基金项目:国家自然科学基金项目"多层环糊精-氧化石墨烯骨架薄膜的制备及其去除水中微污染物的效能与机制研究"(51708014);建筑废砖净化介质透水铺装系统中重金属的强化去除、迁移与转化机制(51678025);长城学者(CIT&TCD20170313);国家水体污染控制与治理科技重大专项(2018ZX07110-008)。
摘    要:研究了不同类型透水铺装系统对径流重金属的去除效能和机制.在实验室搭建了3种典型透水铺装系统(陶瓷透水砖、透水沥青和透水混凝土),研究了其对5种常见径流重金属(Cu、Zn、Cd、Mn、Ni)的去除效能和机制,并分析了不同降雨重现期(2,3,5年)对透水铺装系统去除径流重金属的影响.结果 表明:3种透水铺装系统对5种径流重...

关 键 词:透水铺装  重金属  路面径流  低影响开发  面源污染
收稿时间:2020-03-10

INFLUENCING MECHANISM OF PERMEABLE PAVEMENT TYPE ON REMOVAL EFFICIENCY OF HEAVY METALS FROM RUNOFF
Affiliation:1. Engineering Research Center of Sustainable Urban Sewage System Construction and Risk Control, Beijing University of Civil Engineering and Architecture, Beijing 102616, China;2. Key Laboratory of Urban Stormwater System and Water Environment, Ministry of Education, Beijing University of Civil Engineering and Architecture, Beijing 102616, China
Abstract:This paper studied the removal efficiency and mechanism of heavy metals on different types of permeable pavement systems in runoff water. Three typical permeable pavement systems (ceramic permeable bricks, permeable asphalt, and permeable concrete) were set up in the laboratory, and the removal efficiency and mechanism of five common runoff heavy metals (Cu, Zn, Cd, Mn, Ni) were studied. Furthermore, the effects of rainfall recurrence periods (2 a, 3 a, 5 a) were analyzed. The results showed that the three permeable paving systems had good removal efficiencies on all five heavy metals, and compared with permeable asphalt and permeable concrete, ceramic permeable brick showed the best removal and stable removal efficiency. Ceramic permeable bricks and permeable asphalt could reduce the concentration of heavy metals in a shorter time, but the speed of permeable concrete reaching the adsorption point was slower and the effluent concentration was more unstable especially under different rainfall recurrence periods. Different permeable pavement systems exhibited different performance under different rainfall recurrence periods, with an impact degree sequence of 2 a>5 a>3 a. This result showed that permeable pavement systems had excellent and stable removal performance under the rainfall condition of 3 a, while a too large or too small flow rate would reduce the removal efficiency of heavy metal removal.