全文获取类型
收费全文 | 212篇 |
免费 | 20篇 |
国内免费 | 28篇 |
专业分类
安全科学 | 45篇 |
废物处理 | 25篇 |
环保管理 | 35篇 |
综合类 | 115篇 |
基础理论 | 13篇 |
污染及防治 | 17篇 |
评价与监测 | 4篇 |
社会与环境 | 6篇 |
出版年
2024年 | 1篇 |
2023年 | 6篇 |
2022年 | 12篇 |
2021年 | 12篇 |
2020年 | 11篇 |
2019年 | 9篇 |
2018年 | 15篇 |
2017年 | 8篇 |
2016年 | 8篇 |
2015年 | 9篇 |
2014年 | 22篇 |
2013年 | 22篇 |
2012年 | 17篇 |
2011年 | 15篇 |
2010年 | 3篇 |
2009年 | 5篇 |
2008年 | 8篇 |
2007年 | 8篇 |
2006年 | 13篇 |
2005年 | 13篇 |
2004年 | 12篇 |
2003年 | 7篇 |
2002年 | 10篇 |
2001年 | 3篇 |
2000年 | 5篇 |
1999年 | 4篇 |
1998年 | 1篇 |
1973年 | 1篇 |
排序方式: 共有260条查询结果,搜索用时 343 毫秒
61.
The useful life of consumer electronic devices is relatively short, and decreasing as a result of rapid changes in equipment features and capabilities. This creates a large waste stream of obsolete electronic equipment, electronic waste (e-waste).Even though there are conventional disposal methods for e-waste, these methods have disadvantages from both the economic and environmental viewpoints. As a result, new e-waste management options need to be considered, for example, recycling. But electronic recycling has a short history, so there is not yet a solid infrastructure in place.In this paper, the first half describes trends in the amount of e-waste, existing recycling programs, and collection methods. The second half describes various methods available to recover materials from e-waste. In particular, various recycling technologies for the glass, plastics, and metals found in e-waste are discussed. For glass, glass-to-glass recycling and glass-to-lead recycling technologies are presented. For plastics, chemical (feedstock) recycling, mechanical recycling, and thermal recycling methods are analyzed. Recovery processes for copper, lead, and precious metals such as silver, gold, platinum, and palladium are reviewed. These processes are described and compared on the basis of available technologies, resources, and material input–output systems. 相似文献
62.
我国废电池的回收与处理 总被引:5,自引:0,他引:5
本文详细介绍了国内外常见的各种废电池的种类、有害成分,处理方法,分析了目前我国在度电池回收处理过程中所存在的诸多问题,并有针对性的提出建议。 相似文献
63.
纳米储氢材料贮存使用安全评估方法研究 总被引:2,自引:1,他引:1
李传贵 《中国安全科学学报》2003,13(9):24-26
储氢材料贮存使用的安全可靠性是安全工程和可靠性领域中的特殊问题 ,纳米储氢材料的使用 ,其安全性和贮存可靠性同时占有重要地位。笔者依据纳米储氢材料使用和在正常贮存状态下的失效特点 ,应用Poisson过程理论建立纳米储氢材料使用和贮存安全性评估数学模型和统计分析方法 ,给出了在一定置信度下纳米储氢材料贮存寿命与可靠度之间的关系表达式。为纳米储氢材料和新型能源材料研究和使用等提供了理论基础和应用控制的方法。 相似文献
64.
废旧干电池的环境污染防治及回收利用 总被引:5,自引:0,他引:5
介绍了各种干电池的基本化学组成,分析了废旧干电池污染环境的主要途径及对人类的危害,并就回收利用问题提出建议。 相似文献
65.
燃料电池高效率、无污染、建设周期短、易维护以及低成本的特点被受人们关注。本文介绍了各种类型燃料电池(碱性燃料电池、熔融碳酸盐燃料电池、固体氧化物燃料电池、磷酸燃料电池及质子交换膜燃料电池)的技术进展及其发展现状,对燃料电池的应用前景进行了探讨。 相似文献
66.
J. Bierkens G. Klein P. Corbisier R. Van Den Heuvel L. Verschaeve R. Weltens G. Schoeters 《Chemosphere》1998,37(14-15)
Increasing evidence suggests that the use of a single bioassay will never provide a full picture of the quality of the environment. Only a test battery, composed of bioassays of different animal and plant species from different trophic levels will reduce uncertainty, allowing an accurate assessment of the quality of the environment. In the present study, a test battery composed of 20 bioassays of varying biological endpoints has been compared Apart from lethality and reproductive failure in earthworms, springtails, nematoda, algae and vascular plants, these endpoints also included bioavailibility of metals (bacteria), heat-shock induction (nematodes, algae), DNA damage (bacteria, earthworm, vascular plants), β-galactosidase (Daphnia) and esterase activity (algae) and a range of immunological parameters (earthworm). Four chemicals (cadmium, phenol, pentachlorophenol and triflurahn) — each representing a different toxic mode of action — were applied in a dilution series (from 1 mg/kg up to 1000 mg/kg) onto OECD standard soil. The tests have been performed both on these artificially contaminated soil samples and on aqueous extracts subsequently obtained from these soils. The results show that the immunological parameters and the loss of weight in the earthworms were among the most sensitive solid phase assays. Esterase inhibition and heat-shock induction in algae were shown to be extremely sensitive when applied to soil extracts. As previously shown at the species level, no single biological endpoint was shown to be the most sensitive for all four modes of toxic action. 相似文献
67.
Sudipta B. Sarmah B. Das A. Garg L. Gao R. K. Pai 《International Journal of Green Energy》2020,17(8):510-520
ABSTRACT Estimation of State of Health (SoH) of Lithium-ion (Li-ion) battery is essential to predict the lifespan of batteries of an electric vehicle (EV). The efficient prediction of battery health indicates to the effective and safe operation of EV. However, delivering an effective and accurate method for the estimation of SoH in the real condition is truly a challenging task. The present study proposed a holistic procedure of combining both experimental and numerical investigations to conduct the fundamental study on coupled mechanical-electrochemical behavior of Li-ion battery. The proposed investigation highlighted the effect of stress on the capacity of the battery, considering capacity fade as an equivalent parameter to its health for real-time estimation of SoH. Finally, a simple model of Artificial Neural Network (ANN) is provided, which shows the linear dependency of stress with the SoH. The results obtained from the ANN model are validated with a Linear Regression (LR) model for a better understanding of the inspection. The predicted value of mean Square Error (MSE) and R square error in the ANN training model are found to be 0.000309 and 0.849687, respectively. Whereas for the test model, these predicted values are found to be 0.000438 and 0.819347, respectively. 相似文献
68.
69.
为研究21700和18650新旧2型多用途锂离子电池在航空运输低压环境下的热失控特性差异,采用动压变温实验舱搭建实验平台开展实验。将实验环境压力设定为飞机巡航时的环境压力30 kPa,对比常压101 kPa,使用外部热源加热的方式触发锂电池热失控,利用热传播引发相邻电池热失控,分别从热失控温度变化特性、热释放速率和热解气体组分浓度变化进行分析。研究结果表明:能量密度更高的21700电池热失控峰值温度更高,高温危险性要高于18650电池,但触发热失控所需的热量更多,电池间热传播时间会延长;低压环境有利于降低锂电池热失控燃爆峰值温度,减小燃爆热释放速率,但会产生更多CxHy和CO等具有燃爆性的热解气体,可能会在有限空间内与氧气混合引起二次燃爆。 相似文献
70.
废铅酸蓄电池铅膏性质分析 总被引:1,自引:0,他引:1
为给废旧铅蓄电池铅膏的湿法回收工艺提供理论依据,对湖北金洋冶金股份有限公司破碎分选后的废铅膏进行了XRF、XRD、物理分析及化学分析等,确定了废铅膏的主要成分、理化性质等特性。结果表明,废铅膏粒径细小,碾钵磨细后能过120目的筛下物超过77.4%,这对湿法转化是有利的。废铅膏主要组成为64.5%PbSO4、29.5%PbO2、4.5%PbO、0.8%Pb及其他微量杂质元素,杂质主要包括Fe、Sb和Si等。因此,铅膏湿法处理时应该采取合适的净化工艺。 相似文献