Affiliation: | Key Laboratory of Advanced Coal & Coking Technology, University of Science and Technology Liaoning, Anshan Liaoning 114051, China;Key Laboratory of Advanced Coal & Coking Technology, University of Science and Technology Liaoning, Anshan Liaoning 114051, China;Key Laboratory of Advanced Coal & Coking Technology, University of Science and Technology Liaoning, Anshan Liaoning 114051, China;Key Laboratory of Advanced Coal & Coking Technology, University of Science and Technology Liaoning, Anshan Liaoning 114051, China;Key Laboratory of Advanced Coal & Coking Technology, University of Science and Technology Liaoning, Anshan Liaoning 114051, China;Coking & Refractory Engineering Consulting Corporation, Anshan Liaoning 114002, China;Coking & Refractory Engineering Consulting Corporation, Anshan Liaoning 114002, China |
| |
Abstract: | Long flame coal are abundant and widely distributed in China, but the resource utilization is quite low, the production efficiency is not high. Stamp-charging coke making technology can bend some long flame coal, which can reduce production cost and expand the coking coal resources. The long flame coal of different mass fraction is added into prime coking coal including fat coal from Longhu, 1/3 coking coal from Xinjian and coking coal from Didao in experiment. The swelling pressure is tested on-line detection using pressure sensor in coke making process, and the pores are observed by scanning electron microscopy. The results show that, the swelling pressure first increase and then decrease with the temperature increased and the maximum swelling pressure reduces gradually with mass fraction of the Long flame coal from Shenmu increased in coke making process. The SEM images of resultant coke display that the coke get more and more loose and the amount of pores is increased with mass fraction of the long flame coal from Shenmu increased. The amount pores and the pore diameter both is minimum for coking coal from Didao as prime coking coal under the same fraction of long flame coal. |
| |
Keywords: | swelling pressure coke morphology long flame coal stamp-coking technology |
|
| 点击此处可从《环境科学学报(英文版)》浏览原始摘要信息 |
|
点击此处可从《环境科学学报(英文版)》下载全文 |
|