Waterpipe (aka hookah) tobacco smokers are exposed to toxicants that can lead to oxidative DNA and RNA damage, a precursor to chronic disease formation. This study assessed toxicant exposure and biomarkers of DNA [8-oxo-7, 8-dihydro-2′-deoxyguanosine (8-oxodG)] and RNA [8-oxo-7,8-dihydroguanosine (8-oxoGuo)] oxidative damage during smoking of flavored and non-flavored waterpipe tobacco. Thirty waterpipe smokers completed two counterbalanced 2-h lab waterpipe smoking sessions (flavored vs. non-flavored waterpipe tobacco). Urinary concentrations of 8-oxodG and 8-oxoGuo and expired carbon monoxide (eCO) were measured before and after the smoking sessions. A significant increase in the urinary concentrations of 8-oxodG (from 2.12 ± 0.83 to 2.35 ± 0.91 ng/mg creatinine, p = 0.024) and 8-oxoGuo (from 2.96 ± 0.84 to 3.45 ± 0.76 ng/mg creatinine, p = 0.003) were observed after smoking the non-flavored and flavored waterpipe tobacco, respectively. Our results also showed that the mean ± SD of eCO increased significantly after smoking the flavored (from 1.3 ± 1.1 to 20.3 ± 23.6 ppm, p < 0.001) and non-flavored waterpipe tobacco (from 1.8 ± 1.2 to 24.5 ± 26.1 ppm, p < 0.001). There were no significant differences in the means of 8-oxodG (p = 0.576), 8-oxoGuo (p = 0.108), and eCO (p = 0.170) between the flavored and non-flavored tobacco sessions. Smoking non-flavored and flavored waterpipe tobacco leads to oxidative stress and toxicant exposure. Our findings add to the existing evidence about the adverse effects of waterpipe tobacco smoking (WTS) and the need for strong policies to inform and protect young people from the risks of WTS.
Environmental Science and Pollution Research - The high NO2/NOX ratio in the after-treatment system is beneficial to its performance and achieved by NO catalytic conversion in diesel oxidation... 相似文献
This study investigated crystallization mechanisms for the formation of lead aluminosilicate by sintering lead stabilization with kaolin-based precursors. PbAl2Si2O8 was found to be the only stable lead aluminosilicate in low-PbO system and demonstrates its highly intrinsic resistance to acid attack in leaching test. A three-stage PbAl2Si2O8 formation mechanism was supported by the results of the changing temperature in the system. Amorphization of sintered products was observed in both PbO/kaolinite and PbO/mullite systems at 600–700°C. When the temperature was increased to 750–900°C, the crystallochemical formation of lead aluminosilicates (i.e., Pb4Al4Si3O16, Pb6Al6Si2O21, and PbAl2Si2O8) was observed. Pb4Al4Si3O16 and Pb6Al6Si2O21 were found to be the intermediate phases at 700–900°C. Finally, PbAl2Si2O8 was found to be the only crystallite phase to host Pb at above 950°C. A maximum of 80% and 96.7% Pb can be incorporated into PbAl2Si2O8 in PbO/kaolinite and PbO/mullite systems, respectively, but the final products exhibited different microstructures. To reduce environmental hazard of lead, this strategy demonstrated a preferred mechanism of immobilizing lead into PbAl2Si2O8 structure via kaolin-based precursors. 相似文献