Nickel recovery from spent nickel catalyst.
Authors:Kamala K Sahu  Archana Agarwal  Banshi D Pandey
Institution:National Metallurgical Laboratory, Jamshedpur, India. drkksahu@yahoo.com
Abstract:A process for nickel recovery from a spent catalyst of definite composition has been developed using the hydro-metallurgical route. The processing steps includes direct sulphuric acid leaching followed by separation of iron as well as silica and other impurities. For a 152 microm particle size catalyst, extraction of about 98% nickel was achieved at 363 K in 2 h using a sulphuric acid concentration (v/v) of 8% and a pulp density of 10%. The dissolution of nickel followed diffusion-controlled leaching kinetics. Increase in temperature and sulphuric acid concentration resulted in increase in the nickel recovery. The activation energy for nickel dissolution was calculated to be 62.8 kJ mol(-1). Finally, nickel was recovered as value-added products such as sulphide and oxalate with overall recovery of 90 and 88% of nickel, respectively.
Keywords:
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号