy balance indicated that the most heating value in the sludge was in the gaseous product.  相似文献   

3.
The effects of temperature on the release of chemical components of six solid organic materials under conditions of oversaturation were investigated in this paper. The six materials were peat moss (PM), weathered coals (WC), charred rice husks (CRH), sawdust (Sd), turfgrass clippings (TC), and chicken manure (CM). Significant differences were observed in the available nitrogen and phosphorus content of the aqueous extracts of organic materials at different temperatures. The available nitrogen content in aqueous extracts of PM and WC at 25 °C was higher than that registered at 15 °C and 35 °C. Available nitrogen content in the aqueous extracts of CRH, Sd, TC, and WC at 35 °C was higher than at 15 °C and 25 °C. The available phosphorus content in the aqueous extracts of organic materials at 35 °C was higher than that available at 15 °C and 25 °C, with the exception of Sd. In addition, the release of available phosphorus in the aqueous solution of organic materials at different temperatures varied constantly for 108 h. The release of potassium (K+) and sodium (Na+) ions in the aqueous extracts of organic materials was basically steady over time, with the exception of CM. High temperature (35 °C) may significantly hasten the release of K+ from organic substrates (except for WC) with low temperatures significantly inhibiting release of K+ in Sd and CRH. High temperatures (35 °C) might significantly facilitate the release of Na+ in CM and TC. However, no significant differences were manifested in the release of Na+ from organic substrates at different temperatures, with the exception of CM and TC. Moreover, no significant differences were observed in the release of calcium, magnesium and iron ions with time, nor were there any significant differences in the contents of iron ions in the aqueous extracts of organic materials at different temperatures. The results indicate that multiple mediums should be pretreated in water for a week before being used for planting. They should be used when all mineral elements of organic materials are steady and ignoring the effect of organic mediums.  相似文献   

4.
Upcycling polymer wastes into useful, and valuable carbon based materials, is a challenging process. We report a novel catalyst-free and solvent-free technique for the formation of nano channeled ultrafine carbon tubes (NCUFCTs) and multiwalled carbon nanotubes (MWCNTs) from polyethylene terephthalate (PET) wastes, using rotating cathode arc discharge technique. The soot obtain from the anode contains ultrafine and nano-sized solid carbon spheres (SCS) with a mean diameter of 221 nm and 100 nm, respectively, formed at the lower temperature region of the anode where the temperature is approximately 1700 °C. The carbon spheres are converted into long “Y” type branched and non-branched NCUFCTs and MWCNTs at higher temperature regions where the temperature is approximately 2600 °C, with mean diameters of 364 nm and 95 nm, respectively. Soot deposited on the cathode is composed of MWCNTs with a mean diameter of 20 nm and other nanoparticles. The tubular structures present in the anode are longer, bent and often coiled with lesser graphitization compared to the nanotubes in the soot on the cathode.  相似文献   

5.
Pyrolysis of aseptic packages (tetrapak cartons) in a laboratory apparatus using a flow screw type reactor and a secondary catalytic reactor for tar cracking was studied. The pyrolysis experiments were realized at temperatures ranging from 650 °C to 850 °C aimed at maximizing of the amount of the gas product and reducing its tar content. Distribution of tetrapak into the product yields at different conditions was obtained. The presence of H2, CO, CH4, CO2 and light hydrocarbons, HCx, in the gas product was observed. The Aluminum foil was easily separated from the solid product. The rest part of char was characterized by proximate and elemental analysis and calorimetric measurements. The total organic carbon in the tar product was estimated by elemental analysis of tars. Two types of catalysts (dolomite and red clay marked AFRC) were used for catalytic thermal tar decomposition. Three series of experiments (without catalyst in a secondary cracking reactor, with dolomite and with AFRC) at temperatures of 650, 700, 750, 800 and 850 °C were carried out. Both types of catalysts have significantly affected the content of tars and other components in pyrolytic gases. The effect of catalyst on the tetrapack distribution into the product yield on the composition of gas and on the total organic carbon in the tar product is presented in this work.  相似文献   

6.
In this work, a Brønsted acidic ionic liquid, 1-butyl-3-methyl-imidazolium hydrogen sulfate ([bmim]HSO4), was used to leach copper from waste printed circuit boards (WPCBs, mounted with electronic components) for the first time, and the leaching behavior of copper was discussed in detail. The results showed that after the pre-treatment, the metal distributions were different with the particle size: Cu, Zn and Al increased with the increasing particle size; while Ni, Sn and Pb were in the contrary. And the particle size has significant influence on copper leaching rate. Copper leaching rate was higher than 99%, almost 100%, when 1 g WPCBs powder was leached under the optimum conditions: particle size of 0.1–0.25 mm, 25 mL 80% (v/v) ionic liquid, 10 mL 30% hydrogen peroxide, solid/liquid ratio of 1/25, 70 °C and 2 h. Copper leaching by [bmim]HSO4 can be modeled with the shrinking core model, controlled by diffusion through a solid product layer, and the kinetic apparent activation energy has been calculated to be 25.36 kJ/mol.  相似文献   

7.
Time domain reflectometry (TDR) is a prospective measurement technology for moisture content of sewage sludge composting material; however, a significant dependence upon temperature has been observed. The objective of this study was to assess the impacts of temperature upon moisture content measurement and determine if TDR could be used to monitor moisture content in sewage sludge compost across a range of temperatures. We also investigated the combined effects of temperature and conductivity on moisture content measurement. The results revealed that the moisture content of composting material could be determined by TDR using coated probes, even when the measured material had a moisture content of 0.581 cm3 cm?3, temperature of 70 °C and conductivity of 4.32 mS cm?1. TDR probes were calibrated as a function of dielectric properties that included temperature effects. When the bulk temperature varied from 20 °C to 70 °C, composting material with 0.10–0.70 cm3 cm?3 moisture content could be measured by TDR using coated probes, and calibrations based on different temperatures minimized the errors.  相似文献   

8.
Several animal (lamb, poultry and swine) fatty wastes were pyrolyzed under nitrogen, in a laboratory scale fixed-bed reactor and the main products (liquid bio-oil, solid bio-char and syngas) were obtained. The purpose of this study is to produce and characterize bio-oil and bio-char obtained from pyrolysis of animal fatty wastes. The maximum production of bio-oil was achieved at a pyrolysis temperature of 500 °C and a heating rate of 5 °C/min. The chemical (GC–MS analyses) and spectroscopic analyses (FTIR analyses) of bio-oil showed that it is a complex mixture consisting of different classes of organic compounds, i.e., hydrocarbons (alkanes, alkenes, cyclic compounds…etc.), carboxylic acids, aldehydes, ketones, esters,…etc. According to fuel properties, produced bio-oils showed good properties, suitable for its use as an engine fuel or as a potential source for synthetic fuels and chemical feedstock. Obtained bio-chars had low carbon content and high ash content which make them unattractive for as renewable source energy.  相似文献   

9.
In this work, a product distribution study from thermal degradation of low-density polyethylene (LDPE) is presented. Thermal degradation of the polymer was investigated under dynamic condition in an inert environment using a thermo-gravimetric analyzer (TGA) coupled with evolved products’ analysis using a gas chromatograph (GC). Fractions evolved at nine different temperatures from 200 to 600 °C were injected into GC for a detailed product analysis. The main objective of the present investigation is to highlight the species-specific evolution profiles of LDPE pyrolyzates (C5–C44) at different stages of its degradation under an inert environment. Pyrograms have been analyzed in terms of amount of different products evolved at various pyrolysis temperatures. Volatile pyrolyzates essentially remain low at low decomposition temperature (200–300 °C) of the polymer, which gradually increase to attain a maximum at maximum decomposition temperature (470 °C) and finally level off at 600 °C. In the mechanistic approach adopted to understand the decomposition mechanism of LDPE, the following reaction types were considered: (a) main chain cleavage to form chain-terminus radicals; (b) intramolecular hydrogen transfer to generate internal radicals; (c) intermolecular hydrogen transfer to form both volatile products and radicals; and (d) β-scission to form both volatiles and terminally unsaturated polymer.  相似文献   

10.
A thermodynamic calculation was carried out to predict the behavior and speciation of heavy metals (HMs), Pb, Zn, Cu, and Cd, during municipal solid waste (MSW) incineration with the different moisture levels. The calculation was based on the minimization of the total Gibbs free energy of the multi-components and multi-phases closed system reaching chemical equilibrium. The calculation also indicated the reaction directions and tendencies of HMs components. The impacts of chlorine additives (No PVC, 1%PVC, and 5%PVC) and moisture on the behavior of HMs were investigated at different temperature levels in the system (750 °C, 950 °C, and 1150 °C). Furthermore, because the incineration temperature falls down with the increase in moisture in waste, the co-influence of moisture and temperature in combusting MSW on the HMs was also studied with the given chlorine (as 1%PVC + 0.5%NaCl). The results showed that in the non-chlorine system, the impact of the moisture on Pb, Zn, and Cu was not significant, and the ratio of compound transformation was less than 10%, except the Cd compounds at 950 °C and 1150 °C. In the system with low chlorine (as 1%PVC) at constant temperature, the chlorides of HMs (Cd, Pb, Zn, and Cu) transferred to oxides, and when the content of chlorine rose up (as 5%PVC), the ratio of the chlorides of HMs (Cd, Pb, Zn, and Cu) transferring to oxides fell down noticeably. When the moisture varied together with the temperature, the Zn and Cu compounds transferred from chlorides to oxides with increase in moisture as well as decrease in temperature. At the temperature of 700–1000 °C, the impact of temperature on Pb and Cd was little and the moisture was the main factor; while at the temperature of 1000–1200 °C, the impact of increase in moisture and decrease in temperature on Pb and Cd was almost equal and reversed.  相似文献   

11.
Lead can be recovered from funnel glass of waste cathode ray tubes via reduction melting. While low-temperature melting is necessary for reduced energy consumption, previously proposed methods required high melting temperatures (1400 °C) for the reduction melting. In this study, the reduction melting of the funnel glass was performed at 900–1000 °C using a lab-scale reactor with varying concentrations of Na2CO3 at different melting temperatures and melting times. The optimum Na2CO3 dosage and melting temperature for efficient lead recovery was 0.5 g per 1 g of the funnel glass and 1000 °C respectively. By the reduction melting with the mentioned conditions, 92% of the lead in the funnel glass was recovered in 60 min. However, further lead recovery was difficult because the rate of the lead recovery decreased as with the recovery of increasing quantity of the lead from the glass. Thus, the lead remaining in the glass after the reduction melting was extracted with 1 M HCl, and the lead recovery improved to 98%.  相似文献   

12.
Simultaneous recovery of vanadium (V) and nickel (Ni), which are classified as two of the most hazardous metal species from power plant heavy fuel fly-ash, was studied using a hydrometallurgical process consisting of acid leaching using sulfuric acid. Leaching parameters were investigated and optimized in order to maximize the recovery of both vanadium and nickel. The independent leaching parameters investigated were liquid to solid ratio (S/L) (5–12.5 wt.%), temperature (45–80 °C), sulfuric acid concentration (5–25 v/v%) and leaching time (1–5 h). Response surface methodology (RSM) was used to optimize the process parameters. The most effective parameter on the recovery of both elements was found to be temperature and the least effective was time for V and acid concentration for Ni. Based on the results, optimum condition for metals recovery (actual recovery of ca.94% for V and 81% for Ni) was determined to be solid to liquid ratio of 9.15 wt.%, temperature of 80 °C, sulfuric acid concentration of 19.47 v/v% and leaching time of 2 h. The maximum V and Ni predicted recovery of 91.34% and 80.26% was achieved.  相似文献   

13.
Cellulose/polyethylene (CPE) mixture 3:1, w/w with and without three clay catalysts (K10 – montmorillonite K10, KSF – montmorillonite KSF, B – Bentonite) addition were subjected to pyrolysis at temperatures 400, 450 and 500 °C with heating rate of 100 °C/s to produce bio-oil with high yield. The pyrolytic oil yield was in the range of 41.3–79.5 wt% depending on the temperature, the type and the amount of catalyst. The non-catalytic fast pyrolysis at 500 °C gives the highest yield of bio-oil (79.5 wt%). The higher temperature of catalytic pyrolysis of cellulose/polyethylene mixture the higher yield of bio-oil is. Contrarily, increasing amount of montmorillonite results in significant, almost linear decrease in bio-oil yield followed by a significant increase of gas yield. The addition of clay catalysts to CPE mixture has a various influence on the distribution of bio-oil components. The addition of montmorillonite K10 to cellulose/polyethylene mixture promotes the deepest conversion of polyethylene and cellulose. Additionally, more saturated than unsaturated hydrocarbons are present in resultant bio-oils. The proportion of liquid hydrocarbons is the highest when a montmorillonite K10 is acting as a catalyst.  相似文献   

14.
Sulfur recirculation is a new technology for reducing boiler corrosion and dioxin formation. It was demonstrated in full-scale tests at a Waste to Energy plant in Göteborg (Sweden) during nearly two months of operation. Sulfur was recirculated as sulfuric acid from the flue gas cleaning back to the boiler, thus creating a sulfur loop.The new technology was evaluated by extensive measurement campaigns during operation under normal conditions (reference case) and operation with sulfur recirculation. The chlorine content of both fly ash and boiler ash decreased and the sulfur content increased during the sulfur recirculation tests. The deposit growth and the particle concentration decreased with sulfur recirculation and the dioxin concentration (I-TEQ) of the flue gas was reduced by approximately 25%. Sulfuric acid dew point measurements showed that the sulfuric acid dosage did not lead to elevated SO3 concentrations, which may otherwise induce low temperature corrosion.In the sulfur recirculation corrosion probe exposures, the corrosion rate decreased for all tested materials (16Mo3, Sanicro 28 and Inconel 625) and material temperatures (450 °C and 525 °C) compared to the reference exposure. The corrosion rates were reduced by 60–90%. Sulfur recirculation prevented the formation of transition metal chlorides at the metal/oxide interface, formation of chromate and reduced the presence of zinc in the corrosion products. Furthermore, measured corrosion rates at 525 °C with sulfur recirculation in operation were similar or lower compared to those measured at 450 °C material temperature in reference conditions, which corresponds to normal operation at normal steam temperatures. This implies that sulfur recirculation allows for higher steam data and electricity production without increasing corrosion.  相似文献   

15.
An attempted has been made to recover high-calorific fuel gas and useful carbonaceous residue by the electric arc pyrolysis of waste lubricating oil. The characteristics of gas and residues produced from electric arc pyrolysis of waste lubricating oil were investigated in this study. The produced gas was mainly composed of hydrogen (35–40%), acetylene (13–20%), ethylene (3–4%) and other hydrocarbons, whereas the concentration of CO was very low. Calorific values of gas ranged from 11,000 to 13,000 kcal kg?1 and the concentrations of toxic gases, such as NOx, HCl and HF, were below the regulatory emissions limit. Gas chromatography–mass spectrometry (GC/MS) analysis of liquid-phase residues showed that high molecular-weight hydrocarbons in waste lubricating oil were pyrolyzed into low molecular-weight hydrocarbons and hydrogen. Dehydrogenation was found to be the main pyrolysis mechanism due to the high reaction temperature induced by electric arc. The average particle size of soot as carbonaceous residue was about 10 μm. The carbon content and heavy metals in soot were above 60% and below 0.01 ppm, respectively. The utilization of soot as industrial material resources such as carbon black seems to be feasible after refining and grinding.  相似文献   

16.
This study was performed to suggest the improvements through measuring the amounts of polychlorinated dibenzo-p-dioxins (PCDDs) and polychlorinated dibenzofurans (PCDFs), re-synthesized in peripheral utilities (PUs) of a commercial-scale municipal solid waste incineration facility (MSWIF) where a few research results existed. The PUs examined in this study consisted of air pre-heaters (APHs) and gas/gas re-heater (GGRH) and kerosene-fired duct burner for selective catalytic reduction (SCR) process. PCDDs/PCDFs in flue gas were simultaneously measured at the inlet and outlet of PUs.Flue gas was cooled down from 380 °C to 249 °C by exchanging the heat with fresh air in APHs, and then heated up to 383 °C by GGRH and duct burner from 164 °C at the outlet of bag filter. The results showed that PCDDs/PCDFs were 3–4 times higher within this temperature range of PUs. In comparison of PCDDs/PCDFs concentrations at the inlet with those at the outlet of PUs, particulate-phase PCDDs/PCDFs were about 9.5–10 times enriched while gaseous-phase ones were decreased by about 33–41%. The PCDDs/PCDFs re-synthesized in the PUs, where PCDDs were relatively higher than PCDFs, showed somewhat different patterns compared to those formed at incinerators and emitted at stack. Through the investigations for PUs, we conclude that the PUs used in MSWIFs was a potential source for de novo synthesis of PCDDs/PCDFs.  相似文献   

17.
Lab-scale experiments were conducted to assess the impact of thermobarical treatment of cattle waste on anaerobic digestion. Treatment was at temperatures of 140–220 °C in 20 K steps for a 5-min duration. Methane yields could be increased by up to 58% at a treatment temperature of 180 °C. At 220 °C the abundance of inhibitors and other non-digestible substances led to lower methane yields than those obtained from untreated material. In an extended analysis it could be demonstrated that there is a functional correlation between the methane yields after 30 days and the formation rate and methane yield in the acceleration phase. It could be proved in a regression of these correlation values that the optimum treatment temperature is 164 °C and that the minimum treatment temperature should be above 115 °C.  相似文献   

18.
In this study, biodegradation of low-density polyethylene (LDPE) by isolated landfill-source fungi was evaluated in a controlled solid waste medium. The fungi, including Aspergillus fumigatus, Aspergillus terreus and Fusarium solani, were isolated from samples taken from an aerobic aged municipal landfill in Tehran. These fungi could degrade LDPE via the formation of a biofilm in a submerged medium. In the sterilized solid waste medium, LPDE films were buried for 100 days in a 1-L flask containing 400 g sterile solid waste raw materials at 28 °C. Each fungus was added to a separate flask. The moisture content and pH of the media were maintained at the optimal levels for each fungus. Photo-oxidation (25 days under UV-irradiation) was used as a pretreatment of the LDPE samples. The progress of the process was monitored by measurement of total organic carbon (TOC), pH, temperature and moisture. The results obtained from monitoring the process using isolated fungi under sterile conditions indicate that these fungi are able to grow in solid waste medium. The results of FT-IR and SEM analyses show that A. terreus and A. fumigatus, despite the availability of other organic carbon of materials, could utilize LDPE as carbon source. While there has been much research in the field of LDPE biodegradation under solid conditions, this is the first report of degradation of LDPE by A. fumigatus.  相似文献   

19.
The use of abundant waste materials with high carbohydrate content may contribute substantially to reduction of biofuels production cost. The present study aimed at optimizing the combined effect of thermo-chemical pretreatment and enzymatic hydrolysis of kitchen wastes (KW) for maximizing the production of fermentable soluble sugars. To this end, acid pretreatment of KW samples was performed with hydrochloric acid (0–3% HCl) at 30–100 °C for 0–120 min treatment time. Alternatively, alkaline pretreatment of KW samples was performed with potassium hydroxide solution (0–11%) at constant temperature and time (0 °C and 20 min, respectively). KOH pretreatment at such conditions targets to degrade the resistant starch of KW samples. Both acid and alkaline pretreatments were followed by addition of variable levels of enzyme dosage (0–3.6% v/v α-amylase and 0–3.2% v/v amyloglucosidase-AMG) at constant pH, temperature and time (pH = 5, T = 50 °C and t = 30 min, respectively). Based on our results, glucose concentration increased by ~300% after pretreatment with either acid or KOH in combination with enzymatic hydrolysis (2% HCl, 85 °C, 80 min, 0.1% α-amylase, AMG, and 1% KOH, 0 °C, 20 min, 1.1% α-amylase, 0.4% AMG) compared to raw (untreated) KW. Estimating the different YG yields at KW loading of 5%, an increase of 192% and 121% for total soluble monosugars and total soluble sugars, respectively, was succeeded compared to untreated KW. The effect of solids loading on the obtained sugar yields using the optimum conditions for thermo-chemical pretreatment followed by enzymatic hydrolysis was also tested resulting to 27.5% increase of the soluble glucose yield when half of the solids loading (2.5%) was used. A decrease of total soluble sugars yield by 32.2% was observed when solely acid hydrolysis at optimum conditions from our previous study was applied at 30% solids loading.  相似文献   

20.
The rising popularity of incineration of municipal solid waste (MSW) calls for detailed mathematical modeling and accurate prediction of pollutant emissions. In this paper, mathematical modeling methods for both solid and gaseous phases were employed to simulate the operation of a 450 t/d MSW-burning incinerator to obtain detailed information on the flow and combustion characteristics in the furnace and to predict the amount of pollutant emissions. The predicted data were compared to on-site measurements of gas temperature, gas composition and SNCR de-NOX system. The major operating conditions considered in this paper were grate speed and oxygen concentration. A suitable grate speed ensures complete waste combustion. The predictions are as follows: volatile release increases with increasing grate speed, and the maximal value is within the range of 700–800 kg/m2 h; slow grate speeds result in incomplete combustion of fixed carbon; the gas temperature at slow grate speeds is higher due to adequate oxygenation for fixed carbon combustion, and the deviation reaches 200 K; NOX emission decreases, but CO emission and O2 concentrations increase, and the deviation is 63%, 34% and 35%, respectively. Oxygen-enriched atmospheres promote the destruction of most pollutants due to the high oxygen partial pressure and temperature. The furnace temperature, NO production and CO emission increase as the oxygen concentration increases, and the deviation of furnace exit temperature, NO and CO concentration is 38.26%, 58.43% and 86.67%, respectively. Finally, oxygen concentration is limited to below 35% to prevent excessive CO and NOX emission without compromising plant performance. The current work greatly helps to understand the operating characteristics of large-scale MSW-burning plants.  相似文献   