Gas chromatography-mass spectrometry (GC-MS) methodology was developed to speciate and quantitate several degradation products of polydimethylsiloxane (PDMS) in soil. We have demonstrated that the major degradation product,viz., dimethylsilanediol, can be readily analyzed by GC-MS without derivatization as commonly practiced in analyzing such materials. A mixture of linear siloxane diols (n = 1–5, wheren is the number of Me2SiO units), and cyclic dimethylsiloxanes (n = 4–6) was resolved by GC-MS. We also found that peak identity of various diols required that GC-MS is done in the chemical ionization (CI) mode, since the electron impact (EI) ionization mode produced similar mass fragmentation patterns for diols and cyclics containing the same number of silicon atoms. For siloxane diols, detection limits ranged from 100 pg (forn = 1) to 1 ng (for n = 5). For cyclics, the detection limit was about 1 pg. Dimethylsilanediol, known to be unstable even in the solid state, was shown by NMR techniques to be stable in aqueous solution at <0.1% concentration. A 100-ppm solution was stable for over a year. Purity check for dimethylsilanediol is best carried out by Si-29 solid-state NMR technique.  相似文献   

2.
The degradation products of polymers are identifiable by chromatography. The degradation product patterns (or fingerprints) formed depend on the type of polymer, the degradation mechanism(s), and also the type of additive present in the material. The chromatographic fingerprint of biotically aged degradable low-density polyethylene (i.e., LDPE+starch+prooxidant) shows, in particular, the absence of low molecular weight carboxylic acids, which suggests an assimilation of these carboxylic acids by the microorganisms. The degradation products of natural polymers are usually intermediates that are used again in the anabolic cycles. It is possible to transfer the terminology from the natural polymers, where the catabolism of natural polymers consists of three stages, and apply this also to the degradable synthetic polymers. During stage I the natural polymers degrade to their major building blocks (e.g., amino acids, glycerol, hexoses, pentoses, etc.), during stage II these products are collected and converted to a smaller number of even simpler molecules [e.g., acetyl-coenzyme A (CoA)]. In stage III, finally, the acetyl-CoA enters the citric acid cycle, where energy is gained in parallel with the release of CO2 and H2O.Presented at the international workshop,Polymers from Renewable Resources and their Degradation, Stockholm, Sweden, November 10–11, 1994.  相似文献   

3.
The potential biodegradability of several vegetable oil-based polymers was assessed by respirometry in soil for 60–100 days at temperatures of 30–58°C. Films of soybean oil and linseed oil which were oxidatively polymerized (Co catalyst) on a kraft paper support were 90%–100% mineralized to CO2 after 70 days at 30°C. Mineralization of polymerized tung oil to CO2 was much slower than soy or linseed oils. Mineralization of epoxy resins made from epoxidized soybean oil (ESO) and aliphatic dicarboxylic acids was rapid while mineralization of similar resins made with a triacid (citric) was slower. There was no significant degradation of polyamine/ESO resins after 100 days at 58°C. Mineralization of the available carbon in vegetable oil polyurethanes and cationically polymerized ESO was less than 7.5% after 70 days at 30°C and 25 days at 55°C compared to 100% for soybean oil. From these results, it appears that triglycerides highly cross-linked with non-degradable linkages are not biodegradable to a significant extent while triglycerides cross-linked with hydrolysable bonds such as esters remain biodegradable.  相似文献   

4.
Establishing carbon balances has been proven to be an applicable and powerful tool in testing biodegradability of polymers. In controlled degradation tests at a 4-L scale with the model polymer poly(-hydroxybutyrate) (PHB), it was shown that the degree of degradation could not be determined with satisfactory accuracy from CO2 release alone. Instead, the course of degradation was characterized by means of establishing carbon balances for the degradation of PHB withAcidovorax facilis and a mixed culture derived from compost. Different analytical methods for determining the different carbon fractions were adapted to the particular test conditions and compared. Quantitative determination of biomass and residual polymer were the main problems in establishing carbon balances. Amounts of biomass derived from protein measurements depend strongly on assumptions of the protein content of the biomass. Selective oxidation of biomass with hypochlorite was used as alternative, but here problems arose from insoluble metabolic products. Determination of soluble components with the method of chemical oxygen demand (COD) also includes empirical assumptions but seems acceptable if the dissolved carbon fraction is in the range of some 10% total carbon. Results confirm both analytical assays and theoretical approaches, in ending up at values very close to 100%, within an acceptable standard deviation range under test conditions comparable to standard test practice.Paper presented at the Bio/Environmentally Degradable Polymer Society—Third National Meeting, June 6–8, 1994, Boston, Massachusetts.  相似文献   

5.
Carbohydrate acid amides, diamides and polyamides have been proposed to be utilized as nitrogen plant fertilizers or fertilizer components, and experiments with Brassica rapa demonstrated a positive biological response when these compounds were used as the only source of fixed nitrogen for plant growth. The present study was carried out with the aim of elucidating the mechanism of degradation of these polymers in both soil/compost and in liquid media and the role of microorganisms in this process. The results obtained suggest that a major route of degradation of polyglucaramides in the environment is their abiotic hydrolysis/release of the diacid and diamine building block units of these polymers, which are then utilized for growth by microorganisms. In cell-free crude extracts from enrichment cultures obtained with different poly-D-glucaramides, no enzyme activities catalyzing the release of diamines from these compounds were detected.  相似文献   

6.
In experiments employing the lignocellulose-decaying basidiomycetes Trametes versicolor and Stropharia rugosoannulata degrading uniformly14C-labelled 2,4-dichlorophenol and pentachlorophenol, acombination of size exclusion chromatography (SEC),fractionation, and -scintillation counting wasapplied to quantify polymerisation products formed duringchlorophenol degradation. Time-dependent mass balances weregenerated by analysis of 14C in polymerisation products,CO2, as well as monomer non-polar and polar metabolites.Approximately 30% of the chlorophenols were found to bepolymerised. A major fraction of the polymerised productscorresponded to a molecular weight range from 0.24 – 40 kDa.Only a minor fraction could be attributed to a molecularweight >40 kDa. This method proved to be useful inquantification of polymerisation products and kinetics of thepolymerisation processes, whereas UV/Vis detection ofpolymerisation products separated by SEC led to false positiveresults. The SEC-14C method could also be applied forother complex processes where polymerisation ordepolymerisation occurs (humification, degradation oflignocellulose, formation of bound residues from xenobioticssuch as polycyclic aromatic hydrocarbons or 2,4,6-trinitrotoluene) and where spectrophotometric determinationsare difficult or impossible.  相似文献   

7.
This paper presents a test scheme for assessing the biodegradation potential of polymers, starting with aquatic screening systems (aerobic and anaerobic) and continuing to long-term systems. At the end of the scheme the material has to prove its behavior under the relevant disposal conditions. Aerobic screening was performed mainly under aquatic conditions, but also in soil, using BOD-respirometry. Carbon balances were performed to obtain a better evaluation of the biodegradation potential. Under anaerobic conditions, biodegradation in an aquatic medium was followed by measuring CH4 and CO2 production. Polymers not fully degraded in the screening systems were tested in aquarium systems for at least 1 year. Biodegradation was followed by monitoring the DOC released in the water, mass loss, and microbial growth on the samples and in the water as well as via FTIR spectroscopy and SEM pictures. Results are presented for the polymers PHB, PHBV, PCL, Mater-Bi AI05H and ZF03U, and Bioceta. By combining the data from the screening with the aquarium system, a good picture of the degradation behavior of the polymers is obtained.Paper presented at the Bio/Environmentally Degradable Polymer Society—Third National Meeting, June 6–8, 1994, Boston, Massachusetts.  相似文献   

8.
Polylactic acid (PLA) is a hydrolytically degradable aliphatic polyester, and water vapor permeability may have a significant influence on the rate of degradation. A method is devised to use bags prepared from PLA films and filled with molecular sieves to determine the water vapor permeability in the polymer, its copolymers with caprolactone, and blends with polyethylene glycol. The “solution-diffusion” model is used to determine the permeability parameters. These include the solubility coefficient,S, a measure of the equilibrium water concentration available for hydrolysis and the diffusion coefficient,D, which characterizes the rate of water vapor diffusion into the film under specific conditions. Values ofS andD at 50‡C and 90% relative humidity ranged from 400 × 10-6 to 1000 × 10-6 cm3 (STP)/(cm3 Pa) and 0.20 × 10-6 to 1.0 × 10-6 cm2/s, respectively. TheS andD coefficients were also measured at 20 and 40‡C and compared to those of other polymers. The degree of crystallinity was found to have little influence on the measured permeability parameters. The heat of sorption, δHS, and the activation energy of diffusion, ED, were used to show that the permeability process is best described by the “water cluster” model for hydrophobic polymers. Finally, the diffusion coefficient is used to compare the rate of water diffusion to the rate of water consumption by ester hydrolysis. Results indicate that hydrolytic degradation of PLA is reaction-controlled.  相似文献   

9.
Soil respiration is a large C flux which is of primary importance in determining C sequestration. Here we ask how it is altered by atmospheric CO2 concentration and N additions. Swards of Lolium perenne L. were grown in a Eutric cambisol under controlled conditions with and without the addition of 200 kg NO 3 –N ha–1, at either 350 ppm or 700 ppm CO2, for 3 months. Soil respiration and net canopy photosynthesis were both increased by added N and elevated CO2, but soil respiration increased proportionately less than fixation by photosynthesis. Thus, both elevated CO2 and N appeared to increase potential C sequestration, although adding N at elevated CO2 reduced the C sequestered as a proportion of that fixed relative to elevated CO2 alone. Across all treatments below-ground respiratory C losses were predicted by root biomass, but not by soil solution C and N concentrations. Specific root-dependent respiration was increased by elevated CO2, such that belowg-round respiration per unit biomass and per unit plant N was increased.  相似文献   

10.
The standard test method ASTM D 5988-96 for determining the degree and rate of aerobic biodegradation of plastic materials in contact with soil was applied to poly(3-hydroxybutyrate) and poly(-caprolactone). The method proved to be reliable and supplied reproducible measurements of CO2 production, provided potassium (instead of barium) hydroxide was used as a trapping solution. The trends of CO2 evolution, as a function of time, observed for the degradation of polymer powders in soil are similar to those predicted by simple first order kinetics in solution. The experimental data are described by a Michaelis–Menten type model, which accounts for the heterogeneity of the polymer-soil system. The kinetic equation deduced predicts the degradation rate to the proportional to the exposed polymer surface area.  相似文献   

11.
Testing biodegradability of plastics under varied conditions of the environment as well as under laboratory conditions in accordance with valid international standards is very laborious, lengthy and often also economically demanding. For this reason, applicability was verified of gas chromatography to analyze gaseous phase when investigating the biodegradation course of plastics in an aqueous environment as an alternative to customary employed methods. A mathematical model of acid–basic CO2 equilibrium in a gas–liquid system was worked out, enabling to determine quantity of produced CO2 through chromatographic analysis of gaseous phase, in dependence on ratio of liquid and gas phase volumes (V l/V g) and on actual pH of liquid phase. Experimental conditions for organizing the tests were optimized. A ratio that proved suitable was V l/V g ≅ 0.1 at pH ≈ 7.1 of liquid phase. Under these test conditions, biodegradability of model samples, PHB, Gellan gum and Xanthan gum, was explored; course of biodegradation was studied through produced CO2 (values ) determined by analyzing gaseous phase through gas chromatography on the one hand, and through customary “titration” procedure on the other. With water-soluble polymers, the decrement in dissolved organic carbon (values D DOC) was also studied. Difference between values does not exceed 5%. The procedures in question are alternative “substituting” procedures for observing course of aerobic biodegradation of substances in an aqueous environment.  相似文献   

12.
Organic waste, as a main constituent of municipal solid waste, has as well as solid biomass a high potential for biogas generation. Despite the importance of biogas generation from these materials, the availability of large-scale biogas processes lacks behind the demand. A newly developed double-stage solid–liquid biogas process, consisting of an open hydrolysis stage and a fixed-bed methane reactor, allows the biogas production from almost all biodegradable solid waste and renewable resources like maize, grass, sugar cane, etc. Furthermore, residues from industrial processes, like the glycerine waste water from biodiesel production, can also be converted into biogas successfully. Due to the strong separation of hydrolysis and methanation, the process is extremely stable. No malfunction has been detected so far. The open hydrolysis releases CO2 and allows oxidation of sulfur. Consequently, the biogas has a high methane (>72%) and low H2S concentration (<100 ppm). Stirrers or other agitation equipment are not necessary; only liquids are pumped. The biogas generation becomes controllable for the first time; thus, the actual generation can be easily adapted to the consumption.  相似文献   

13.
Microorganisms which can assimilate a new polyester synthesized from polyethylene glycol (PEG) as a dihydroxyl compound and phthalic acid as a dicarboxyl compound were isolated from soils by enrichment culture techniques. Two cultures, K and N, were obtained: Culture K grew on PEG 4000 polyester and culture N assimilated PEG 6000 polyester. Each culture included two bacteria indispensable for the degradation of polyesters: bacteria K1 and K2 for PEG 4000 polyester-utilizing culture K and bacteria N1 and N2 for PEG 6000 polyester-utilizing culture N. Bacteria K2 and N2 were responsible for the hydrolysis of ester bonds in a polyester and both were identified as the same species,Comamonas acidovorans. Bacteria K1 and N6 could assimilate PEG as a sole carbon and energy source. Both are Gram-negative, non-spore-forming rods and resembled each other on their colony characteristics, although strain K1 could not grow on PEG 6000.C. acidovorans N2 (K2) grew on dialkyl phthalates (C2–C4) and phthalate and tributyrin, but not on PEG, diphthalic PEG, and PEG phthalate polyesters. Their culture supernatant and washed cells hydrolyzed PEG (400–20,000) phthalate and sebacate polyesters.C. acidovorans had higher esterase activity toward PEG phthalate, isophthalate, and terephthalate polyesters than known esterase and lipases. The esterase seemed to be an extracellular one and attached to the cell surface.  相似文献   

14.
In this paper we studied the synthesis of biodegradable optically active poly(ester-imide)s containing different amino acid residues in the main chain. These pseudo-poly(amino acid)s were synthesized by polycondensation of N,N′-(pyromellitoyl)-bis-l-tyrosine dimethyl ester as a diphenolic monomer and two chiral trimellitic anhydride-derived diacid monomers containing s-valine and l-methionine. The direct polycondensation reaction of these diacids with aromatic diol was carried out in a system of tosyl chloride (TsCl), pyridine (Py) and N,N′-dimethylformamide (DMF) as a condensing agent. The structures and morphology of these polymers were studied by FT-IR, 1H-NMR, powder X-ray diffraction, field emission scanning electron microscopy (FE-SEM), specific rotation, elemental and thermogravimetric analysis (TGA) techniques. TGA profiles indicate that the resulting PEIs have a good thermal stability. Morphology probes showed these polymers were noncrystalline and nanostructured polymers. The monomers and prepared polymers were buried under the soil to study the sensitivity of the monomers and the obtained polymers to microbial degradation. The high microbial population and prominent dehydrogenase activity in the soil containing polymers showed that the synthesized polymers are biologically active and microbiologically biodegradable. Wheat seedling growth in the soil buried with synthetic polymers not only confirmed non-toxicity of polymers but also showed possibility of phyto-remediation in polymer-contaminated soils.  相似文献   

15.
Residual cellulose acetate (CA) films with initial degree of substitution (DS) values of 1.7 and 2.5 (CA DS-1.7 and DS-2.5) were recovered from a simulated thermophilic compost exposure and characterized by gel permeation chromatography (GPC), proton nuclear magnetic resonance (1H NMR), and scanning electron microscopy (SEM) to determine changes in polymer molecular weight and DS and to study microbial colonization and surface morphology, respectively. During the aerobic degradation of CA DS-1.7 and CA DS-2.5 films exposed for 7 and 18 days, respectively, the number-average molecular weight (M n) of residual polymer decreased by 30.4% on day 5 and 20.3% on day 16, respectively. Furthermore, a decrease in the degree of substitution from 1.69 to 1.27 (4-day exposure) and from 2.51 to 2.18 (12-day exposure) was observed for the respective CA samples. In contrast, CA films (DS-1.7 and DS-2.5) which were exposed to abiotic control vessels for identical time periods showed no significant changes inM n and DS. SEM photographs of CA (DS-1.7 and DS-2.5) film surfaces after compost exposures revealed severe erosion and corresponding microbial colonization. Similar exposure times for CA films in abiotic control vessels resulted in only minor changes in surface characteristics by SEM observations. The conversion of CA DS-1.7 and DS-2.5 to CO2 was monitored by respirometry. In these studies, powdered CA was placed in a predigested compost matrix which was maintained at 53°C and 60% moisture content throughout the incubation period. A lag phase of 10- and 25-day duration for CA DS-1.7 and DS-2.5, respectively, was observed, after which the rate of degradation increased rapidly. Mineralization of exposed CA DS-1.7 and DS-2.5 powders reported as the percentage theoretical CO2 recovered reached 72.4 and 77.6% in 24 and 60 days, respectively. The results of this study demonstrated that microbial degradation of CA films exposed to aerobic thermophilic laboratory-scale compost reactors not only results in film weight loss but also causes severe film pitting and a corresponding decrease in chainM n and degree of substitution for the residual material. Furthermore, conversions to greater than 70% of the theoretical recovered CO2 for CA (DS 1.7 and 2.5) substrates indicate high degrees of CA mineralization.Guest Editor: Dr. Graham Swift, Rohm & Haas.  相似文献   

16.
A co-product stream from soy-based biodiesel production (CSBP) containing glycerol, fatty acid soaps, and residual fatty acid methyl esters (FAME) was utilized as a fermentation feedstock for the bacterial synthesis of poly(3-hydroxybutyrate) (PHB) and medium-chain-length poly(hydroxyalkanoate) (mcl-PHA) polymers. Pseudomonas oleovorans NRRL B-14682 and P. corrugata 388 grew and synthesized PHB and mcl-PHA, respectively, when cultivated in up to 5% (w/v) CSBP. In shake flask culture, P. oleovorans grew to 1.3 ± 0.1 g/L (PHA cellular productivity = 13–27% of the bacterial cell dry weight; CDW) regardless of the initial CSBP concentration, whereas P. corrugata reached maximum cell yields of 2.1 g/L at 1% CSBP, which tapered off to 1.7 g/L as the CSBP media concentration was increased to 5% (maximum PHA cellular productivity = 42% of the CDW at 3% CSBP). While P. oleovorans synthesized PHB from CSBP, P. corrugata produced mcl-PHA consisting primarily of 3-hydroxyoctanoic acid (C8:0; 39 ± 2 mol%), 3-hydroxydecanoic acid (C10:0; 26 ± 2 mol%) and 3-hydroxytetradecadienoic acid (C14:2; 15 ± 1 mol%). The molar mass (Mn) of the PHB polymer decreased by 53% as the initial CSBP culture concentration was increased from 1% to 5% (w/v). In contrast, the Mn of the mcl-PHA polymer produced by P. corrugata remained constant over the range of CSBP concentrations used.  相似文献   

17.
Chain-extension reactions were carried out using titanium-iso-propoxide (TIP) as a catalyst for a series of polyesters or copolyesterethers with low molecular weights (M n =1500–10,000) synthesized by the ring-opening copolymerization of succinic anhydride (SA) with ethylene oxide (EO). The copolymers having aM n from 25,000 to 50,000 of different properties were obtained. Both the melting point (T m ) and the fusion heat (H), which indicate the crystallinity of the copolymers, rose with an increase in SA content in the copolymers. Semitransparent films were prepared by compression molding of the copolymers. The biodegradation of the copolymer films was evaluated by enzymatic hydrolysis by lipases and by an aerobic gas evolution test in standard activated sludge. The hydrolyzability of these copolymers by three kinds of lipases was affected by their copolymer composition SA/EO, form, andM n . The copolyesterether (SA/EO=43/57,M n =48,900) was more easily biodegraded by standard activated sludge compared to the polyester (SA/EO=47/53,M n =36,300).Presented at the Pacifichem-95, December 17–22, 1995, Honolulu, Hawaii.  相似文献   

18.
Melt-pressed films of polycaprolactone (PCL) and poly(lactic acid) (PLA) with processing additives, CaCO3, SiO2, and erucamide, were subjected to pure fungal cultures Aspergillus fumigatus and Penicillium simplicissimum and to composting. The PCL films showed a rapid weight loss with a minor reduction in the molecular weight after 45 days in A. fumigatus. The addition of SiO2 to PCL increased the rate of (bio)erosion in A. fumigatus and in compost. The use of a slip additive, erucamide, was shown to modify the properties of the film surface without decreasing the rate of bio(erosion). Both the rate of weight loss and the rate of molecular weight reduction of PCL increased with decreasing film thickness. The addition of CaCO3 to PLA significantly reduced the thermal degradation during processing, but it also reduced the rate of the subsequent (bio)degradation in the pure fungal cultures. PLA without additives and PLA containing SiO2 exhibited the fastest (bio)degradation, followed by PLA with CaCO3. The degradation of the PLA films was initially governed by chemical hydrolysis, followed by an acceleration of the weight change and of the molecular weight reduction. PLA film subjected to composting exhibits a rapid decrease in molecular weight, which then remains unchanged during the measurement period, probably because of crystallization.  相似文献   

19.
The ASTM D5210-91 protocol for evaluating the biodegradability of a polymer was examined. The reactor design was modified not only to account for the total CO2 evolved but also to allow for the simultaneous carbon assessment in microbes, soluble products, and solid samples. Improvements in the test procedure were implemented such as (1) refining the CO2 pretrap and posttrap design, (2) optimizing the carbon dioxide removal efficiency, (3) accounting for the total polymeric carbon, (4) standardizing the inoculum, and (5) revising the nutrient medium. By growing the sludge on a suitable substrate prior to polymeric exposure, a constant microbial density was obtained. The modified ASTM method provides an assessment of the polymeric carbon degradation at any given time. The results of this work have specific significance to the behavior of polymers in a sewage waste treatment plant, where sludge is continuously being acrated, and also for aerobic biodegradation in general.  相似文献   

20.
The natural degradation of monophenylheptamethylcyclotetrasiloxane and 2,6-cis-diphenylhexamethylcyclotetrasiloxane in soil was evaluated under laboratory conditions. Both monophenyl and 2,6-cis underwent rapid degradation in dry soil generating the same products in varying proportions. During the first 24 hr, approximately 99% of the two materials underwent significant chemical transformations forming silanols of various structures, dimethyl cyclic siloxanes of the structure (Me2SiO)x, and rearrangement products (geometrical isomers) of diphenylhexamethylcyclotetrasiloxane. Among the silanols, the following were identified as trimethylsilyl derivatives: HOSiMe2OH, HOSiMePhOH, HOSiMe2OSiMe2OH, HOSiMePhOSiMe2OH, HOSiMePhOSiMePhOH, HOSiMe2OSiMe2OSiMe2OH, HOSiMePhOSiMe2OSiMe2OH, HOSiMe2OSiMePhOSiMe2OH, HOSiMePhSiMe2OSiMePhOH, HOSiMePhOSiMePhOSiMe2OH, HOSiMePhOSiMe2OSiMe2OSiMe2OH, HOSiMe2OSiMePhOSiMe2OSiMe2OH, HOSiMePhOSiMe2OSiMePhOSiMe2OH, HOSiMePhOSiMePhOSiMe2OSiMe2OH, HOSiMePhOSiMe2OSiMe2OSiMePhOH, HOSiMe2OSiMePh-OSiMePhOSiMe2OH. Derivatization was carried out using bis(trimethylsilyl)trifluoroacetamide. Gas chromatography-mass spectrometry and liquid chromatography-mass spectrometry (atmospheric pressure chemical ionization) analyses were used to derive structures. Structures were confirmed by gas chromatography-mass spectrometry comparisons of synthetic standards. Degradation was slower in wet soil. Nevertheless, in 14 days, the chemical transformation was essentially found to be complete as soil was allowed to dry. Detection of phenol as one of the degradation products revealed the occurrence of carbon–silicon bond cleavage promoted by soil.  相似文献   