1.
Wet-air oxidation of diluted black liquor (chemical oxygen demand [COD] approximately 3250 to 14 500 mg/L) was performed at mild operating conditions (temperature = 388 to 423 K and total pressure = 0.6 MPa) in the presence of heterogeneous 60% copper oxide (CuO)/ 40% cerium oxide (CeO2) catalyst. Maximum COD reduction of 77.3% was obtained at 423 K at pH 3.0, which was marginally higher than that obtained at 413 K temperature (77.1%). In the acidic environment (pH < or = 3), most of the COD was removed in the form of settleable solids during the transient heating of the wastewater from room temperature to the desired one. The solid residue obtained after the reaction has a heating value of 20.1 MJ/kg, which is comparable with that of Indian coal. Thermal degradation kinetic determination suggested that thermal characteristics of the solid residue are well represented by a power law model with Agarwal and Sivasubramanian approximation (Safi et al., 2004).  相似文献   

2.
The present study was performed to investigate the performance of activated carbon-supported copper and manganese base catalyst for catalytic wet oxidation (CWO) of pulping effluent. CWO reaction was performed in a high pressure reactor (capacity?=?0.7 l) at temperatures ranging from 120 to 190 °C and oxygen partial pressures of 0.5 to 0.9 MPa with the catalyst concentration of 3 g/l for 3 h duration. With Cu/Mn/AC catalyst at 190 °C temperature and 0.9 MPa oxygen partial pressures, the maximum chemical oxygen demand (COD), total organic carbon (TOC), lignin, and color removals of 73, 71, 86, and 85 %, respectively, were achieved compared to only 52, 51, 53, and 54 % removals during the non-catalytic process. Biodegradability (in terms of 5-day biochemical oxygen demand (BOD5) to COD ratio) of the pulping effluent was improved to 0.38 from an initial value of 0.16 after the catalytic reaction. The adsorbed carbonaceous fraction on the used catalyst was also determined which contributed meager TOC reduction of 3–4 %. The leaching test showed dissolution of the metals (i.e., Cu and Mn) from the catalysts in the wastewater during CWO reaction at 190 °C temperature and 0.9 MPa oxygen partial pressures. In the future, the investigations should focus on the catalyst reusability.  相似文献   

3.
Chang DJ  Chen IP  Chen MT  Lin SS 《Chemosphere》2003,52(6):943-949
Wet air oxidation of a prepared reactive dye solution was performed to assess the efficacy of CoAlPO(4)-5 and CeO(2) as catalysts in the reaction. Via adsorption and oxidation of dye, CoAlPO(4)-5 effectively decreased American Dye Manufacturers Institute and chemical oxygen demand (COD) values in the dye solution. At a reaction temperature of 135 degrees C and an applied pressure of 1.0 MPa, color and COD removal were as high as 95% and 90%, respectively, after 2 h. Active sites on the outer surface of CoAlPO(4)-5 are responsible for adsorption and decomposition of dye while active sites in the pores dominate further destruction and oxidation of intermediate products. Since the outer surface only represents a minor part of the total surface, the color removal does not increase appreciably with loading of CoAlPO(4)-5. The CeO(2) catalyst, calcined from cerium chloride under high thermal impact (type A CeO(2)) was very effective in removing color and COD from the solution. This catalyst demonstrated near 100% color removal at temperatures above 135 degrees C and the COD removal could be above 95% at 165 degrees C. With both CoAlPO(4)-5 and CeO(2) catalysts, COD rose and then fell back during the reaction, a feature typical of a consecutive reaction. In contrast to prepared CeO(2), a commercial CeO(2) did not exhibit any catalytic ability for the removal of color and COD. The durability of both CoAlPO(4)-5 and prepared CeO(2) is considered to be fair.  相似文献   

4.
通过浸渍法制备CuO/SBA-15和CuO-CeO2/SBA-15两种介孔材料催化剂,采用BET、XRD、TPR和XPS等对催化剂进行表征,重点考察催化剂对萘氧化反应的催化活性及对产物CO2的选择性。BET、XRD和XPS等实验结果表明CuO高度分散于介孔分子筛SBA-15中,CeO2可促进CuO在载体上的分散,同时能降低催化剂的TPR还原温度。活性测试结果表明CuO/SBA-15对萘氧化反应的催化活性较高,但是催化氧化的CO2选择性较低,温度在380℃时CO2的生成率仅为60%左右;CeO2的添加不仅提高了CO2的生成率,15%CuO-15%CeO2/SBA-15在325℃使CO2生成率达到99%,而且CeO2增强了催化剂的稳定性。  相似文献   

5.
为了综合利用废椰壳,进行了废椰壳制备活性炭并负载氧化铜处理活性艳红X-3B废水的研究。采用正交实验法,以COD和色度去除率为目标函数确定了活性炭的最佳制备工艺条件为:磷酸浓度65%(质量百分数),m(磷酸)/m(椰壳)比3∶1,活化时间2.5 h,活化温度500℃。在该活性炭上负载氧化铜处理活性艳红X-3B染料废水,其COD和色度去除率分别为83.70%和99.72%。用扫描电镜(SEM)和X衍射仪(XRD)对裸活性炭和载铜活性炭样品表面形貌和结构进行了表征和分析。通过单因素实验法确定了废水处理的最佳工艺条件为:pH值5,曝气时间4 h和催化剂用量0.55 g,在此条件下,COD和色度去除率分别为86.70%和99.75%,相应的出水指标为75 mg/L和32稀释倍数。  相似文献   

6.
通过活性炭负载CuO和CeO2来制备吸附剂,采用固定床吸附方式,在不同反应条件下对吸附剂的吸附性能进行测试,筛选出去除效率最好的吸附剂,并通过BET和XRD对吸附剂的理化性质进行分析。结果表明,CuO和CeO2的加入大大改变了原活性炭的比表面积和孔结构,改善了活性炭的吸附性能。CuO-CeO2/AC中CuO和CeO2质量比不同,对汞的去除效率也不同,在1∶2时去除效率最好;CuO-CeO2/AC中所负载的CuO和CeO的总量为5%时,能大大促进汞的吸附效率,增长有效吸附时间;CuO-CeO2/AC对汞的吸附性能随反应温度的增加呈先增加后减小的趋势,在80℃时达到最大值。  相似文献   

7.
Chang L  Chen IP  Lin SS 《Chemosphere》2005,58(4):485-492
It has been shown that the CeO2/gamma-Al2O3 catalyst is a feasible alternative to CeO2 for the catalytic wet air oxidation (CWAO) of phenol because it remains an effective catalyst and yet is cheaper to prepare. In this study, we found that the optimal cerium content in the CeO2/gamma-Al2O3 catalyst was 20 wt.%, regardless of catalyst loading. Furthermore, at 180 degrees C, with a phenol concentration of 1000 mg l(-1), and an O2 partial pressure of 1.0M Pa or 1.5M Pa, the optimal catalyst loading was 3.0 gl (-1). The efficacy of CWAO of phenol improved with O2 partial pressure, although the effects of O2 pressure were more significant between 0.5 MPa and 1.5 MPa than between 1.5 MPa and 2.0 MPa. After 2 h of reaction, approximately 100% phenol conversion and 80% total organic carbon (TOC) removal was recorded at 180 degrees C, 1000 mg l(-1) of phenol and 3.0 g l(-1) of catalyst. Because these percentages subsequently leveled off, it is suggested that 2 h is a suitable time over which to run the reaction. The efficacy of CWAO of phenol decreased as initial phenol concentration was raised (from 400 to 2500 mg l(-1)), with the exception of phenol conversion after about 2 h, for which 400 mg l(-1) produced the lowest phenol conversion figure. Higher phenol concentrations require both catalyst loading and O2 partial pressure to be increased to maintain high performance. For example, for 2000 mg l(-1) and 2500 mg l(-1) phenol, nearly 100% phenol conversion and 90% TOC removal after 4 h of reaction at 180 degrees C required 4.0 g l(-1) of catalyst and 2.0 MPa.  相似文献   

8.
活性炭纤维(ACF)经硝酸处理后采用浸渍法制备了CeO2-CoO/ACF复合催化剂,测试了其在以氨气为还原剂的低温SCR过程中的催化活性,同时研究了金属氧化物浸渍顺序及负载量、催化剂煅烧温度、空速比(SV)、NH,/NO(摩尔比)、O2含量等因素对NO转化效率的影响。研究发现,负载量为10%的CeO2-CoO/ACF复合催化剂经煅烧后在120—240℃时具有很高的催化活性,并且在N0初始浓度为1000mg/m3、空速比(SV)为6000h~、NH3/NO为1.05、O:体积分数在3.0%时具有较高的NO转化效率。  相似文献   

9.
Wang CH  Lin SS  Chen CL  Weng HS 《Chemosphere》2006,64(3):503-509
A fixed bed reactor was used to assess the catalytic incineration of toluene by various transition-metal oxide species supported on gamma-Al(2)O(3). CuO/gamma-Al(2)O(3) was found to be the most active of seven catalysts investigated. The CuO species, with a Cu content of 5% (wt), was hence used with four different supports (CeO(2), gamma-Al(2)O(3), TiO(2) and V(2)O(5)) in order to define the optimal combination. Results of the catalytic incineration of toluene, X-ray diffraction (XRD) analysis, oxygen-temperature programmed desorption (O(2)-TPD), toluene-temperature programmed desorption (toluene-TPD) and hydrogen-temperature programmed reduction (H(2)-TPR) showed that CuO/CeO(2) was the most active catalyst, followed by CuO/gamma-Al(2)O(3). The activity of CuO/CeO(2) with respect to the VOC molecule was observed to follow this sequence: toluen>p-xylene>benzene. The addition of water vapor or CO(2) significantly inhibited the activity of the CuO/CeO(2) and CuO/gamma-Al(2)O(3) catalysts. The inhibiting effect of both was reversible for CuO/gamma-Al(2)O(3). For CuO/CeO(2), the inhibiting effect of CO(2) was reversible and even insignificant at a higher temperature (220 degrees C), but the effect of H(2)O vapor was somewhat irreversible at lower incineration temperatures (220 degrees C). For complete oxidation of toluene, the required reaction temperature increased with gas hourly space velocity (GHSV) and toluene inlet concentration.  相似文献   

10.
Catalyst sorbents based on alumina-supported CuO, CeO2, and CuO-CeO2 were applied to a dry scrubber to clean up the SO2/HCl/NO simultaneously from pilot-scale fluidized-bed incineration flue gas. In the presence of organic compounds, CO and the submicron particles SO2 and HCI removed by the fresh catalyst sorbents and NO reduced to N2 by NH3 under the catalysis of fresh and spent desulfurization/dechloridization (DeSO2/DeHCl) catalyst sorbents (copper compounds, Cu, CuO, and CuSO4) were evaluated in this paper. The fresh and spent catalyst sorbents were characterized by the Brunner-Emmett-Teller method (BET), X-ray powder diffraction (XRPD), scanning electron microscopy (SEM), inductively coupled plasma-mass spectrometry (ICP-MS), and the elemental analyzer (EA). The study showed that the performances of CuO, CeO2, and CuO-CeO2/gamma-Al2O3 were better than that of Ca(OH)2. The removal efficiency of SO2 and HCl was 80-95% in the dry scrubber system. Under NH3/NO = 1, NO could not be reduced to N2 because it was difficult to control the ratio of air/fuel in the flue gas. For estimating the feasibility of regenerating the spent catalyst sorbents, BET and EA analyses were used. They indicated that the pore structures were nearly maintained and a small amount of carbon accumulated on their surface.  相似文献   

11.
CuO(-CeO_2)/SBA-15对萘氧化的催化活性及CO_2选择性研究   总被引:1,自引:0,他引:1  
通过浸渍法制备CuO/SBA-15和CuO-CeO2/SBA-15两种介孔材料催化剂,采用BET、XRD、TPR和XPS等对催化剂进行表征,重点考察催化剂对萘氧化反应的催化活性及对产物CO2的选择性。BET、XRD和XPS等实验结果表明CuO高度分散于介孔分子筛SBA-15中,CeO2可促进CuO在载体上的分散,同时能降低催化剂的TPR还原温度。活性测试结果表明CuO/SBA-15对萘氧化反应的催化活性较高,但是催化氧化的CO2选择性较低,温度在380℃时CO2的生成率仅为60%左右;CeO2的添加不仅提高了CO2的生成率,15%CuO-15%CeO2/SBA-15在325℃使CO2生成率达到99%,而且CeO2增强了催化剂的稳定性。  相似文献   

12.
用H2O2作为氧化剂,在595~704 K、18~30 MPa条件下,对活性染料废水进行超临界水氧化反应.实验结果表明,COD去除率随温度、压力、停留时间和氧化剂量的增加而上升,在704 K、28 MPa时,COD去除率可达到98.4%,停留时间小于35 s.COD、H2O2和水的反应级数分别为1、0和0;反应活化能Ea为37.21 kJ/mol;指前因子A为76.69 s-1.  相似文献   

13.
Catalytic wet-air oxidation (CWAO) of wastewater (chemical oxygen demand [COD] = 1800 mg O2/dm3) from a fine chemicals plant was investigated in a fixed-bed reactor at T = 393-473 K under total pressure of 5.0 or 8.0 MPa. Catalysts containing 0.3% wt. of platinum deposited on two supports, mixed silica-titania (SM1) and carbon black composites (CBC) were used. The CBC-supported catalyst appeared to be more active than the SM1-supported one. A slow decrease of activity of the platinum on SM1 (Pt-SM1) during the long-term operation is attributed to recrystallization of titania and leaching of a support component, while the Pt-CBC catalyst is deteriorated, owing to combustion of the support component. The power-law-kinetic equations were used to describe the rate of COD removal at CWAO over the catalysts. The kinetic parameters of COD reduction for the wastewater were determined and compared with the kinetic parameters describing phenol oxidation over the same catalysts. Rates of COD removal for the wastewater were found higher than those for phenol oxidation over the same catalysts and under identical operating conditions.  相似文献   

14.
Industrial dyeing wastewater was oxidized in supercritical water in a transpiring-wall reactor, using hydrogen peroxide as an oxidant. Experiments were performed at 595 to 704 K and 18 to 30 MPa, with an oxidant dosage ratio ranging from 0.6 to 2.0. A chemical oxygen demand (COD) removal of more than 98.4% was achieved at 704 K and 28 MPa, with a retention time less than 35 seconds, which increased with the temperature, pressure, and oxidant. A modified first-order rate expression was regressed from experimental data, taking into account the influence of induction time. The resulting pre-exponential factor, A, and activation energy, Ea, were 1.07 seconds(-1) and 12.12 kJ x mol(-1), respectively, while the reaction order for feed wastewater (based on COD) and oxidant were assumed to be 1 and 0, respectively. Gas chromatography/mass spectrometry analysis for effluents indicated that carbon dioxide, carbon monoxide, and nitrogen were the main reaction products, and phenol; benzenecarboxylic acid; 1, 2-benzenedicarboxylic acid; and isoquinoline were detected as intermediates.  相似文献   

15.
A method involving supercritical fluid extraction (SFE) with a solid phase trap containing activated alumina was investigated for the rapid analysis of polychlorinated dibenzo-p-dioxins (PCDDs), polychlorinated dibenzofurans (PCDFs), and dioxin like polychlorinated biphenyls (DL-PCBs) in soils and sediments. The samples were extracted by using supercritical carbon dioxide with water (2% versus CO(2) flow velocity) being used as an entrainer at a pressure of 30 MPa and a temperature of 130 degrees C for 50 min. The extracts were adsorbed on an activated alumina trap that was maintained at a temperature of 150 degrees C, and then, PCDD/DFs and DL-PCBs were eluted with 20 ml of hexane at 60 degrees C. After concentration, they were measured with a high-resolution gas chromatograph interfaced to a high-resolution mass spectrometric detector. The average concentrations of PCDD/DFs and DL-PCBs corresponded to the results obtained by the conventional method, and the reproducibility of this SFE method was below 21% of the relative standard deviations for all samples. The total time required for the analysis of the pretreatment of this method was only 2 h.  相似文献   

16.
用浸渍法在活性炭(AC)上负载氧化铈(CeO2)制备催化刺CeO2/AC催化臭氧氧化去除邻苯二甲酸二甲酯(DMP),考察了臭氧投加量,DMP初始浓度和溶液初始pH的影响.结果表明,CeO2/AC催化臭氧氧化去除DMP的最佳臭氧投加量为50mg/h,DMP初始浓度和溶液初始pH对CeO2/AC催化臭氧氧化DMP过程都有一定的影响.在DMP初始质量浓度为30 mg/L、溶液初始pH为5、臭氧投加量为50 mg/h、反应60 min时,CeO2/AC的加入(1.5g/L)有利于催化臭氧氧化DMP过程中总有机碳(TOC)的去除,TOC去除率由AC催化臭氧氧化的48%提高到68%.而单独臭氧氧化过程中的TOC去除率仅22%;且单独臭氧氧化与AC、CeO2/AC催化臭氧氧化DMP的矿化过程均符合二级反应动力学方程,CeO2/AC催化臭氧氧化DMP时TOC降解的二级反应动力学常数为0.0015L/(mg·min),分别是AC催化臭氧氧化的2.5倍和单独臭氧氧化的7.5倍.  相似文献   

17.
The photo-Fenton reaction effect on the biodegradability improvement of 100 mg/L solution of 2,4-dichlorophenol (DCP) has been investigated. Biochemical oxygen demand (BOD) at 5 and 21 days, BODn/ chemical oxygen demand (COD) and BODn/total organic carbon (TOC) ratios, average oxidation state, and inhibition on activated sludge were monitored. For 50 mg/L hydrogen peroxide and 10 mg/L iron(II) initial concentrations and 40 minutes of reaction time in the photo-Fenton process, the biodegradability of the pretreated solution, measured as BOD5/COD ratio, was improved from 0 for the original DCP solution up to 0.18 (BOD21/COD = 0.24). At that point, all DCP was eliminated from the solution. To study the effect of the pretreatment step, the biological oxidation of pretreated solutions was tested in two semicontinuous stirred tank reactors, one operated with activated sludge and one with biomass acclimated to phenol. Results showed that more than 80% TOC removal could be obtained by codigestion of the pretreated solution with municipal wastewater. Total organic carbon removals of approximately 60% were also obtained when the sole carbon source for the aerobic reactors was the pretreated solution. The hydraulic retention times used in the bioreactors were of the same order of magnitude as those used at domestic wastewater treatment plants (i.e., between 12 and 24 hours). Kinetic studies based on pseudo-first-order kinetics have also been carried out. Constants were found to be in range 0.67 to 1.7 L x g total volatiles suspended solids(-1) x h(-1).  相似文献   

18.
ClO2三相催化氧化处理硝基苯生产废水的试验   总被引:2,自引:0,他引:2  
硝基苯(NB)生产废水中含有大量NB及其衍生物,对生物具有毒性,属难生物降解物质.采用ClO2三相催化氧化工艺对NB废水进行处理.结果表明,每升废水投加280、350 mg ClO2,废水在活性炭加载含铜复合金属氧化物的催化剂床层停留56min,NB和色度的去除率均达到95%以上,COD去除率达到90%以上.吨废水处理成本约为10.5元.  相似文献   

19.
以H2O2为氧化剂用间歇式超临界水氧化装置对聚乙烯醇(PVA)废水进行降解研究。通过正交实验,考察了反应温度、压力、时间及氧化剂过氧倍数对降解效果的影响,并且采用GC/MS对液相降解产物进行表征推测其可能降解途径。结果表明:PVA在SCWO体系中能完全降解,反应温度440℃、压力28 MPa、氧化剂过氧倍数4、反应40 min时,COD去除率为99.03%,出水COD=89.09 mg/L。PVA在SCWO体系中降解为烯烃、烯酮、醇和羧酸类中间产物、最终降解为小分子的饱和直链烷烃类液相产物。  相似文献   

20.
活性炭纤维载体生物膜法处理洗车废水研究   总被引:2,自引:2,他引:0  
为了实现洗车废水的循环使用,进行了以聚丙烯腈基活性炭纤维(PAN-ACF)为生物膜载体处理洗车废水的实验研究。以LAS、COD和NH3-N等指标考察了活性炭纤维生物膜反应器对洗车废水的处理效果。结果表明:在常温下、pH=6.5~7,当进水流量在30 mL/min时,反应器达到最佳运行参数,活性炭纤维载体生物膜法对LAS、COD和NH3-N等的去除率分别达到了97%、80%和60%。出水水质完全达到《生活杂用水水质标准》(CJ/T48-99)中洗车用水主要水质指标的规定。此外,实验表明PAN-ACF作为生物膜载体具有很好的生物亲和性和再生性。  相似文献   