Resin adsorption and subsequent electrodeposition were used for nickel recovery.Treated wastewater can meet the Electroplating Pollutant Discharge Standard.The spent resin is completely regenerated by 3 BV of 4% HCl solution.95.6% of nickel in concentrated eluent was recovered by electrodeposition. Effective recovery of high-value heavy metals from electroplating wastewater is of great significance, but recovering nickel ions from real electroplating wastewater as nickel sheet has not been reported. In this study, the pilot-scale fixed-bed resin adsorption was conducted to recover Ni(II) ions from real nickel plating wastewater, and then the concentrated Ni(II) ions in the regenerated solution were reduced to nickel sheet via electrodeposition. A commercial cation-exchange resin was selected and the optimal resin adsorption and regeneration conditions were investigated. The resin exhibited an adsorption capacity of 63 mg/g for Ni(II) ions, and the average amount of treated water was 84.6 bed volumes (BV) in the pilot-scale experiments. After the adsorption by two ion-exchange resin columns in series and one chelating resin column, the concentrations of Ni(II) in the treated wastewater were below 0.1 mg/L. After the regeneration of the spent resin using 3 BV of 4% (w/w) HCl solution, 1.5 BV of concentrated neutral nickel solution (>30 g/L) was obtained and used in the subsequent electrodeposition process. Using the aeration method, alkali and water required in resin activation process were greatly reduced to 2 BV and 3 BV, respectively. Under the optimal electrodeposition conditions, 95.6% of Ni(II) in desorption eluent could be recovered as the elemental nickel on the cathode. The total treatment cost for the resin adsorption and regeneration as well as the electrodeposition was calculated. 相似文献
Sb release characteristics of blast furnace slag, mining waste rock and tailing sand were investigated in static immersion and dynamic leaching test. These three kinds of waste samples were collected from the antimony mine in Lengshuijiang, China, produced in mining smelting process. Effects of solid/liquid ratio, sample size and pH of leaching solution on Sb release characteristics were inspected based on the analysis of scanning electron microscope, pH and EC of leachate. The optimal parameters for Sb leaching of each sample were analyzed. For blast furnace slag and mining waste rock, Sb release contents increased along with the decline of solid/liquid ratio. The maximum accumulative release contents were 42.13, 34.26 mg/kg at the solid/liquid ratio of 1:20. While Sb release content for tailing sand decreased first and then increased with the reduction of solid/liquid ratio. When the solid/liquid ratio was 1:5, the accumulative Sb release content reached the most (24.30 mg/kg). Sb release content of mining waste rock increased with the drop of leaching solution pH, with the highest accumulative release content of 26.01 mg/kg at pH 2.0. Sb release contents of blast furnace slag and tailing sand showed positive correlation with the variation of leaching solution pH. The maximum accumulative release contents of these two samples were 215.91 and 147.83 mg/kg, respectively, when leaching solution pH was 7.0. In summary, Sb release capacity of the three samples in descending order was tailing sand, blast furnace slag and mining waste rock. pH and EC of the leachate in dynamic test varied independently with the initial pH of leaching solution while showing close relationship with mineral hydrolysis in the waste. 相似文献
Environment, Development and Sustainability - This study attempts to introduce haze pollution into the environmental efficiency evaluation framework and measures PM2.5 environmental efficiency in... 相似文献
Regional Environmental Change - In recent decades, human activities have significantly influenced land use/land cover. Identifying pattern changes in regional land use/land cover and their drivers... 相似文献
In this study, farmland and mining ecotypes of Solanum photeinocarpum (a potential cadmium (Cd) hyperaccumulator plant) were reciprocally hybridized each other, and the Cd accumulation characteristics of the F1 hybrids were studied. In pot experiments, higher biomasses and Cd extraction abilities were found for two S. photeinocarpum F1 hybrids than for the parents, but the Cd contents in various organs were lower in the hybrids than the parents. However, the differences between the Cd contents in the two hybrids were not significant. The antioxidant enzyme (superoxide dismutase and peroxidase) activities were higher for the S. photeinocarpum F1 hybrids than the parents. Less DNA methylation was found in the hybrids than the parents because more demethylation occurred in the hybrids than the parents. The biomass, Cd content, and Cd extraction ability effects in field experiments were similar to the effects in the pot experiments. It was concluded that reciprocally hybridizing different S. photeinocarpum ecotypes improved the ability of S. photeinocarpum to be used to phytoremediate contaminated land.
Fluorine or fluoride can have toxic effects on bone tissue and soft tissue at high concentrations. These negative effects include but not limited to cytotoxicity, immunotoxicity, blood toxicity, and oxidative damage. Apoptosis plays an important role in fluoride-induced toxicity of kidney, liver, spleen, thymus, bursa of Fabricius, cecal tonsil, and cultured cells. Here, apoptosis activated by high level of fluoride has been systematically reviewed, focusing on three pathways: mitochondrion-mediated, endoplasmic reticulum (ER) stress-mediated, and death receptor-mediated pathways. However, very limited reports are focused on the death receptor-mediated apoptosis pathways in the fluoride-induced apoptosis. Therefore, understanding and discovery of more pathways and molecular mechanisms of fluoride-induced apoptosis may contribute to designing measures for preventing fluoride toxicity. 相似文献