Rengaraj S  Li XZ 《Chemosphere》2007,66(5):930-938
A series of Bi(3+)-doped TiO(2) (Bi(3+)-TiO(2)) catalysts with a doping concentration up to 2wt% were prepared by a sol-gel method. The prepared photocatalysts were characterized by different means to determine their chemical composition, surface structure and light absorption properties. The photocatalytic activity of different Bi(3+)-TiO(2) catalysts was evaluated in the photocatalytic reduction of nitrate in aqueous solution under UV illumination. In the experiments, formic acid was used as a hole scavenger to enhance the photocatalytic reduction reaction. The experiments demonstrated that nitrate was effectively degraded in aqueous Bi(3+)-TiO(2) suspension by more than 83% within 150min, while the pH of the solution increased from 3.19 to 5.83 due to the consumption of formic acid. The experimental results indicate that the presence of Bi(3+) in TiO(2) catalysts substantially enhances the photocatalytic reaction of nitrate reduction. It was found that the optimal dosage of 1.5wt% Bi(3+) in TiO(2) achieved the fastest reaction of nitrate reduction under the experimental condition. Bismuth ions deposit on the TiO(2) surface behaves as sites where electrons accumulate. Better separation of electrons and holes on the modified TiO(2) surface allows more efficient channeling of the charge carriers into useful reduction and oxidation reactions rather than recombination reactions. Two intermediate products of nitrite and ammonia during the reaction were also monitored to explore the possible mechanisms of photoluminescence quenching and photocatalytic reduction in the context of donor-acceptor interaction with electron trapping centers.  相似文献   

2.
采用酸催化的溶胶-凝胶法制备了一系列Fe^3+掺杂TiO2/凹凸棒(Fe^3+-TiO2/ATP)复合光催化剂材料。在可见光条件下,以亚甲基蓝(MB)溶液的光催化降解反应,评价了样品的光催化性能,研究了TiO2负载量、Fe^3+掺杂量和焙烧温度对复合材料光催化性能的影响。在单因素实验的基础上,采用正交实验设计(L25(53))优化了催化剂的制备条件。光催化实验结果表明,MB在复合材料上的光催化降解反应遵循Langmuir-Hinshelwood(L-H)动力学模型。正交实验结果表明,当TiO2负载量为15%、Fe^3+掺杂量为0.5%和焙烧温度为550℃时,得到的复合材料对MB的光催化降解效率最佳,测得表观反应速率常数kapp为6.09×10^-3min^-1,反应4 h后MB的降解率(Dt)可达75.88%,相同实验条件下与P25(1.51×10^-3min^-1)相比较,反应速率提高了4.03倍,降解率提高了45.05%。另外,复合材料的沉降性能优于P25,易于分离,是一类有应用前景的复合光催化剂。敏世雄王芳魏立强王永生冯雷佟永纯韩玉琦  相似文献   

3.
模拟室内环境下掺杂TiO_2纳米晶体的光催化性能   总被引:1,自引:0,他引:1  
采用环境测试舱模拟可见光下的室内环境,以甲醛气体的光催化降解为探针反应,评价了通过溶胶-凝胶法分别制备的8种(银Ag、铜Cu、铁Fe、钨W、铈Ce、镧La、硫S和氯C l)掺杂TiO2纳米晶体的光催化活性及对甲醛气体的去除效果。用X射线衍射、激光粒度分析和紫外-可见分光光谱表征了掺杂钠米TiO2的微晶尺寸、晶体结构与光学性能。结果表明,Cu掺杂可以提高TiO2对氧的吸附能力,减少纳米粒子表面光生电子与光生空穴的复合,使TiO2的光吸收带边发生红移且有利于对可见光的吸收,从而使Cu掺杂TiO2在模拟室内环境下光催化甲醛气体的能力得到明显提高。  相似文献   

4.
TiO2结构对光催化性能的影响及其提高的途径   总被引:1,自引:0,他引:1  
文中介绍了TiO2的晶体结构与表面态性质对其光催化活性的影响,综述了近年来有关贵金属沉积、金属离子掺杂、表面光敏化、复合半导体、表面酸化和无机模板合成纳米粒子等改性技术的研究现状.还简单地介绍了电化学、微波场和超声波等外加场辅助光催化的进展.  相似文献   

5.
Hou YD  Wang XC  Wu L  Chen XF  Ding ZX  Wang XX  Fu XZ 《Chemosphere》2008,72(3):414-421
Mesoporous nanocrystalline N-doped SiO2/TiO2 visible-light photocatalysts were prepared by treating SiO2/TiO2 xerogels in a flow of nitrogen gas bubbled through concentrated ammonia solution. Structural characterization and performance analysis results revealed that the addition of SiO2 remarkably altered the phase composition, specific surface area, microstructure, as well as the photocatalytic activity of N-doped TiO2. The presence of SiO2 in N-doped TiO2 particles suppressed the formation of rutile phase and the crystal growth of N-doped TiO2 particles during thermal calcinations. When weight ratio of SiO2/TiO2 was in 0.05-0.20, the N-doped SiO2/TiO2 exhibited higher photocatalytic activity than the N-doped TiO2, and optimum ratio was found to be 0.05. The enhanced photocatalytic activity could be attributed to the higher specific area, larger pore volume, and more surface hydroxyl groups in the catalyst.  相似文献   

6.
纳米TiO2光催化氧化去除水中痕量双氯芬酸的研究   总被引:1,自引:0,他引:1  
以TiCl4为前驱体,采用水解法经不同温度煅烧制备了具有不同理化性能的纳米TiO2光催化剂。利用X射线衍射(XRD)、扫描电子显微镜(SEM)、透射电子显微镜(TEM)、物理吸附仪、紫外—可见光漫反射吸收光谱(UV-Vis DRS)等手段对纳米TiO2的晶相结构、粒径、孔径分布以及禁带宽度等进行了表征。以蒸馏水配制的双氯芬酸溶液为目标物,进行了纳米TiO2光催化氧化去除双氯芬酸的活性测试,研究了纳米TiO2的理化性能与光催化氧化活性之间的关系。结果表明,经400℃煅烧制得的纳米TiO2样品具有最高的光催化氧化活性,其在紫外光照射60min下对双氯芬酸的去除率为98%左右,比单独紫外光照射高出85百分点。纳米TiO2光催化氧化去除双氯芬酸的反应近似一级反应动力学模型,其中经400℃煅烧制得的纳米TiO2光催化氧化去除双氯芬酸的表观反应速率常数为0.054 54min-1,是普通商用TiO2的2倍左右,与德国Degussa P-25TiO2的光催化氧化活性最相近。  相似文献   

7.
模拟自然条件下的可见光,以甲醛的光催化降解为探针反应,评价了通过溶胶-凝胶法分别制备的8种(银Ag、铜Cu、铁Fe、钨W、铈Ce、镧La、硫S、氯Cl)掺杂TiO2纳米晶体的光催化活性及对甲醛水溶液的去除效果。用X射线衍射、激光粒度分析和紫外-可见分光光谱表征了掺杂纳米TiO2的微晶尺寸、晶体结构与光学性能。结果表明:Ce离子尽管有较大的半径但是主要还是掺杂到晶格中,Ce掺杂可以促进TiO2由非正分锐钛矿相向锐钛矿相和金红石相的转变,抑制载流子复合,使TiO2的光吸收带边发生红移且有利于对可见光的吸收,从而使Ce掺杂TiO2在模拟可见光下光催化甲醛水溶液的能力得到明显提高。  相似文献   

8.
采用自制的负载型纳米RuO2-TiO2光催化剂对农药厂生产废水进行光电催化降解试验。考察了煅烧时间、催化剂用量、光辐照强度、电流密度、废水初始pH值和反应时间对废水COD和色度去除率的影响。结果表明,自制光催化剂光电催化性能显著,最佳光电催化活性是同样降解条件下、同样含量的Degussa P-25 TiO2的1.38倍,是Ru0.3Ti0.7O2的1.81倍。其COD和色度去除率分别为64.3%和95.2%。  相似文献   

9.
Liu H  Ma HT  Li XZ  Li WZ  Wu M  Bao XH 《Chemosphere》2003,50(1):39-46
In this study, conventional TiO2 powder was heated in hydrogen (H2) gas at a high temperature as pretreatment. The photoactivity of the treated TiO2 samples was evaluated in the photodegradation of sulfosalicylic acid (SSA) in aqueous suspension. The experimental results demonstrated that the photodegradation rates of SSA were significantly enhanced by using the H2-treated TiO2 catalysts and an optimum temperature for the H2 treatment was found to be of 500-600 degrees C. The in situ electron paramagnetic resonance (EPR) signal intensity of oxygen vacancies (OV) and trivalent titanium (Ti3+) associated with the photocatalytic activity was studied. The results proved the presence of OV and Ti3+ in the lattice of the H2-treated TiO2 and indicated that both were contributed to the enhancement of photocatalytic activity. Moreover, the experimental results presented that the EPR signal intensity of OV and Ti3+ in the H2-treated TiO2 samples after 10 months storage was still significant higher than that in the untreated TiO2 catalyst. The experiment also demonstrated that the significant enhancement occurred in the photodegradation of phenol using the H2-treated TiO2.  相似文献   

10.
以钼酸铵和氨水分别为钼源和氮源,采用溶胶-凝胶法制备了Mo-N-TiO2光催化剂,并对其进行了XRD、XPS和UV-visDRS表征。XRD结果表明,Mo、N共掺杂有效抑制了TiO2晶粒的生长,提高了TiO2由锐钛矿向金红石相的转变温度。UV-vis表明,Mo-N-TiO2光催化剂可见光吸收能力增强,吸收带边明显"红移",且钼酸铵添加量(相对TiO2)为0.5%的样品"红移"程度最大,最大吸收带边为550 nm。XPS分析结果表明,Mo取代了TiO2晶格中的部分Ti4+,以Mo6+形式存在的,而N以Ti—N及N—Ti—O形式存在。以罗丹明B为模型污染物,重点考察了钼酸铵添加量与焙烧温度对Mo-N-TiO2光催剂性能的影响。结果表明,400℃焙烧下、钼酸铵添加量为0.5%的样品催化活性最好。模拟太阳光下光照120min对罗丹明B的降解率达到96.8%,是纯TiO2的2.42倍。  相似文献   

11.
Effect of ZnFe2O4 doping on the photocatalytic activity of TiO2   总被引:9,自引:0,他引:9  
Liu GG  Zhang XZ  Xu YJ  Niu XS  Zheng LQ  Ding XJ 《Chemosphere》2004,55(9):1287-1291
The photocatalytic oxidation of the organic pollutants with the TiO2 as photocatalyst has been widely studied in the world, and many achievements have been got. The degradation of pollutants is highly related with the photocatalytic activity of TiO2. It is demonstrated that doping ions or oxides to TiO2 is one way to enhance the photocatalytic activity of TiO2. In this paper, the ZnFe2O4-doped TiO2 nanoparticles were prepared from butyl titanate by a sol-gel method and characterized by means of X-ray diffraction (XRD) and transmission electron microscopy (TEM). The results showed that when TiO2 was doped with ZnFe2O4, its particle size will decrease and its crystal structure will partly transform from anatase to rutile. The photocatalytic activity of the elaborated powders was studied following the degradation of Rhodamine B. The results showed that doping ZnFe2O4 to TiO2 will enhance the photocatalytic activity of TiO2 and that ZnFe2O4-doped TiO2 in the coexistence of anatase and rutile has higher efficiency for the degradation of Rhodamine B than that in the anatase phase alone. Also the different role of O2 in the direct photolysis and photocatalysis of Rhodamine B was discussed.  相似文献   

12.
Li XZ  Fan CM  Sun YP 《Chemosphere》2002,48(4):453-460
This study aimed at improving the photocatalytic (PC) oxidation of humic acids (HA) in TiO2 suspensions by adding cationic ion such as calcium or magnesium. A set of tests was first conducted in the dark to study the adsorption of HA onto TiO2 in suspensions at different pH and calcium concentrations. The experiment demonstrated that the adsorption of HA onto the TiO2 particles was either pH-dependent or calcium strength-dependent due to electrostatic interaction and calcium ion bridging. The photodegradation of HA in the presence of UV irradiation was investigated as a function of pH and the concentration of calcium and magnesium ions. The results showed that the adsorption behavior between HA and TiO2 played a very important role during the PC oxidation process. The PC oxidation could be enhanced at neutral pH by increasing the cation strength. The kinetics of HA PC degradation in TiO2 suspensions with different initial concentrations was also studied using the Langmuir-Hinshelwood model.  相似文献   

13.
BACKGROUND: The photocatalytic degradation of pyrene under UV (125 W Hg-Arc, 10.4 mW/cm2) irradiation of TiO2 aqueous suspension has been found to be highly improved with the dissolved transition metal ions like Cu2+, Fe3+, Ag+, and Au3+, etc. As the reduction potential of these metals lies below the conduction band (CB) position (?0.1 eV) of TiO2, the photoexcited electron transfer occurs more readily and reduces electron–hole recombination rate. Therefore, it has a beneficial influence on the photocatalytic ability of TiO2 because of rapid Fermi energy equilibrium between the CB of TiO2 and its surface adsorbed metal ions. RESULTS AND DISCUSSION: The Fermi level is referred to as the electrochemical potential and plays an important role in the band theory of solids. When metal and semiconductor are in contact, electron migration from photoirradiated semiconductor to the deposited metal occurs at the interface until two Fermi levels equilibrate and enhanced the photocatalytic activity of semiconductor photocatalyst. Ni2+ having more negative reduction potential (?0.25 eV) than the CB of TiO2 imparts negligible co-catalytic activity to TiO2 photoreaction. It also revealed that loading of Au3+ ions displayed higher degradation rate of pyrene than Au photodeposition. Furthermore, when the amount of dissolved Fe+3 and Au3+ ions gradually increases from 0.1 to 2 wt.%, the pyrene photodecomposition rate also become faster.  相似文献   

14.
Yang JK  Lee SM 《Chemosphere》2006,63(10):1677-1684
The removal efficiencies of Cr(VI) and HA, using a TiO(2)-mediated photocatalytic process, were investigated with variations in the pH, TiO(2) dosage and Cr(VI)/HA ratio. During the photocatalytic reaction, the total removal of Cr(VI) occurred through adsorption onto TiO(2), as well as its reduction to Cr(III). However, oxidation and adsorption were identified as important removal processes for the treatment of HA. Due to the anionic type adsorption onto TiO(2) and its acid-catalyzed photocatalytic reduction, the removal of Cr(VI) decreased with increasing pH, while that of HA increased with increasing pH. The TiO(2) dosage was also an important parameter for the removal of Cr(VI). As the TiO(2) dosage was increased to 2.5 g l(-1), the removal of Cr(VI) was continuously enhanced, but decreased at dosages above 3 g l(-1) due to the increased blockage of the incident UV light used for the photocatalytic reaction. The removal of Cr(VI) was greatly enhanced when the system contained both HA and Cr(VI) compared to Cr(VI) alone. Also, the removal of HA was greatly enhanced when the system contained both HA and Cr(VI) compared to HA alone. The removal of Cr(VI) was continuously enhanced as the HA concentration gradually increased; however, no further increase was observed above 20 mg l(-1) HA due to the increased absorption of the UV light. This result supports that the photocatalytic reaction, with illuminated TiO(2), could be applied to more effectively treat wastewater containing both Cr(VI) and HA than that containing a single species only.  相似文献   

15.
Photocatalytic degradation of lignin using Pt/TiO2 as the catalyst   总被引:1,自引:0,他引:1  
Ma YS  Chang CN  Chiang YP  Sung HF  Chao AC 《Chemosphere》2008,71(5):998-1004
Photocatalytic degradation of lignin was studied with the use of catalysts TiO(2) and Pt/TiO(2). The influence of several experimental parameters, i.e. pH, catalyst dosage and illumination on lignin degradation was investigated. The results showed that application of UV irradiation alone has almost no effect on the reduction of dissolved organic carbon (DOC) and American Dye Manufacture Institute value (ADMI). However, the addition of TiO(2) and Pt/TiO(2) reduced the original DOC (251 mg l(-1)) by more than 40% within 30 min of treatment and the reaction can be simulated with pseudo-first order kinetics. Rapid degradation of lignin was observed in acidic solution using either TiO(2) or Pt/TiO(2) as the catalyst compared to high pH cases. The content of Pt in the Pt/TiO(2) catalyst is 1%. In addition, too much catalyst addition has not increased the DOC and ADMI reduction proportionally. The investigation also indicated that the photocatalytic degradation rates could be enhanced 1-6 times faster after doping TiO(2) with Pt in different pH cases. A modified Nernst type model was adopted to simulate the decoloring process using TiO(2) and Pt/TiO(2) based on the profiles of oxidation reduction potential during the photocatalytic reaction. The developed equation can be used to predict the color removal efficiency of lignin wastewater by the photocatalytic process.  相似文献   

16.
Photocatalytic degradation of pentachlorophenol on TiO2 sol-gel catalysts   总被引:6,自引:0,他引:6  
The photocatalytic degradation of pentachlorophenol (PCP) in aqueous solution was investigated using TiO2 catalysts. The samples were prepared by the sol-gel method using different gelation pH and different calcination temperatures. The solids were characterized by specific surface area, X-ray diffraction, UV-Vis absorbance, FTIR and pentachlorophenol adsorption. The catalytic activity of the solids was evaluated in a conventional photoreactor at 298 K using 30 ppm of pentachlorophenol. It was found that the reaction follows a first-order reaction and the kinetic constant values change slightly with the pH of gelation and more significantly with the calcination temperature.  相似文献   

17.
Photocatalytic oxidation of gaseous DMF using thin film TiO2 photocatalyst   总被引:2,自引:0,他引:2  
Chang CP  Chen JN  Lu MC  Yang HY 《Chemosphere》2005,58(8):1071-1078
The heterogeneous photocatalytic oxidation of gaseous N,N'-dimethylformamide (DMF) widely used in the manufacture of synthetic leather and synthetic textile was investigated. The experiments were carried out in a plug flow annular photoreactor coated with Degussa P-25 TiO2. The oxidation rate was dependent on DMF concentration, reaction temperature, water vapor, and oxygen content. Photocatalytic deactivation was observed in these reactions. The Levenspiel deactivation kinetic model was used to describe the decay of catalyst activity. Fourier transform infrared (FTIR) was used to characterize the surface and the deactivation mechanism of the photocatalyst. Results revealed that carbonylic acids, aldehydes, amines, carbonate and nitrate were adsorbed on the TiO2 surface during the photocatalytic reaction. The ions, NH4+ and NO3-, causing the deactivation of catalysts were detected on the TiO2 surface. Several treatment processes were applied to find a suitable procedure for the regeneration of catalytic activity. Among these procedures, the best one was found to be the H2O2/UV process.  相似文献   

18.
Li SX  Zheng FY  Liu XL  Wu F  Deng NS  Yang JH 《Chemosphere》2005,61(4):589-594
The surface of nanometer size TiO(2) was simply and fast modified by chemical adsorption in saturated solution of 5-sulfosalicylic acid. After surface modification, a stable, yellow surface complex was formed quickly, the wavelength response range of TiO(2) was expanded, it has obvious absorption in the region from 320 to 450 nm; the adsorption efficiency of p-nitrophenol (PNP) by TiO(2) was enhanced from 42% to 84%. The photocatalytic activity was tested on the degradation of PNP. The influences of catalyst and its dosage, pH value, and PNP concentration on the degradation were investigated. On optimal photodegradation conditions, including initial pH 4.0, PNP 5 mg l(-1), catalyst 100 mg, irradiation time 120 min with 160 W high-pressure mercury lamp, the degradation efficiency of PNP was increased from 40% to 88% after surface modification. Surface modification led not only to an increase in the light utilization, but also improved the surface coverage of PNP in comparison with the pure TiO(2). Both of these factors are crucial for the photocatalytic activity of heterogeneous photocatalysis, especially for photodegradation of benzenoid pollutants.  相似文献   

19.
V/Ce共掺杂TiO2光催化降解甲醛的实验研究   总被引:1,自引:0,他引:1  
采用溶胶-凝胶法制备了不掺杂、V掺杂、Ce掺杂、V/Ce共掺杂纳米TiO2光催化剂,并将其分别负载于瓷砖上,利用X射线衍射分析(XRD)和扫描电镜分析(SEM)技术对薄膜样品的结构和形貌进行了表征。通过对甲醛的降解实验评价光催化剂的光催化活性。实验结果表明,光催化剂的负载量、共掺杂离子的掺杂量、掺杂配比、煅烧温度影响纳米TiO2的光催化活性。V/Ce共掺杂TiO2光催化剂产生了协同效应,其光催化活性优于纯TiO2和单掺杂TiO2样品。  相似文献   

20.
附载型复合光催化剂TiO2·SiO2/beads降解有机磷农药   总被引:5,自引:0,他引:5  
研究以四异丙醇钛 [Ti( iso- O C3 H7) 4]、硅酸乙酯为原料 ,以空心玻璃微球为载体 ,用溶胶—凝胶法制备可漂浮附载型复合光催化剂 Ti O2 · Si O2 / beads的过程 ,利用附载型复合光催化剂降解有机磷农药。结果表明 ,复合型光催化剂 Ti O2 · Si O2 摩尔比存在最佳值 ,n ( Ti O2 ) / m ( Si O2 ) =30 / 70时 ,光催化剂活性最高 ,其活性是同样降解条件下、同样含量 Degussa P- 2 5Ti O2 的 2倍左右。该光催化剂比表面大 ,吸附性强。并用 XRD和 SEM对附载型复合光催化剂进行表征  相似文献   