1.
A respirometric system was used to analyze the biodegradation of high molecular weight (120,000 to 200,000 g mol–1) polylactic acid (PLA) plastic films in soil under laboratory conditions. The respirometric system consisted of air-conditioning pretraps, a soil reactor, and a carbon dioxide (CO2) posttrap. A 200-g homogeneous soil mixture of all-purpose potting soil : manure soil : sand [1 : 1 : 1 (w/w)] and 1.5 g of PLA plastic films in 1 × 1-cm2 squares was added to each bottle. The respirometers were placed in a 28, 40, or 55°C water bath for 182 days. Treatments (three replicates) included native corn starch (positive control), polyethylene (Glad Cling Wrap; negative control), and three PLA films: Ca-I (Cargill Dow Polymers LLC, monolayer), GII (Cargill Dow Polymers LLC, Generation II), and Ch-I (Chronopol; monolayer). The degree of polymer mineralization was indicated by the cumulative CO2 liberated from each respirometer. The initial average mineralization rate and total percentage mineralized of the PLA plastic films at 28, 40, and 55°C was 24.3, 41.5, and 76.9 mg/day with a 27, 45, and 70% carbon loss, respectively. No decrease in soil pH was observed after 182 days of mineralization. Hence, increase in soil temperature drastically enhanced the biodegradation of PLA plastic films in soil under laboratory conditions (P < 0.0001).  相似文献   

2.
Dialdehyde starch (DAS) and zein, a hydrophobic corn protein, were investigated to produce biodegradable plastics with improved water resistance and mechanical properties. In the study, dialdehyde starch and zein ratio, plasticizers, and degree of starch oxidation were examined. Increased molding temperature and level of starch oxidation decreased water absorption of the plastic. Tensile strength and Young's modulus increased with starch oxidation. The biodegradation of starting materials and ground plastic specimens was studied in aerobic soil reactors maintained at 25°C for 180 days. Biodegradation of corn starch, zein, and dialdehyde starch for 180 days produced CO2 equivalent to 64, 63, and 10% of theoretical carbon, respectively. Specimens of molded DAS and zein (3 : 1) plastic showed accelerated CO2 evolution compared to DAS and other raw materials alone. By 180 days, specimens made with starch of low oxidation (1 and 5% oxidized) demonstrated a 60% biodegradation, and specimens with highly oxidized starch (90% oxidized) achieved 37% biodegradation.Paper presented at the Bio/Environmentally Degradable Polymer Society—Third National Meeting, June 6–8, 1994, Boston, Massachusetts.Journal Paper J-15927 of the Iowa Agriculture and Home Economics Experiment Station, Ames, Project No. 3258.  相似文献   

3.
A new test method is described for assessing biodegradation of plastic material under simulated soil conditions. An inert substrate can be activated with soil extract and nutrient and used in place of soil in biodegradation tests. The biodegradation level is evaluated by determining the carbon dioxide (CO2) production released by the test reactors. Effects of substrate nature, solution pH, nutrient composition, soil extract concentration, and activation duration on CO2 production were investigated, and the experimental conditions were optimized. Results obtained with cellulose showed a biodegradation rate of 80% within 28 days. Moreover, with this kind of substrate, reaction products and residues can be easily extracted and analysed.  相似文献   

4.
Hydrocarbon biodegradation is an important process for remediating petroleum hydrocarbons and managing large sites. However, this biodegradation results in what are essentially unavoidable CO2 emissions to the atmosphere. A feasibility assessment was conducted to quantitatively consider reuse options for petroleum brownfields that would offset contaminant respiration emissions rates in the 2 to 10 micromoles CO2 per meters squared per second (μmol CO2 m?2 s?1) typically observed. Under a wide range of solar resource scenarios, placement of solar panels over only a fraction (no more than 35%) of the site footprint is estimated as necessary to achieve an emissions offset. Similarly, placement of one 30‐meter tall wind turbine of moderate rating (approximately 30 to 50 kW) is sufficient to provide an offset for a nominal 1,000 square meters site. For spreading of spent calcium‐rich construction materials, under even a high emissions scenario, the required footprint for the offset is less than the site footprint. While these approaches appear feasible, revegetation as forestland is estimated as sufficient only at contaminant respiration rates up to 2 μmol CO2 m?2 s?1. Revegetation as rangeland and cropland, which sequesters CO2 mainly in soil organic carbon, is estimated as requiring more than the site footprint under many contaminant respiration rates. Revegetation as a wetland fares slightly better from a carbon storage perspective, but it also has the potential for N2O and CH4 emissions that may largely undo the benefit from sequestration in soil organic matter. Overall, the results indicate several methods that are viable for achieving emissions offsets and a quantitation method that can be honed with site‐specific input parameters as appropriate.  相似文献   

5.
In the present project, twenty materials (e.g., polyhydroxybutyrate-hydroxyvalerate, polycaprolactone, cellulose acetate, polyacticacid, polyethylene), representing varied biodegradability levels were studied. An aerobic respirometric test, based on the CEN Draft, was setup. The biodegradability of each plastic film was evaluated by measuring the percentage of carbon converted into CO2 during 35 days. The values of the CO2 production were plotted versus days as a cumulative function. In order to reduce its number of points, the cumulative curve was modeled using a sigmoïd function (Hill sigmoïd). This model was compared to one found in the literature. A i 2 test showed that the biodegradation curve was more accurately fitted with the model than the previous one. Three kinetic parameters were determined by this Hill model: one represents the maximal percentage of carbon converted into CO2, the second the half-life time in days of the degrading part of the material and the third one the curve radius.In addition, the following analyses were carried out on each sample: elemental analysis, thickness, hydrophobicity and surface free energy measurements. In order to compress the information and to keep only relevant pieces, these parameters were submitted to a Principal Component Analysis. PCA found linear combinations of variables that describe major trends in the data. The two principal components which separate groups of materials were closely related to a chemical and a physical axis respectively. Materials showing a high biodegradability were related to high oxygen (and nitrogen) contents and low hydrophobicity: Material thickness did not influence the likeliness to biodegradability described by the maximum biodegradation rate. Finally, this study established the correlation between the biodegradation and the structure of biopolymers.  相似文献   

6.
To simulate the behavior of agricultural mulch coextruded poly(lactic acid)(PLA)/starch films, two stages were carried out. The first was an ultraviolet treatment (UV) at 315 nm, during which glass transition temperature Tg, weight, and molecular weight (MW) decreased and a separation between PLA and starch phase was observed. For the second stage, the mineralization of the carbon of the material was followed using the ASTM (D 5209–92 and 5338–92) and ISO/CEN (14852 and 14855) standard procedures. To measure the biodegradability of polymer material, the assessment of the carbon balance allowed determination of the distribution between the carbon rate used to the biomass synthesis or the respiration process (released CO2), as well as the dissolved organic carbon into the culture medium and the carbon in the residual insoluble material. The influence of the nature of the medium and the standardized procedures on the final rate of biodegradation was investigated. Whatever the standardized method, the biodegradation percentage was significantly stronger in liquid medium (92.4–93.4) than on inert medium (80–83%). In the case of the compost process, only released CO2 was measured and corresponded to 79.1–80.3%.  相似文献   

7.
This study investigates the processability and biodegradability of composite bioplastic materials. Biocomposites were processed using twin-screw compounding of the bioplastic poly(butylene succinate) (PBS) with bio-based fillers derived from co-products of biofuel production. An extensive biodegradability evaluation was conducted on each biocomposite material, as well as the base materials, using respirometric testing to analyze the conversion of organic carbon into carbon dioxide. This evaluation revealed that the presence of meal-based fillers in the biocomposites increased the rate of biodegradation of the matrix polymer, degrading at a faster pace than both the pure PBS polymer and the switchgrass (SG) composite. This degradation was further confirmed using FT-IR and thermal analysis of the material structure before and after biodegradation. The increased biodegradation rate is attributed to the high concentration of proteins in the meal-based composites, which enhanced the hydrolytic biodegradation of the material and facilitated micro-organism growth. The SG-based composite degraded slower than the pure polymer due to its lignin content, which degrades via a different mechanism than the polymer, and slowed the biodegradation process.  相似文献   

8.
This paper discusses the results of biodegradability tests of natural fibers used by the automotive industry, namely: coir, coir with latex, and sisal. The biodegradation of coir, coir with latex, and of sisal fibers was determined by monitoring the production of carbon dioxide (CO2) (IBAMA—E.1.1.2, 1988) and fungal growth (DIN 53739, 1984). The contents of total extractives, lignin, holocellulose, ashes, carbon, nitrogen and hydrogen of the fibers under study were determined in order to ascertain their actual content and to understand the results of the biodegradation tests. The production of CO2 indicated low biodegradation, i.e., about 10% in mass, for all the materials after 45 days of testing; in other words, no material inhibited glucose degradation. However, the percentage of sisal fiber degradation was fourfold higher than that of coir with latex in the same period of aging. The fungal growth test showed a higher growth rate on sisal fibers, followed by coir without latex. In the case of coir with latex, we believe the fungal growth was not intense, because natural latex produces a bactericide or fungicide for its preservation during bleeding [1]. An evaluation of the materials after 90 days of aging tests revealed breaking of the fibers, particularly sisal and coir without latex, indicating fungal attack and biodegradation processes.  相似文献   

9.
The standard test method ASTM D 5988-96 for determining the degree and rate of aerobic biodegradation of plastic materials in contact with soil was applied to poly(3-hydroxybutyrate) and poly(-caprolactone). The method proved to be reliable and supplied reproducible measurements of CO2 production, provided potassium (instead of barium) hydroxide was used as a trapping solution. The trends of CO2 evolution, as a function of time, observed for the degradation of polymer powders in soil are similar to those predicted by simple first order kinetics in solution. The experimental data are described by a Michaelis–Menten type model, which accounts for the heterogeneity of the polymer-soil system. The kinetic equation deduced predicts the degradation rate to the proportional to the exposed polymer surface area.  相似文献   

10.
The biodegradability properties of poly(ɛ-caprolactone) (PCL) and modified adipate-starch (AS) blends, using Edenol-3203 (E) as a starch plasticizer, were investigated in laboratory by burial tests of the samples in previously analyzed agricultural soil. The biodegradation process was carried out using the respirometric test according to ASTM D 5988-96, and the mineralization was followed by both variables such as carbon dioxide evolution and mass loss. The results indicated that the presence of AS-E accelerated the biodegradation rate as expected.  相似文献   

11.
Soil respiration is a large C flux which is of primary importance in determining C sequestration. Here we ask how it is altered by atmospheric CO2 concentration and N additions. Swards of Lolium perenne L. were grown in a Eutric cambisol under controlled conditions with and without the addition of 200 kg NO? 3 ?N ha?1, at either 350 ppm or 700 ppm CO2, for 3 months. Soil respiration and net canopy photosynthesis were both increased by added N and elevated CO2, but soil respiration increased proportionately less than fixation by photosynthesis. Thus, both elevated CO2 and N appeared to increase potential C sequestration, although adding N at elevated CO2 reduced the C sequestered as a proportion of that fixed relative to elevated CO2 alone. Across all treatments below-ground respiratory C losses were predicted by root biomass, but not by soil solution C and N concentrations. Specific root-dependent respiration was increased by elevated CO2, such that below-ground respiration per unit biomass and per unit plant N was increased.  相似文献   

12.
Effective sequestration of carbon dioxide (CO2) by algae reduces greenhouse gases effect on global warming. Algae biomass or residual such as biomeal from algae biofuel processing can be judiciously used for industrial applications such as fertilizer, animal feed, and plastics. Conversion of algae into useful plastic materials can be accomplished by extrusion technology. During algal plastic manufacturing, up to 20% thermoplastic algal blends can be fixated into or encapsulated by a non-biodegradable polymer such as polyolefin, which is known to be resistant to abiotic or biotic degradation. As a result, CO2 that is captured by algae through photosynthesis is permanently stored in a form of biomass and will not be released back into the atmosphere. The extrusion of microalgae reported in this article is a novel process to sequester CO2 and at the same time it makes a good use of the algae biomass in plastic manufacturing. Mechanical properties of the thin plastic films containing microalgae are comparable to the neat polyurethane or polyethylene films. Injection molded articles containing microalgae are dimensionally stable. However, a lower tensile strength, especially elongation at break, is observed in comparison to the neat polypropylene.  相似文献   

13.
Soil respiration is a large C flux which is of primary importance in determining C sequestration. Here we ask how it is altered by atmospheric CO2 concentration and N additions. Swards of Lolium perenne L. were grown in a Eutric cambisol under controlled conditions with and without the addition of 200 kg NO 3 –N ha–1, at either 350 ppm or 700 ppm CO2, for 3 months. Soil respiration and net canopy photosynthesis were both increased by added N and elevated CO2, but soil respiration increased proportionately less than fixation by photosynthesis. Thus, both elevated CO2 and N appeared to increase potential C sequestration, although adding N at elevated CO2 reduced the C sequestered as a proportion of that fixed relative to elevated CO2 alone. Across all treatments below-ground respiratory C losses were predicted by root biomass, but not by soil solution C and N concentrations. Specific root-dependent respiration was increased by elevated CO2, such that belowg-round respiration per unit biomass and per unit plant N was increased.  相似文献   

14.
Utilizing stable carbon isotope data to account for aceticlastic and non-aceticlastic pathways of methane generation, a model was created to describe laboratory batch anaerobic decomposition of cellulosic materials (office paper and cardboard). The total organic and inorganic carbon concentrations, methane production volume, and methane and CO2 partial pressure values were used for the model calibration and validation. According to the fluorescent in situ hybridization observations, three groups of methanogens including strictly hydrogenotrophic methanogens, strictly aceticlastic methanogens (Methanosaeta sp.) and Methanosarcina sp., consuming both acetate and H2/H2CO3 as well as acetate-oxidizing syntrophs, were considered. It was shown that temporary inhibition of aceticlastic methanogens by non-ionized volatile fatty acids or acidic pH was responsible for two-step methane production from office paper at 35 °C where during the first and second steps methane was generated mostly from H2/H2CO3 and acetate, respectively. Water saturated and unsaturated cases were tested. According to the model, at the intermediate moisture (150%), much lower methane production occurred because of full-time inhibition of aceticlastic methanogens. At the lowest moisture, methane production was very low because most likely hydrolysis was seriously inhibited. Simulations showed that during cardboard and office paper biodegradation at 55 °C, non-aceticlastic syntrophic oxidation by acetate-oxidizing syntrophs and hydrogenotrophic methanogens were the dominant methanogenic pathways.  相似文献   

15.
Mater-Bi: Properties and biodegradability   总被引:1,自引:0,他引:1  
This paper examines the biodegradability of a new class of materials based on starch and vinylalcohol copolymers, which have been commercialized under the Mater-Bi trademark. Particular attention is given to the biodegradation process for natural and synthetic components of different Mater-Bi grades for film blowing in an aerobic respirometric test, in a SCAS (semicontinuous activated sludge) test, and by submersion in lake water. The correlation between morphology and biodegradation behavior is also considered. Taking into account the prior art on biodegradation of insoluble substrates, a two-step mechanism is proposed for Mater-Bi products.  相似文献   

16.
Increased energy consumption due to industrial growth has increased the levels of carbon dioxide (CO2) emission being released into the atmosphere. CO2 emission is a type of greenhouse gas which is a major cause of global warming. Since the issue of CO2 emissions has drawn much attention in recent years, the development of CO2 capture technology has become a necessity. Although CO2 adsorbents are still at the early development stage, it has been suggested that CO2 adsorbents are the most effective technology in controlling CO2 emissions. Solid adsorbents have great potential as an alternative method to conventional adsorbents in adsorbing CO2. In this paper, low cost adsorbents including activated carbon, zeolites, mesoporous silica and clays are discussed in terms of adsorbent preparation methods and CO2 adsorption capacity. The low cost adsorbents are mainly derived from waste materials such as fly ash, steel slag, red mud, bagasses wastes and wood wastes. Besides that, natural resources such as clays have also been applied as low cost CO2 adsorbents. Surface modifications have also been applied to the low cost adsorbents, including metal ion exchange and amine impregnation to enhance CO2 adsorption capacity. In the last section, the current status of CO2 adsorbents is summarized and future trends are discussed briefly to predict the potential materials which can be applied as CO2 adsorbents.  相似文献   

17.
Biodegradability under composting conditions is assessed by test methods, such as ASTM D 5338-92, based on the measurement of CO2 released by test materials when mixed with mature compost and maintained in a controlled composting environment. However, in real composting, biodegradation occurs in fresh waste. To clarify this point, the biodegradation of paper and of a starch-based biodegradable thermoplastic material, Mater-Bi ZI01U, was followed by measuring the weight loss of samples introduced either into a mature compost or into a synthetic waste. The weight loss in mature compost was higher at the beginning but tended to decrease; in synthetic waste a first lag phase was followed by an exponential phase. Complete degradation of paper was noticed simultaneously in the two substrates (after 25 days). The bulkier Mater-Bi samples were fully degraded after 20 days in fresh waste, but after 45 days in mature compost. Therefore, the test methods using mature compost as a substrate can possibly underestimate the biodegradation rate occurring in fresh waste, i.e., in real composting plants, and have to be considered as conservative test methods. The test procedure described in this paper seems very suitable as a screening method to verify the compostability of plastic materials in a composting environment.  相似文献   

18.
The ASTM D5210-91 protocol for evaluating the biodegradability of a polymer was examined. The reactor design was modified not only to account for the total CO2 evolved but also to allow for the simultaneous carbon assessment in microbes, soluble products, and solid samples. Improvements in the test procedure were implemented such as (1) refining the CO2 pretrap and posttrap design, (2) optimizing the carbon dioxide removal efficiency, (3) accounting for the total polymeric carbon, (4) standardizing the inoculum, and (5) revising the nutrient medium. By growing the sludge on a suitable substrate prior to polymeric exposure, a constant microbial density was obtained. The modified ASTM method provides an assessment of the polymeric carbon degradation at any given time. The results of this work have specific significance to the behavior of polymers in a sewage waste treatment plant, where sludge is continuously being acrated, and also for aerobic biodegradation in general.  相似文献   

19.
Gasification is considered to be an effective process for energy conversion from various sources such as coal, biomass, and waste. Cleanup of the hot syngas produced by such a process may improve the thermal efficiency of the overall gasification system. Therefore, the cleanup of hot syngas from biomass gasification using molten carbonate is investigated in bench-scale tests. Molten carbonate acts as an absorbent during desulfurization and dechlorination and as a thermal catalyst for tar cracking. In this study, the performance of molten carbonate for removing H2S was evaluated. The temperature of the molten carbonate was set within the range from 800 to 1000 °C. It is found that the removal of H2S is significantly affected by the concentration of CO2 in the syngas. When only a small percentage of CO2 is present, desulfurization using molten carbonate is inadequate. However, when carbon elements, such as char and tar, are continuously supplied, H2S removal can be maintained at a high level.To confirm the performance of the molten carbonate gas-cleaning system, purified biogas was used as a fuel in power generation tests with a molten carbonate fuel cell (MCFC). The fuel cell is a high-performance sensor for detecting gaseous impurities. When purified gas from a gas-cleaning reactor was continuously supplied to the fuel cell, the cell voltage remained stable. Thus, the molten carbonate gas-cleaning reactor was found to afford good gas-cleaning performance.  相似文献   

20.
Testing biodegradability of plastics under varied conditions of the environment as well as under laboratory conditions in accordance with valid international standards is very laborious, lengthy and often also economically demanding. For this reason, applicability was verified of gas chromatography to analyze gaseous phase when investigating the biodegradation course of plastics in an aqueous environment as an alternative to customary employed methods. A mathematical model of acid–basic CO2 equilibrium in a gas–liquid system was worked out, enabling to determine quantity of produced CO2 through chromatographic analysis of gaseous phase, in dependence on ratio of liquid and gas phase volumes (V l/V g) and on actual pH of liquid phase. Experimental conditions for organizing the tests were optimized. A ratio that proved suitable was V l/V g ≅ 0.1 at pH ≈ 7.1 of liquid phase. Under these test conditions, biodegradability of model samples, PHB, Gellan gum and Xanthan gum, was explored; course of biodegradation was studied through produced CO2 (values ) determined by analyzing gaseous phase through gas chromatography on the one hand, and through customary “titration” procedure on the other. With water-soluble polymers, the decrement in dissolved organic carbon (values D DOC) was also studied. Difference between values does not exceed 5%. The procedures in question are alternative “substituting” procedures for observing course of aerobic biodegradation of substances in an aqueous environment.  相似文献   